A Facile Method for Low-Temperature Synthesis of NaV₃O₈ as Cathode Materials for Lithium Secondary Batteries
Source abstract
Abstract
A facile method has been used to synthesize NaV3O8 powders with oxalic acid as the complexing agent. This soft-synthesis technique can effectively reduce the calcination temperature for synthesizing NaV3O8 powders to 300 °C, which is much lower than that in the solid-state synthesis. The thus-synthesized NaV3O8 powders are characterized by XRD, SEM and galvanostatic charge-discharge test. Among the as-prepared powders, the NaV3O8 powder obtained at 350 °C exhibits morphology of porous particles. The electrochemical analysis reveals that this powder demonstrates high discharge capacity and good cycleability.http://dx.doi.org/10.5755/j01.ms.17.1.252
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Transition Metal Oxide Nanomaterials · Semiconductor materials and devices · Advancements in Battery Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.