Preparation and electrical properties of polyimide/carbon nanotubes composites

Aseel A. Kareem

Materials Science-Poland· Volume 35· Issue 4

Abstract

Abstract Polyimide/MWCNTs nanocomposites have been fabricated by solution mixing process. In the present study, we have investigated electrical conductivity and dielectric properties of PI/MWCNT nanocomposites in frequency range of 1 kHz to 100 kHz at different MWCNTs concentrations from 0 wt.% to 15 wt.%. It has been observed that the electrical conductivity and dielectric constants are enhanced significantly by several orders of magnitude up to 15 wt.% of MWCNTs content. The electrical conductivity increases as the frequency is increased, which can be attributed to high dislocation density near the interface. The rapid increase in the dielectric constant at a high MWCNTs content can be explained by the formation of a percolative path of the conducting network through the sample for a concentration corresponding to the percolation threshold. The high dielectric constant at a low frequency (1 kHz) is thought to originate from the space charge polarization mechanism. I-V characteristics of these devices indicate a significant increase in current with an increase in multi-walled carbon nanotube concentration in the composites. The SEM images show improved dispersion of MWCNTs in the PI matrix; this is due to the strong interfacial interactions.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Conducting polymers and applications · Carbon Nanotubes in Composites · Dielectric materials and actuators

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Physics, College of Science, University of Baghdad, Baghdad , Iraq

References (16)

Show source-provided references
1. [1] WEI B.Q., VAJTAI R., AJAYAN P.M., Appl. Phys. Lett., 79 (2001), 1172.10.1063/1.1396632 ↗
2. [2] UPADHYAY A.N., TIWARI R.S., SINGH K., Adv. Mater. Lett., 6 (2015), 1098.10.5185/amlett.2015.5978 ↗
3. [3] KHARE R., BOSE S., J. Miner. Mater. Character. Eng., 4 (2005), 31.10.4236/jmmce.2005.41004 ↗
4. [4] NAYAK L., RAHAMAN M., ALDALBAHI A., CHAKI T.K., KHASTGIR D., Poly. Eng. Sci., (2016). DOI 10.1002/pen.24412.10.1002/pen.24412
5. [5] ZHANG Q., LI J., ZHAO X., CHEN D., Poly. Int., 58 (2009), 557.10.1002/pi.2568
6. [6] CHEN Y., LIN B., ZHANG X., WANG J., LAI CH., SUN Y., LIUAB Y., YANGA H., J. Mater. Chem., 2 (2014), 14118.10.1039/C4TA01818D10.1039/C4TA01818D ↗
7. [7] PARK S., CHAE S., RHEE J., KANG S., Bull. Korean Chem. Soc., 31 (2010), 2279.10.5012/bkcs.2010.31.8.2279
8. [8] MO T., WANG H., CHEN S., YEH Y., Poly. Compos., 29 (2008), 451.10.1002/pc.20468 ↗
9. [9] JIANG X., BIN Y., MATSUO M., Poly., 46 (2005), 7418.10.1016/j.polymer.2005.05.127 ↗
10. [10] THUAU D., KOUTSOS V., CHEUNG R., J. Vac. Sci. Technol., 27 (2009), 3139.10.1116/1.3250192 ↗
11. [11] OUNAIES Z., PARK C., WISE K.E., SIOCHI E.J., HARRISON J.S., Comp. Sci. Technol., 63 (2003), 1637.
12. [12] ZHANG Y., YU L., ZHAO L., TONG W., HUANG H., KE S., CHAN H. L. W., J. Electron. Mater., 41 (2012), 2281.10.1007/s11664-012-2037-2
13. [13] KIM B.S., Macromol. Res., 15 (2007), 357.10.1007/BF03218799 ↗
14. [14] YUEN S., MA C. M., CHIANG C., LIN Y., TENG C., J. Poly. Sci. Poly. Chem., 45 (2007), 3349.10.1002/pola.22085
15. [15] QU L., LIN Y., HILL D. E., ZHOU B., WANG W., SUN X., KITAYGORODSKIY A., SUAREZ M., CONNELL J. W., ALLARD L. F., SUN Y., Macromol., 37 (2004), 6055.10.1021/ma0491006 ↗
16. [16] LIM J., SHIN D.G., YEO H., GOH M., KU B., YANG C., LEE D.S., HWANG J., PARK B., YOU N., J. Poly. Sci. Poly. Phys., 52 (2014), 960.10.1002/polb.23515