Strain ageing embrittlement behaviour of X80 self-shielded flux-cored girth weld metal
Source abstract
Abstract
Strain ageing embrittlement behaviour of X80 self-shielded flux-cored arc welding (FCAW) girth weld metal at different strain ageing conditions (1% prestrain, and aged at 150°C/100°C for 1 –6 h, and 80°C for 1–30 days) was studied. Microstructure of FCAW girth weld generally consisted of coarse granular bainite and lath bainite. After strain ageing, toughness notably decreased, and higher ageing temperature or longer ageing induced lower toughness, until ageing is fully yielded. At initial stage of strain ageing, more dimples were found accompanying with cleavage facet. With the progress of strain ageing, the embrittlement was more obvious, while larger cleavage facet and less dimples were found. Meanwhile, the critical size for cleavage fracture initiation site became smaller. Martensite–austenite constituent (1–2 μm) was found to initiate cleavage fracture when partially strain aged, while submicron inclusions could initiate cleavage facet when fully strain aged.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Production and operation department, PipeChina West East Gas Pipeline Company, China
Pipeline Material and Anti-corrosion Technology Center, China Petroleum Pipeline Research Institute CO.,LTD, China
Science and technology information center, China Oil & Gas Piping Network Corporation, China
School of Materials Science and Engineering, China University of Petroleum (East China), China
References (24)
Show source-provided references
1. Cui TC, Zheng L, Wu HF. Effect of strain aging on mechanical properties of high strength pipeline steel with different composition[J]. Mater Mech Eng. 2010;34(5):30–32+55.
2. 10.4028/www.scientific.net/MSF.654-656.12210.4028/www.scientific.net/MSF.654-656.122 ↗
3. 10.1016/j.msea.2012.04.09510.1016/j.msea.2012.04.095 ↗
4. Cheng YF. Some technical considerations on ensuring the long term safe operation of China Russia east gas pipeline[J]. Oil Gas Storage Transp. 2020;39(1):1–8.
5. 10.1016/j.engfailanal.2019.10435910.1016/j.engfailanal.2019.104359 ↗
6. 10.1007/s42243-019-00313-y10.1007/s42243-019-00313-y ↗
7. Zhang ZY. Key points of safety lifting design for girth weld of high grade and large diameter natural gas pipeline[J]. Oil Gas Storage Transp. 2020;39(7):740–748.
8. Shuai J, Wang X, Zhang YH, et al. Main characteristics and safety evaluation of girth weld of high grade steel pipeline[J]. Oil Gas Storage Transp. 2020;39(6): 623–631
9. 10.1088/0370-1298/62/1/30810.1088/0370-1298/62/1/308 ↗
10. 10.1179/mtlr.1971.16.1.110.1179/mtlr.1971.16.1.1 ↗
11. 10.1007/BF0265853610.1007/BF02658536 ↗
12. 10.1115/IPC2010-3137110.1115/IPC2010-31371 ↗
13. 10.1007/s11665-013-0683-z10.1007/s11665-013-0683-z ↗
14. 10.1016/j.engfailanal.2020.10484410.1016/j.engfailanal.2020.104844 ↗
15. Yang J, Bi ZY, Nan HH, et al. Strain aging behavior and sensitive temperature of X90 high strength pipeline steel[J]. Chin J Mater Res. 2021;35(10):769–777.
16. Wang HK, Shang XX, Liu W, et al. Study on strain aging embrittlement of girth weld of high grade oil and gas pipeline[J]. Pressure Vessel Technol. 2021;38(5):8–13.
17. 10.1179/mst.1985.1.3.23410.1179/mst.1985.1.3.234 ↗
18. 10.1080/0950711880945112810.1080/09507118809451128 ↗
19. 10.1016/j.msea.2019.13889710.1016/j.msea.2019.138897 ↗
20. 10.1179/stw.1998.3.5.23310.1179/stw.1998.3.5.233 ↗
21. 10.1016/j.jmatprotec.2004.04.28510.1016/j.jmatprotec.2004.04.285 ↗
22. 10.1179/mst.1985.1.5.35710.1179/mst.1985.1.5.357 ↗
23. Yu P, Tian ZL, Pan C, et al. Gas in weld of self shielded flux cored wire[J]. Trans China Weld Inst. 2007;28(2):67–70.
24. Gao SS, Di XJ, Li CN, et al. Effect of strain aging on fracture toughness of welded joints of high strain pipeline steel[J]. Trans China Weld. 2021;42(10):22–28.