Stress-induced Hydride Reorientation and Cracking in Fuel Cladding Tube

Albertas GRYBĖNAS, Vidas MAKAREVIČIUS, Tadas KALIATKA, Gintautas DUNDULIS, Rita KRIŪKIENĖ

Materials Science· Volume 20· Issue 4

Abstract

Goal of this research was to find out if reorientation can influence cladding failure and determine conditions and possible mechanism of failure. Reorientation tests were done on zircaloy nuclear fuel cladding specimens. Specimens were made having two triangular notches along specimen axis which are similar to the surface flaw that can form during operation. Loading was applied using PLT loading fixture to give stress proportional to a distance from the specimen front. When loaded, specimen was cooled from 340 to 40 °C at a cooling rate 0.25 °/min., total duration of test was 20h. After testing, specimen was examined layer by layer metallographically to determine hydride reorientation under certain stress conditions. In case of a surface flaw reorientation of hydrides takes place perpendicular to the stress direction. It was found that hydride reorientation occurs at a stress range 77 – 89 MPa, for initiation of DHC process larger stress is required than for hydride reorientation. DOI: http://dx.doi.org/10.5755/j01.ms.20.4.5477
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Nuclear reactor physics and engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.