journal article·2014-04-01

Mechanical Performance of Polyamid 66 and Influence of Glass Fiber Content on Moisture Absorption

Sami Sayer

Materials Testing· Volume 56· Issue 4
Publisher page

Abstract

Abstract This study investigates the determination of the mechanical performance of polyamid 66 and the influence of moisture and short glass fiber content (15 wt.-% and 30 wt.-%) at six different conditioning times (1, 2, 4, 8, 16, 32 minutes) in 105 °C water vapor. It was determined that as the glass fiber content increases, moisture absorption decreases. While the moisture absorption increases, tensile strength decreases and the percental elongation and toughness increases. It can also be derived that continuation of moisture absorption after 16 minutes is not effective and beneficial. The moisture absorption values observed in this study are equivalent to the amount of moisture that can be absorbed at 50 % relative humidity and 23 °C room temperature in the air for four months.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Natural Fiber Reinforced Composites · Mechanical Behavior of Composites · Structural Analysis of Composite Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Izmir , Turkey

References (27)

Show source-provided references
1. 2003
2. The influence of fiber length, diameter and concentration on the modulus of glass fiber-reinforced polyamide 66, Composites Part A
3. Mechanism of fracture of short glass fiber-reinforced polyamide thermoplastic10.1007/BF01120023 ↗
4. Tensile, impact and fiber length properties of injection-molded short and long glass fiber-reinforced polyamide composites10.1177/0731684404033960 ↗
5. Nylon under the hood: History of innovation
6. 2011 · 500
7. Effect of water absorption in polymers at low and high temperatures10.1016/S0032-3861(98)00560-6 ↗
8. 1997
9. 2006
10. 722
11. The durability of epoxies10.1080/03602557808055845 ↗
12. Thermal spike enhanced moisture absorption by polymer matrix, carbon fiber composites10.1016/S0266-3538(96)00168-6 ↗
13. The effect of water on the glass transition temperature of poly(methyl methacrylate)10.1016/0032-3861(88)90405-3 ↗
14. Effect of absorbed water, temperature and strain rate on the yield strength of two methyl methacrylate-based plastic10.1007/BF02385402 ↗
15. Influence of moisture on impact fracture behaviour of polymers as exemplified by polyamid 66
16. The hygrothermal behavior of glass fiber-reinforced PA66 composites: A study of the effect of water absorption on their mechanical properties10.1007/BF01160550 ↗
17. Moisture absorption and its influence on the tensile properties of glass fiber-reinforced polyamide 6610.1177/096739119400200601 ↗
18. 1999
19. 2006
20. Ford's Prototype Electric Ka
21. 1989
22. Characterization by means of a finite element model of the influence of moisture content on the mechanical and fracture properties of the polyamide 6 reinforced with short glass fiber10.1016/j.polymertesting.2011.03.001 ↗
23. 1975
24. 1992
25. CAMPUS® 5.0 data base, BASF-2004-05-24
26. 2007
27. Moisture absorption in polyamide-6 silicate nanocomposites and its influence on the mechanical properties10.1016/j.polymer.2005.10.096 ↗