journal article·2015-03-31Open access

The influence of the technological parameters on the ionic conductivity of samarium doped ceria thin films

Mantas Sriubas, Giedrius Laukaitis

Materials Science· Volume 21· Issue 1

Abstract

Sm0,20Ce0,80O2 powder was used for the formation of samarium doped cerium oxide (SDC) thin films using e-beam. Surface area of powder was 34.9 m2/g and particle size – 0.3-0.5 μm. Thin films were deposited using physical vapor deposition system on SiO2 and Alloy 600 substrates. 2 Å/s – 16 Å/s growth rate and 20 °C – 600 °C substrate temperature were used during the deposition. Ionic conductivity investigation revealed that the maximum ionic conductivity (1.67 S/m) has the thin film deposited on 300 °C temperature substrate using 4 Å/s growth rate. Minimum ionic conductivity (0.26 S/m) has thin film which was deposited on 20 °C temperature substrate using 8 Å/s growth rate. Vacancy activation energies vary in 0.87 eV – 0.97 eV range. Furthermore the calculations of crystallite size revealed that crystallite size increases with increasing substrate temperature: from 7.50 nm to 46.23 nm on SiO2 substrate and from 9.30 nm to 44.62 nm on Alloy 600 substrate. Molar concentration of samarium in initial evaporated material is 19.38 mol% and varies from 11.37 mol% to 21 mol% in formed thin films depending on technological parameters.DOI: http://dx.doi.org/10.5755/j01.ms.21.1.5700
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Catalytic Processes in Materials Science

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.