Abstract Heat treatable aluminium alloys of the 6xxx series are widely used in the hood, trunk and roof sections of a car body as they offer better corrosion resistance, high strength to weight ratio and excellent weldability characteristics. Gas metal arc welding (GMAW), a high productivity process is extensively employed in the automobile sector due to its ease of automation. HAZ softening is one of the most common problems that occurs during the welding of aluminium alloys by GMAW because of its high heat input. Cold metal transfer (CMT) is the most suitable welding process for welding aluminium alloys especially for controlling HAZ softening issues that occur due to the low heat input involved in this process. However, softening continues to exist in the welded joints. In this investigation, Post -weld heat treatment (PWHT) was employed to increase joint efficiency and to minimize the HAZ softening of AA6061-T6 aluminum alloy joints welded by GMAW and CMT. The results show that the tensile strength of a post-weld heat treated CMT joint is 10 % higher i. e., 242 MPa (76 % of joint efficiency), than that of the as welded CMT joint. This is due to the nucleation of strengthening precipitates in the weld metal and heat affected zone regions.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Chidambaram , India
References (37)
Show source-provided references
1. Mechanisms controlling the artificial aging of Al-Mg-Si Alloys10.1016/j.actamat.2011.02.010 ↗
2. Quantitative evaluation of softened regions in weld heat-affected zones of 6061-T6 aluminum alloy – characterizing of the laser beam welding process10.1007/s11661-999-0022-z ↗
3. Recovery of mechanical properties of a 6061-T6 aluminum weld by heat treatment after welding10.1007/s11661-016-3483-x ↗
4. Effect of post weld heat treatment on properties of variable polarity TIG welded AA2219 aluminum alloy joints10.1016/S1003-6326(14)63193-9 ↗
5. The precipitation sequence in Al-Mg – Si alloys10.1016/S1359-6454(98)00059-7 ↗
6. Influences of post-weld heat treatment on tensile properties of friction stir-welded AA6061 aluminum alloy joints10.1016/j.matchar.2007.09.006 ↗
7. Effect of a post-weld heat treatment on the mechanical and microstructure properties of AA6061 joints welded by the gas metal arc welding cold metal transfer method10.1016/j.matdes.2011.06.007 ↗
8. Microstructure and mechanical property change during FSW and GTAW of Al6061 alloy10.1007/s11661-012-1588-4 ↗
9. Effect of post weld heat treatment on microstructure and mechanical properties of gas tungsten arc welded AA6061-T6 alloy10.1016/S1003-6326(16)64442-4 ↗
10. The microstructure and mechanical strength of Al-6061-T6 GMA welds obtained with the modified indirect electric arc joint10.1016/j.matdes.2009.12.017 ↗
11. Effects of heat treatments on the microstructure and mechanical properties of a 6061 aluminum alloy10.1016/j.msea.2010.12.011 ↗
12. Effect of heat treatment on microstructure and corrosion behavior of Al6061 alloy weldment10.1016/j.matdes.2009.12.001 ↗
13. Analysis of heat input effect on the mechanical properties of Al-6061-T6 alloy weld joints10.1016/j.matdes.2013.05.081 ↗
14. Effect of TIG current on microstructural and mechanical properties of 6061-T6 aluminum alloy joints by TIG–CMT hybrid welding10.1016/j.jmatprotec.2017.12.006 ↗
15. Microstructure and hardness of Al-Mg-Si weldments produced by pulse GTA welding10.1007/s00170-006-0849-z ↗
16. Softening behaviour of Al–Zn–Mg alloys due to welding10.1016/S0921-5093(99)00020-9 ↗
17. Influences of pulsed current welding and post weld aging treatment on fatigue crack growth behaviour of AA7075 aluminum alloy joints10.1016/j.ijfatigue.2007.04.012 ↗
18. Microstructure and mechanical properties of AA7075(T6) hybrid laser/GMA welds10.1016/j.msea.2006.12.094 ↗
19. Temperature evolution, microstructure and mechanical properties of friction stir welded thick 2219-O aluminum alloy joints10.1016/j.matdes.2008.09.021 ↗
20. The study of MIG weldability of heat-treated aluminum alloys10.1007/s00170-012-4462-z ↗
21. Post-weld residual stresses and heat treatments of gas tungsten arc welded aluminum alloy AA6061-T65110.1260/1708-5284.10.1.11 ↗
22. Influence of the thermal route on the peak-aged microstructures in an Al-Mg-Si aluminum alloy10.1016/j.scriptamat.2012.10.006 ↗
23. Comparative experimental study on the modification of microstructural and mechanical properties of friction stir welded and gas metal arc welded EN AW-6061 O aluminum alloys by post-weld heat treatment10.1002/mawe.201700137 ↗
24. Effect of PWHT on behaviors of precipitates and hardness distribution of 6061 Al alloy joints by friction stir welding method10.4028/www.scientific.net/MSF.449-452.601 ↗
25. CO2 laser beam welding of 6061-T6 aluminum alloy thin plate10.1007/s11661-997-0022-9 ↗
26. Microstructure, mechanical and corrosion behavior of high strength AA7075 aluminum alloy friction stir welds – Effect of post weld heat treatment10.1016/j.dt.2015.04.003 ↗
27. Post-weld heat treatment effects on hardness and impact strength of aluminum alloy 6061 friction stir butt weld10.2320/matertrans.M2015074 ↗
28. The effect of post weld heat treatment on the properties of 6061 friction stir welded joints10.1023/A:1013701104029 ↗
29. Investigation into the influence of post-weld heat treatment on the friction stir welded AA6061 Al-Alloy plates with different temper conditions10.1007/s11661-013-2026-y ↗
30. Effect of post weld heat treatment on the 6061 aluminum alloy produced by ultrasonic additive manufacturing10.1016/j.msea.2016.12.083 ↗
31. Effect of pulsed current and post weld aging treatment on tensile properties of argon arc welded high strength aluminum alloy10.1016/j.msea.2006.12.125 ↗
32. Effect of post weld heat treatment on the microstructure and tensile properties of dissimilar friction stir welded {AA2219 and AA 6061} alloys10.1007/s12666-009-0002-4 ↗
33. Influences of welding processes and post-weld ageing treatment on mechanical and metallurgical properties of AA2219 aluminum alloy joints10.1007/BF03321386 ↗
34. Influence of aging conditions on the microstructure and tensile strength of aluminum alloy 606310.4028/www.scientific.net/MSF.396-402.1211 ↗
35. Studies on softening of heat-affected zone of pulsed-current GMA welded Al-Zn-Mg alloy10.1016/j.jmatprotec.2006.06.008 ↗
36. Effects of aging treatment and heat input on the microstructures and mechanical properties of TIG-welded 6061-T6 alloy joints, International Journal of Minerals10.1007/s12613-013-0721-8 ↗
37. Post-phases and their influence on microstructure and hardness in 6xxx Al-Mg-Si alloys10.1007/s10853-005-2470-1 ↗