Backside metallization affects residual stress and bending strength of the recast layer in laser-diced Si
Source abstract
Abstract
Thin Silicon dies separated by laser dicing form a thin layer via redeposition of ablated silicon known as recast layer . This work analyzed the influence of the recast layer microstructure and nanoscale residual stress gradients on the bending strength of bare and metalized silicon dies <100 μm. Scanning and transmission electron microscopy revealed an intricate microstructure of ablated silicon and elements of the wafer backside metallization within the recast layer. Refined silicon grains decorated by nanoscopic metallic precipitates at their grain boundaries were observed. Cross-sectional synchrotron X-ray nanodiffraction revealed that the altered microstructure increased the tensile residual stress from 200 to 295 MPa for bare and metalized dies, respectively. Additionally, the metalized die exhibited gradients in residual stress and grain size between the die front- and backside. Despite their similar frontside bending strengths of ∼340 MPa, observed in 3-point bending experiments, a considerable strengthening of the backside from 425 up to 957 MPa was measured for bare and metalized die, respectively. The origins of the tensile residual stress and the influence of the backside metallization on the die bending strength are discussed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Surface Polishing Techniques · Laser Material Processing Techniques · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Three-dimensional silicon integration10.1147/JRD.2008.5388564 ↗
2. Overview and outlook of through‐silicon via (TSV) and 3D integrations10.1108/13565361111127304 ↗
3. Integrated circuit packaging review with an emphasis on 3D packaging10.1016/j.vlsi.2017.09.008 ↗
4. Ultrathin wafer pre-assembly and assembly process technologies: a review10.1080/10408436.2014.992585 ↗
5. Femtosecond laser dicing of ultrathin Si wafers with Cu backside layer - a fracture strength and microstructural study10.1016/j.jmapro.2021.01.001 ↗
6. Effect of nanosecond laser dicing on the mechanical strength and fracture mechanism of ultrathin Si dies with Cu stabilization layer10.1109/TCPMT.2015.2497271 ↗
7. Fracture strength and microstructural study of ultrathin Si die with Cu backside layer diced with picosecond laser10.1016/j.msea.2019.04.103 ↗
8. Influence of deposited metal structures on the failure mechanisms of silicon-based components10.1016/j.jeurceramsoc.2012.06.027 ↗
9. A novel approach to assess the mechanical reliability of thin, ceramic-based multilayer architectures10.1016/j.jeurceramsoc.2020.02.016 ↗
10. 2003
11. Weibull · 1939
12. Induced stresses and structural changes in silicon wafers as a result of laser micro-machining10.1016/S0169-4332(01)01043-1 ↗
13. Femtosecond versus nanosecond laser machining: comparison of induced stresses and structural changes in silicon wafers10.1016/j.apsusc.2004.08.029 ↗
14. Stress analysis of Si chip sidewalls using micro-Raman spectroscopy
15. Analysis of residual stress in diamond films by x-ray diffraction and micro-Raman spectroscopy10.1063/1.1431431 ↗
16. Tutorial: understanding residual stress in polycrystalline thin films through real-time measurements and physical models10.1063/1.4949263 ↗
17. 30 nm X-ray focusing correlates oscillatory stress, texture and structural defect gradients across multilayered TiN-SiOx thin film10.1016/j.actamat.2017.11.049 ↗
18. X-ray nanodiffraction reveals strain and microstructure evolution in nanocrystalline thin films10.1016/j.scriptamat.2012.07.034 ↗
19. Grain boundary design of thin films: using tilted brittle interfaces for multiple crack deflection toughening10.1016/j.actamat.2016.09.027 ↗
20. Nanoscale residual stress and microstructure gradients across the cutting edge area of a TiN coating on WC Co10.1016/j.scriptamat.2020.02.031 ↗
21. Evolution of stress fields during crack growth and arrest in a brittle-ductile CrN-Cr clamped-cantilever analysed by X-ray nanodiffraction and modelling10.1016/j.matdes.2020.109365 ↗
22. An improved three-point bending test method for the investigation of nanosecond laser dicing of ultrathin Si dies with Cu stabilization layer10.1016/j.matchar.2017.11.060 ↗
23. In situ mapping of crack progression in nanocrystalline FeCr: nanoscale stress-strain evolution in nanocrystalline microstructure
24. Multiaxial stress-strain transfer across indenter-sample interface during in-situ indentation of soft high-entropy shape memory alloys and h
25. PyFAI, a versatile library for azimuthal regrouping10.1088/1742-6596/425/20/202012 ↗
26. The fast azimuthal integration Python library: pyFAI10.1107/S1600576715004306 ↗
27. Bestimmung der Grosse und inneren Struktur von Kolloidteilchen mittels Rontgenstrahlen
28. The Scherrer equation versus the ‘Debye-Scherrer equation10.1038/nnano.2011.145 ↗
29. X-ray analysis of residual stress gradients in TiN coatings by a Laplace space approach and cross-sectional nanodiffraction: a critical comparison10.1107/S0021889813019535 ↗
30. Calculated elastic constants for stress problems associated with semiconductor devices10.1063/1.1661935 ↗
31. Ultrashort pulse laser dicing of thin Si wafers: the influence of laser-induced periodic surface structures on the backside breaking strength10.1088/0960-1317/26/11/115004 ↗
32. A structure zone diagram including plasma-based deposition and ion etching10.1016/j.tsf.2009.10.145 ↗
33. Binary alloy phase diagrams
34. Thermodynamic modeling of the V–Si system supported by key experiments10.1016/j.calphad.2007.12.005 ↗
35. The Ni−Si (Nickel-Silicon) system10.1007/BF02868885 ↗
36. The Ag-Au-Si system: experimental and calculated phase diagram10.1007/BF02647235 ↗
37. Origins of microstructure and stress gradients in nanocrystalline thin films: the role of growth parameters and self-organization10.1016/j.actamat.2013.07.009 ↗
38. Linear thermal expansion coefficients of amorphous and microcrystalline silicon films10.1016/S0022-3093(02)00930-4 ↗
39. Study of die break strength and heat-affected zone for laser processing of thin silicon wafers10.2351/1.4916979 ↗
40. What is the young's modulus of silicon?10.1109/JMEMS.2009.2039697 ↗
41. Elastic stiffness and thermal expansion coefficients of various refractory silicides and silicon nitride films10.1016/0040-6090(80)90364-8 ↗
42. Grain boundary segregation engineering in metallic alloys: a pathway to the design of interfaces10.1016/j.cossms.2014.06.002 ↗
43. On grain boundary segregation in molybdenum materials10.1016/j.matdes.2017.09.019 ↗
44. Assessment of grain boundary cohesion of technically pure and boron micro-doped molybdenum via meso-scale three-point-bending experiments10.1016/j.matdes.2021.109848 ↗
45. Precipitation-based grain boundary design alters inter- to trans-granular fracture in AlCrN thin films10.1016/j.actamat.2022.118156 ↗
46. Lawn · 1993