Silicon damage control through the use of aromatic hydrocarbon ion implantation
Source abstract
Abstract
Abstract The continuous shrinking of transistor devices calls for precise doping profile control. Generally, monomer carbon (C+) is implanted at doses too low to adequately form an amorphous layer in silicon. Previous experiments used a molecular carbon species combined with dedicated vaporizer-based hardware, but this experiment was carried out using a commercial implanter and source with a liquid precursor material. The use of higher mass molecular carbon ions, such as C7H7+, impart significantly more damage to the silicon than the monomer, and can easily result in a well-defined amorphous layer. There are many species of molecular carbon that can be implanted, but in order to utilize a hot cathode plasma (HCP) ion source some additional criteria must be met. The source feed material should fragment with high-yield of molecular carbon (Cx+, x = 2–8) ions, which could then be extracted at beam currents sufficient to meet production needs using standard ion implant techniques. In this work, we surveyed several candidates for forming the molecular carbon species that could meet the requirements outlined above, reported the performance in plasma formation, and investigated materials properties of the Si after implantation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ion-surface interactions and analysis · Silicon and Solar Cell Technologies · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Design of ion-implanted MOSFET's with very small physical dimensions10.1109/JSSC.1974.1050511 ↗
2. Sze · 2006
3. Physical mechanisms of transient enhanced dopant diffusion in ion-implanted silicon10.1063/1.364452 ↗
4. Transient boron diffusion in ion‐implanted crystalline and amorphous silicon10.1063/1.339926 ↗
5. Carbon incorporation in silicon for suppressing interstitial‐enhanced boron diffusion10.1063/1.113204 ↗
6. Advanced source/drain engineering for box-shaped ultrashallow junction formation using laser annealing and pre-amorphization implantation in sub-100-nm SOI CMOS10.1109/TED.2002.803634 ↗
7. Park, Bo Hyun. 1998, Method for Forming Shallow Junction for Semiconductor Device. Hyundai Electronics Industries C., Ltd., Kyoungki-do, U.S. Patent No. vol. 5,795,808.
8. Pre-amorphization damage in ion-implanted silicon10.1016/0920-2307(91)90001-4 ↗
9. Ion implantation in semiconductors—Part II: damage production and annealing10.1109/PROC.1972.8854 ↗
10. Ion implantation in semiconductors10.1088/0031-9112/20/5/002 ↗
11. Formation of amorphous silicon by ion bombardment as a function of ion, temperature, and dose10.1063/1.1661223 ↗
12. Ion implantation in CMOS Technology: machine challenges
13. Jacobson, et al. 2011, Cluster Ion Implantation for Defect Engineering. SEMEQUIP, Inc., Massachusetts U.S. Patent No. vol. 7,919,402.
14. Cluster carbon implants—cluster size and implant temperature effect
15. Annealing behavior of clustercarbon™ implants
16. Ion sources
17. Brown · 2004
18. Linstrom, P. J., and W. G. Mallard. "NIST Chemistry Webbook (http://webbook.nist.Gov/chemistry)." NIST Standard Reference Database 69.
19. Sources of variation in Therma Wave measurements of ion implanted wafers10.1016/0168-583X(93)95050-F ↗
20. Pre-amorphization damage in ion-implanted silicon10.1016/0920-2307(91)90001-4 ↗
21. Formation of amorphous layers by ion implantation10.1063/1.334840 ↗
22. Kalra · 2008