Effect of carbon contents and Ti addition on microstructure of ultralow carbon steel
Source abstract
Abstract
The microstructures of a series of ultralow carbon steels with various carbon contents (50–200 ppm) and Ti addition (<500 ppm) were studied by optical microscope, scanning electron microscope and transmission electron microscope. The specimens were fabricated under the process of hot rolling, cold rolling and two-step continuous annealing. The experimental results showed that the increase in carbon content decreased the grain size, whereas the addition of Ti resulted in a larger grain size compared with those without Ti addition. Dislocation (cell) structures were introduced by cold rolling, but it was removed by two-step annealing. Only MnS precipitated from the Ti free specimens. However, a larger amount of fine TiN, a few coarse TiS and an extremely low number of much coarser Ti3AlC were observed in the Ti added specimens. In addition, the reduction in MnS inclusion was obtained by the addition of Ti.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (8)
Show source-provided references
1. 10.1016/j.matchar.2005.11.01010.1016/j.matchar.2005.11.010 ↗
2. 10.1088/0370-1298/62/1/30810.1088/0370-1298/62/1/308 ↗
3. Seal RK: ‘New ultra-low carbon high strength steels with improved bake hardenability for enhanced stretch formability and dent resistance’, Master’s dissertation, Indian Institute of Technology, Bombay, India, 2006.
4. 10.1016/j.msea.2006.10.10010.1016/j.msea.2006.10.100 ↗
5. Adebiyi DI · J. Appl. Sci. Res. · 2009 · 5 · 1344
6. 10.1016/j.actamat.2004.04.01910.1016/j.actamat.2004.04.019 ↗
7. 10.1361/10599499977034639610.1361/105994999770346396 ↗
8. 10.1016/j.actamat.2004.03.04610.1016/j.actamat.2004.03.046 ↗