The Influence of Thermal Annealing on Texture of Yttrium Stabilized Zirconia Thin Films
Source abstract
Abstract
Yttrium stabilized zirconia (YSZ) thin films were grown evaporating tetragonal phase zirconia stabilized by 8 wt. % ofyttrium (8YSZ) ceramic powder. YSZ thin films were deposited on optical quartz substrates using e-beam depositiontechnique controlling deposition parameters: substrate temperature and electron gun power influencing thin filmproperties. YSZ thin films (1.5 μm – 2 μm of thickness) were deposited at different substrate temperatures (250 ºC,400 ºC, 600 ºC) and the electron gun power was 0.66 kW, 0.9 kW, 1.05 kW, and 1.2 kW during thin films deposition. Tounderstand the stability and influence of temperature on the structure of formed thin films the deposited YSZ layers wereannealed at 1100 ºC temperature, in air and were investigated by X-ray diffraction (XRD). It was found that annealingtemperature, electron gun power, and substrate temperature influence the crystallite size of YSZ: crystallite size beforeannealing was 12.2 nm – 46.2 nm and after annealing was 23 nm – 49.8 nm. It was found that the main orientation of theYSZ thin films texture repeats the characteristics of the evaporated YSZ powder and dominant crystal structure oftetragonal phase of YSZ thin films is (101). The same (101) tetragonal phase remains after annealing at 1100 ºCtemperature. The crystallite size and coefficient of texture increases but repeats the character of the curves as it was beforethe annealing. The temperature and substrate material does not influence the texture of YSZ thin films.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electrophoretic Deposition in Materials Science · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.