Ge heteroepitaxy on Si(111) substrate featuring sputtering method
Source abstract
Abstract
Ge(111) epitaxial layers grown on Si(111) substrates have attracted considerable interest as buffer substrates for preparing functional materials, such as Ge-based two-dimensional materials and Ge 1− x Sn x (111). To prepare the Ge/Si(111) buffer substrate, we focused on the sputtering process because of its high deposition rate, compatibility with CMOS processes, and cost efficiency. Because few studies have reported Ge(111) sputtering heteroepitaxy, we performed a comprehensive study focusing on a two-step growth method and post-deposition annealing (PDA). In this study, we investigated the effects of thickness of the low-temperature-grown Ge (LT-Ge) layer and PDA on the surface morphology and crystalline properties of Ge(111) layers. We found that Ge(111) layers followed by PDA with LT-Ge layer thicknesses less than 10 nm exhibited a flatter surface (root mean square roughness <2 nm), a narrower ω rocking curve (full width at half maximum of ∼0.07°), and a lower sheet carrier density of the Ge/n-Si(111) structure. Furthermore, we observed that the types of defects introduced at the initial Ge growth stage depended on the LT-Ge layer thickness. An LT-Ge layer thickness of less than 10 nm induced threading dislocations, whereas a thickness greater than 40 nm induced stacking faults. Because threading dislocations can move during PDA, they were likely annihilated, whereas stacking faults persisted even after PDA. This behavior resulted in superior crystallinity and a flat Ge(111) heteroepitaxial layer when an ultra-thin LT-Ge layer was introduced.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and interfaces · Semiconductor Quantum Structures and Devices · Surface and Thin Film Phenomena
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Segregation control for ultrathin Ge layer in Al/Ge(111) system10.35848/1347-4065/ac19ff ↗
2. Impact of substrate heating during Al deposition and post annealing on surface morphology, Al crystallinity, and Ge segregation in Al/Ge(111) structure10.35848/1347-4065/ac5fbc ↗
3. Layer transfer of ultrathin Ge crystal segregated on Al/Ge(111) structure10.35848/1347-4065/acb65c ↗
4. Intrinsic carrier mobility of germanene is larger than graphene's: first-principle calculations10.1039/C4RA01802H ↗
5. Monte-Carlo study of electronic transport in non-σh-symmetric two-dimensional materials: silicene and germanene10.1063/1.5037581 ↗
6. Massive Dirac quasiparticles in the optical absorbance of graphene, silicene, germanene, and tinene10.1088/0953-8984/25/39/395305 ↗
7. Quantum spin hall effect in silicene and two-dimensional germanium10.1103/PhysRevLett.107.076802 ↗
8. Low-energy effective Hamiltonian involving spin-orbit coupling in silicene and two-dimensional germanium and tin10.1103/PhysRevB.84.195430 ↗
9. Observation of Room-Temperature Magnetoresistance Effect in Co2Fe(Al,Si)/Ge/Co2FeSi Vertical Spin-Valve Devices on Si10.1016/j.mssp.2025.109809 ↗
10. Semiconductor spintronics with Co2-Heusler compounds10.1557/s43577-022-00351-0 ↗
11. Half‐metallic heusler Alloy/GaN heterostructure for semiconductor spintronics devices10.1002/aelm.202300045 ↗
12. Electrical properties of a low-temperature fabricated Ge-based top-gate MOSFET structure with epitaxial ferromagnetic Heusler-alloy Schottky-tunnel source and drain10.1016/j.mssp.2023.107763 ↗
13. Effect of Sn doping on low-temperature growth of Ge epilayers on half-metallic Co2FeSi10.1016/j.mssp.2023.107987 ↗
14. Dislocation-free Stranski-Krastanow growth of Ge on Si(100)10.1103/PhysRevLett.64.1943 ↗
15. Calculation of critical layer thickness versus lattice mismatch for GexSi1−x/Si strained-layer heterostructures10.1063/1.96206 ↗
16. Reduced pressure chemical vapor deposition of Ge thick layers on Si(001), Si(011) and Si(111)10.1016/j.jcrysgro.2008.08.062 ↗
17. Growth of smooth, low-defect germanium layers on (111) silicon via an intermediate islanding process10.1143/APEX.5.071301 ↗
18. High quality relaxed germanium layers grown on (110) and (111) silicon substrates with reduced stacking fault formation10.1063/1.4825130 ↗
19. High Crystallinity Ge Growth on Si (111) and Si (110) by Using Reduced Pressure Chemical Vapor Deposition10.1149/2162-8777/acbb9d ↗
20. Formation of tensilely strained germanium-on-insulator10.1143/APEX.5.015701 ↗
21. Structural and electrical properties of Ge(111) films grown on Si(111) substrates and application to Ge(111)-on-Insulator10.1016/j.tsf.2015.11.020 ↗
22. Ge growth mode modification on carbon-induced Si(001)-c(4×4) surfaces10.1016/S0040-6090(00)01465-6 ↗
23. Sputter epitaxial growth of flat germanium film with low threading-dislocation density on silicon (001)10.1149/2.0091410jss ↗
24. Comprehensive study on epitaxial growth of GeSn(111) layers with high Sn content on Si(111) featuring Ge buffer layer10.1149/11402.0215ecst ↗
25. Thermal expansion and lattice parameters of group IV semiconductors10.1016/S0254-0584(96)01808-1 ↗
26. Acceptor like behavior of defects in SiGe alloys grown by molecular beam epitaxy10.1143/JJAP.47.4630 ↗
27. Thin-body Ge-on-insulator p-channel MOSFETs with Pt germanide metal source/drain10.1016/j.tsf.2005.07.339 ↗
28. High-quality single-crystal Ge stripes on quartz substrate by rapid-melting-growth10.1063/1.3182795 ↗
29. Characterization of Shallow- and deep-level defects in undoped Ge1−xSnx epitaxial layers by electrical measurements10.1149/2.0151604jss ↗