journal article·2022-03-21

Microstructural study and mechanical characterisation of heat-treated direct metal laser sintered Ti6Al4V for biomedical applications

Dheepa Srinivasan, Anubhav Singh, Anigani Sudarshan Reddy, Kaushik Chatterjee

Materials Technology· Volume 37· Issue 4
Publisher page

Abstract

Direct metal laser sintering (DMLS) of Ti6Al4V is being widely used to manufacture biomedical implants. The rapid solidification process can result in undesired microstructure that imparts poor ductility and end up residual stresses. An optimum heat treatment minimizes distortion and enables a desirable microstructure. In this work, we have examined the efficacy of heat treatment in vacuum and in air, at 800°C and 1100°C. There were minimal differences in the microstructure and mechanical properties when heat treated in air or vacuum, at 800°C. Heat treatment at 1100°C was feasible in vacuum but not in air. Comparisons were made with two-layer thicknesses (30 and 50mm) to enable higher productivity. These results were validated using a cranial implant. Thus, it may be possible to do heat treatment in air at 800°C for DMLS Ti6Al4V thereby enabling manufacturing of implants by DMLS process in a timely and cost-effective manner.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

INTECH DMLS, Pvt. Ltd., Peenya Industrial Area

Pratt and Whitney R &D centre

Indian Institute of Science, C.V. Raman Avenue

Funding

Uchchatar Avishlkar Yojana

References (33)

Show source-provided references
1. 10.1155/2019/974821210.1155/2019/9748212 ↗
2. 10.1016/j.mtbio.2019.10002410.1016/j.mtbio.2019.100024 ↗
3. 10.1080/10667857.2016.117316910.1080/10667857.2016.1173169 ↗
4. 10.1080/10667857.2020.180030610.1080/10667857.2020.1800306 ↗
5. 10.1179/1753555715Y.000000007910.1179/1753555715Y.0000000079 ↗
6. 10.1016/j.pmatsci.2008.06.00410.1016/j.pmatsci.2008.06.004 ↗
7. 10.1080/09506608.2020.173582910.1080/09506608.2020.1735829 ↗
8. 10.1016/j.matdes.2018.10755510.1016/j.matdes.2018.107555 ↗
9. 10.1186/s40729-016-0051-510.1186/s40729-016-0051-5 ↗
10. 10.1016/j.jmbbm.2011.06.01810.1016/j.jmbbm.2011.06.018 ↗
11. 10.3390/ma1201017610.3390/ma12010176 ↗
12. 10.1016/j.rinp.2018.07.00810.1016/j.rinp.2018.07.008 ↗
13. 10.1016/j.msea.2015.10.06810.1016/j.msea.2015.10.068 ↗
14. 10.1155/2016/859097110.1155/2016/8590971 ↗
15. 10.1080/10667857.2017.138905210.1080/10667857.2017.1389052 ↗
16. 10.1007/s13534-018-0080-510.1007/s13534-018-0080-5 ↗
17. 10.1016/j.jfma.2019.07.02310.1016/j.jfma.2019.07.023 ↗
18. 10.1039/C9TB00093C10.1039/C9TB00093C ↗
19. 10.1155/2017/592071410.1155/2017/5920714 ↗
20. 10.1038/s41598-017-18030-510.1038/s41598-017-18030-5 ↗
21. 10.1002/jbm.a.3559210.1002/jbm.a.35592 ↗
22. 10.1166/jbt.2014.123210.1166/jbt.2014.1232 ↗
23. 10.1016/S2589-7500(19)30067-610.1016/S2589-7500(19)30067-6 ↗
24. 10.4028/www.scientific.net/MSF.828-829.30510.4028/www.scientific.net/MSF.828-829.305 ↗
25. 10.1007/s11665-018-3477-510.1007/s11665-018-3477-5 ↗
26. 10.1088/1742-6596/371/1/01208410.1088/1742-6596/371/1/012084 ↗
27. Tao P Li H Huang B et al. Tensile behavior of Ti-6Al-4V alloy fabricated by selective laser melting: effects of microstructures and as-built surface quality. China Foundry. 2018;15:243–252. https://link.springer.com/article/10.1007/s41230-018-8064-8.10.1007/s41230-018-8064-8 ↗
28. 10.1108/1355254101108337110.1108/13552541011083371 ↗
29. 10.1016/j.prostr.2016.06.39510.1016/j.prostr.2016.06.395 ↗
30. 10.1016/j.prostr.2019.05.05510.1016/j.prostr.2019.05.055 ↗
31. 10.1016/j.actamat.2018.09.06410.1016/j.actamat.2018.09.064 ↗
32. 10.1007/s40684-018-0062-110.1007/s40684-018-0062-1 ↗
33. 10.1016/j.protcy.2015.07.03710.1016/j.protcy.2015.07.037 ↗