Investigation of Damaged Paper by Ink Corrosion
Source abstract
Abstract
The investigation of cotton fibers sheets treated with different historical writing inks: Pfalz ink from red wine (ink-1,pH 3.51), Ink from the oak’s bark extracts (ink-2, pH 3.69); Iron-gall ink (ink-3, pH 1.66), Black ink with iron(II)sulphate (ink-4, pH 1.52 ), Black ink with copper(II) sulphate (ink-5, pH 2.14), Logwood tree ink (ink-6, pH 5.73),German recipe A (iron(II) sulphate) (ink-7, pH 1.94), German recipe B (iron(II) sulphate) (ink-8, pH 1.62) wasperformed using FTIR spectroscopy. The paper and ink treated paper samples were artificially aged (accelerated thermaland photo ageing) also analyzed and the results compared with the non-treated ones. The study focus was on thespectrum range between 1500 cm–1 and 1900 cm–1, where the products of the paper ageing appear as various carbonylgroups. After immersing paper to inks with metal ions, the increase of absorption at 1713 cm–1 – 1745 cm–1 wasobserved. Also, the drastic decreasing of polymerization degree of ink treated samples was estimated.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Cultural Heritage Materials Analysis · Advanced Cellulose Research Studies · Material Properties and Processing
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.