journal article·2025-12-31

Influence of annealing temperature of seed layer on the structural and optical properties of ZnO nanorods synthesized by SILAR and CBD techniques

Ahmed Fattah Abdulrahman, Sozan Hussien Mostafa, Shayma Mohammed Ahmed, Amad Nori Abdulqodus, Awaz Adil Kareem, Sabah M. Ahmed, Shujahadeen B. Aziz, Munirah Abdullah Almessiere, Samir Mustafa Hamad, Dilshad Shaikhah

Materials Technology· Volume 40· Issue 1
Publisher page

Abstract

In this study, zinc oxide nanorods were synthesized using chemical bath deposition with a ZnO seed layer on glass substrates via successive ionic layer adsorption and reaction. The effect of annealing temperature on the seed layer was investigated using various characterization techniques. Results show that annealing temperature significantly influenced the morphology and quality of ZnO NRs. As the temperature increased from 0°C to 500°C, the nanorod length grew from 591 to 1008 nm. Optimal conditions were found at 450°C, with a growth rate of 4.2 nm/min and an aspect ratio of 11. The crystalline size ranged from 10.56 to 52.93 nm, confirmed by XRD analysis, showing the hexagonal wurtzite structure. The bandgap energy varied from 3.221 eV to 3.2656 eV, reflecting the impact of annealing on optical properties. Optical transmittance was highest at 0°C, decreasing from 57% to 13% as the annealing temperature increased.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: ZnO doping and properties · Gas Sensing Nanomaterials and Sensors · Ga2O3 and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Duhok Polytechnique University

University of Zakho

University of Duhok

University of Sulaimani

Charmo University

Imam Abdulrahman Bin Faisal University

Soran University

University of Leeds

References (83)

Show source-provided references
1. 10.1364/oe.23.01893710.1364/oe.23.018937 ↗
2. 10.1021/nl304163n10.1021/nl304163n ↗
3. 10.1063/1.490538910.1063/1.4905389 ↗
4. 10.1155/2013/43683110.1155/2013/436831 ↗
5. 10.1016/j.snb.2011.12.07310.1016/j.snb.2011.12.073 ↗
6. 10.1063/1.490252010.1063/1.4902520 ↗
7. 10.1016/j.jcrysgro.2020.12599710.1016/j.jcrysgro.2020.125997 ↗
8. 10.3390/ma304221810.3390/ma3042218 ↗
9. 10.1016/j.optmat.2015.03.01210.1016/j.optmat.2015.03.012 ↗
10. Fulati A. Mechanical characterization and electrochemical sensor applications of zinc oxide N anostructures No. 1323. 2010. [Online]. Available http://hv.diva-portal.org/smash/record.jsf?pid=diva2:324728
11. 10.3390/coatings1204047410.3390/coatings12040474 ↗
12. 10.5185/amlett.2016.629810.5185/amlett.2016.6298 ↗
13. 10.1016/j.cplett.2005.04.03810.1016/j.cplett.2005.04.038 ↗
14. 10.1021/jp065501710.1021/jp0655017 ↗
15. 10.1166/jnn.2011.339510.1166/jnn.2011.3395 ↗
16. 10.1088/0957-4484/18/23/23560410.1088/0957-4484/18/23/235604 ↗
17. 10.1111/j.1551-2916.2009.03022.x10.1111/j.1551-2916.2009.03022.x ↗
18. 10.1007/s10971-009-2138-410.1007/s10971-009-2138-4 ↗
19. 10.1007/s11051-013-2115-210.1007/s11051-013-2115-2 ↗
20. 10.5402/2012/65146810.5402/2012/651468 ↗
21. 10.1002/pssa.20052139810.1002/pssa.200521398 ↗
22. 10.1155/2013/13054110.1155/2013/130541 ↗
23. 10.1063/1.307399310.1063/1.3073993 ↗
24. 10.1016/j.physb.2010.03.04110.1016/j.physb.2010.03.041 ↗
25. 10.1016/S1452-3981(23)07912-910.1016/S1452-3981(23)07912-9 ↗
26. 10.1021/nl050788p10.1021/nl050788p ↗
27. 10.3329/bjsir.v53i4.3918610.3329/bjsir.v53i4.39186 ↗
28. 10.1002/adma.20039010810.1002/adma.200390108 ↗
29. 10.1557/adv.2019.6510.1557/adv.2019.65 ↗
30. 10.1016/j.optmat.2023.11386910.1016/j.optmat.2023.113869 ↗
31. 10.1016/j.sna.2021.11265610.1016/j.sna.2021.112656 ↗
32. 10.1007/s10854-020-03995-310.1007/s10854-020-03995-3 ↗
33. 10.5012/bkcs.2011.32.3.88010.5012/bkcs.2011.32.3.880 ↗
34. 10.1002/pssc.20067427910.1002/pssc.200674279 ↗
35. 10.1016/j.solidstatesciences.2020.10637910.1016/j.solidstatesciences.2020.106379 ↗
36. Huang J-S, Lin C-F. Controlled growth of zinc oxide NR array in aqueous solution by zinc oxide sol-gel thin film in relation to growth rate and optical property IEEE Conference on Nanotechnology 2008 135–138.
37. 10.1002/sia.326210.1002/sia.3262 ↗
38. 10.4028/www.scientific.net/AMR.979.20410.4028/www.scientific.net/AMR.979.204 ↗
39. 10.1016/j.physe.2010.05.00410.1016/j.physe.2010.05.004 ↗
40. 10.1186/1556-276X-9-63210.1186/1556-276X-9-632 ↗
41. 10.1016/j.matlet.2012.05.13010.1016/j.matlet.2012.05.130 ↗
42. 10.1371/journal.pone.005040510.1371/journal.pone.0050405 ↗
43. 10.1038/nmat138710.1038/nmat1387 ↗
44. Gowthaman P, Saroja M, Venkatachalam M, et al. Structural and optical properties of ZnO NRs prepared by chemical bath deposition method. Australian J Basic Appl Sci. 2011;5(11):1379–1382 .
45. 10.1021/jp077133s10.1021/jp077133s ↗
46. 10.1016/S1003-6326(14)63119-810.1016/S1003-6326(14)63119-8 ↗
47. 10.1021/jp076870l10.1021/jp076870l ↗
48. 10.3365/KJMM.2015.53.2.13910.3365/KJMM.2015.53.2.139 ↗
49. 10.3390/nano1103067710.3390/nano11030677 ↗
50. 10.1016/j.matlet.2006.12.06410.1016/j.matlet.2006.12.064 ↗
51. 10.1016/j.sse.2015.11.00410.1016/j.sse.2015.11.004 ↗
52. 10.3390/cryst1005038610.3390/cryst10050386 ↗
53. 10.14716/ijtech.v6i4.194810.14716/ijtech.v6i4.1948 ↗
54. 10.1016/j.jmrt.2014.07.00110.1016/j.jmrt.2014.07.001 ↗
55. 10.1016/j.tsf.2015.11.07110.1016/j.tsf.2015.11.071 ↗
56. 10.1016/j.jallcom.2013.02.17210.1016/j.jallcom.2013.02.172 ↗
57. 10.1016/j.apsusc.2011.03.11310.1016/j.apsusc.2011.03.113 ↗
58. 10.1016/j.jallcom.2014.02.00310.1016/j.jallcom.2014.02.003 ↗
59. 10.1016/j.apsusc.2008.11.05110.1016/j.apsusc.2008.11.051 ↗
60. 10.1002/crat.20130021610.1002/crat.201300216 ↗
61. 10.1016/j.matlet.2015.02.05010.1016/j.matlet.2015.02.050 ↗
62. 10.1007/s10854-011-0323-z10.1007/s10854-011-0323-z ↗
63. 10.1007/s00339-009-5271-610.1007/s00339-009-5271-6 ↗
64. 10.3390/photonics908059410.3390/photonics9080594 ↗
65. 10.1016/j.molstruc.2023.13506310.1016/j.molstruc.2023.135063 ↗
66. 10.1007/s10854-015-2976-510.1007/s10854-015-2976-5 ↗
67. 10.1016/j.cap.2015.04.03510.1016/j.cap.2015.04.035 ↗
68. 10.1016/j.jmrt.2014.07.00110.1016/j.jmrt.2014.07.001 ↗
69. Gayen RN, Bhar R, Pal AK. Synthesis and characterization of vertically aligned ZnO NRs with controlled aspect ratio. Indian J Pure Appl Phys. 2010;48:385–393.
70. 10.1007/s10971-015-3646-z10.1007/s10971-015-3646-z ↗
71. 10.1016/j.jssc.2011.01.02110.1016/j.jssc.2011.01.021 ↗
72. 10.12691/jmpc-2-2-410.12691/jmpc-2-2-4 ↗
73. 10.7567/JJAP.55.01AE1510.7567/JJAP.55.01AE15 ↗
74. 10.1016/j.jpcs.2006.05.04810.1016/j.jpcs.2006.05.048 ↗
75. 10.1016/j.tsf.2009.11.08210.1016/j.tsf.2009.11.082 ↗
76. 10.1149/1.331610510.1149/1.3316105 ↗
77. Patil GR, Gaikwad RS, Shelar MB, et al. Role of concentration and temperature on well-aligned ZnO NR by low temperature wet chemical bath deposition method. Archiv Phys Res. 2012;3(5):401–406.
78. 10.1007/s10008-014-2737-z10.1007/s10008-014-2737-z ↗
79. 10.18502/keg.v1i1.50910.18502/keg.v1i1.509 ↗
80. 10.12691/jfnr-2-12-1310.12691/jfnr-2-12-13 ↗
81. 10.24271/psr.2022.343112.113610.24271/psr.2022.343112.1136 ↗
82. 10.1016/j.rinp.2013.01.00510.1016/j.rinp.2013.01.005 ↗
83. 10.1155/2013/79293010.1155/2013/792930 ↗