journal article·2023-06-27

Wear properties of borided WC-Co

Tuna Aydogmus, Derya Peker, Polat Topuz

Materials Testing· Volume 65· Issue 6
Publisher page

Abstract

Abstract Today, artificially produced tungsten carbide (WC) tools are used as an alternative to diamonds such as mining, drilling, cutting, or machining. Although it is called WC, it also contains a certain amount of cobalt (Co). The most important reason for this is that it increases the wear resistance of the WC. Boriding is a type of surface hardening method that provides wear, hardness, and corrosion resistance to the applied surface. In boriding, which is a kind of diffusion process, there is no change in the dimensions of the materials since the boride layer grows from the outer surface of the materials to the inside. In this study, the development of surface properties by boriding of 90 wt% WC and 10 wt% Co-containing abrasive bits used for drilling were investigated. The samples were borided in an atmosphere-controlled furnace at 1173, 1273, and 1373 K for 1, 2, and 3 h by the pack boriding method. After the boriding processes, the microstructure, hardness, and chemical composition of the boride layers formed on the surface of the samples were examined, and finally, the wear tests were carried out to reveal the differences compared to the unborided sample.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Technical Sciences Vocational School , Hitit Universitesi , Corum , 19019 , Türkiye

Faculty of Arts and Sciences, Physic Department , Eskişehir Osmangazi Üniversitesi , Eskisehir , Türkiye

Vocational School , İstanbul Gedik University , Gedik Meslek Yüksekokulu, Sülüntepe Mh. Yunus Emre Cd. No: 1/1 Şeyhli, Pendik , Istanbul , 34876 , Türkiye

References (28)

Show source-provided references
1. Y. Yang, C. Zhang, D. Wang, L. Nie, D. Wellman, and Y. Tian, “Additive manufacturing of WC-Co hard metals: a review,” Int. J. Adv. Des. Manuf. Technol., vol. 108, pp. 1653–1673, 2020, https://doi.org/10.1007/s00170-020-05389-5.10.1007/s00170-020-05389-5 ↗
2. G. S. Upadhyaya, Cemented Tungsten Carbides: Production, Properties and Testing, Westwood, NJ, USA, Noyes Publications, 1998.10.1016/B978-081551417-6.50019-8 ↗
3. H. M. T. Bangalore, Production Technology, Gautam Buddha Nagar, Uttar Pradesh, India, Tata McGraw-Hill Education, 2001.
4. K. J. A. Brookes, “Fine-structured hard metals and grain-growth inhibitor,” Met. Powder Rep., vol. 71, no. 2, pp. 92–99, 2016, https://doi.org/10.1016/j.mprp.2015.10.076.10.1016/j.mprp.2015.10.076 ↗
5. B. Vasyliv, A. Ivasyshyn, and O. Ostash, “Effect of corrosion environment on the fatigue behavior of WC-Co hard alloy teeth of drill bits,” in Innovative Superhard Materials and Sustainable Coatings for Advanced Manufacturing, Springer Science & Business Media, vol. 200, 2005, pp. 469–475.10.1007/1-4020-3471-7_40 ↗
6. Available at: https://www.boartlongyear.com/insite/check-your-buttons-proven-tips-for-more-meters-per-bit/ [accessed: Jan. 12, 2022].
7. J. A. M. Ferreira, M. A. P. Amaral, F. V. Antunes, and J. D. M. Costa, “A study on the mechanical behavior of WC/Co hardmetals,” Int. J. Refract. Metals Hard Mater., vol. 27, no. 1, pp. 1–8, 2009, https://doi.org/10.1016/j.ijrmhm.2008.01.013.10.1016/j.ijrmhm.2008.01.013 ↗
8. P. Topuz, E. Gündoğdu İş, and E. Yılmaz, “Kinetic investigations of boronized cold work tool steels,” Mater. Test., vol. 56, no. 2, pp. 104–110, 2014, https://doi.org/10.3139/120.110531.10.3139/120.110531 ↗
9. N. Orlovskaya and M. Lugovy, Boron Rich Solids: Sensors, Ultra High-Temperature Ceramics, Thermoelectrics, Armor, Orlando, Florida, USA, Springer Science & Business Media, 2010.10.1007/978-90-481-9818-4 ↗
10. R. Beatty, “The Elements,” in Boron, New York, 99 White Plains Road, Tarrytown, USA, Marshall Cavendish Benchmark, 2005, pp. 4–7.
11. Ş. G. Alpaydin and Y. Y. Aksoy, “The effects of colemanite and ulexite additives on the geotechnical index properties of bentonite and sand-bentonite mixtures,” in Proceedings of China-Europe Conference on Geotechnical Engineering, 2018, pp. 778–781.10.1007/978-3-319-97112-4_174 ↗
12. A. K. Sinha, “Boriding (boronizing),” in ASM Handbook, Heat Treating Vol. 4, USA, ASM International, Materials Park OH., 1991.
13. C. Zimmerman, “Boriding (boronizing) of metals,” in ASM Handbook, Vol. 4A: Steel Heat Treating Fundamentals and Processes, J. L. Dossett and G. E. Totten, Eds., USA, ASM International, Materials Park OH., 2013.10.31399/asm.hb.v04a.a0005772 ↗
14. T. S. Kim, J. H. Yeo, K. B. Nam, M. J. Kim, and J. M. Yoo, “Boron carbide coating to improve the chemical stability of nm-thick graphite films,” Thin Solid Films, vol. 704, p. 138002, 2020, https://doi.org/10.1016/j.tsf.2020.138002.10.1016/j.tsf.2020.138002 ↗
15. N. E. Maragoudakis, G. Stergioudis, H. Omar, E. Pavlidou, and D. N. Tsipas, “Boro-nitriding of steel US 37-1,” Mater. Lett., vol. 57, no. 4, pp. 949–952, 2002, https://doi.org/10.1016/S0167-577X(02)00902-3.10.1016/S0167-577X(02)00902-3 ↗
16. M. A. Béjar, E. Moreno, “Abrasive wear resistance of boronized carbon and low-alloy steels,” J. Mater. Process. Technol. vol. 173, no. 3, pp. 352–358, 2006, https://doi.org/10.1016/j.jmatprotec.2005.12.006.10.1016/j.jmatprotec.2005.12.006 ↗
17. R. H. Biddulph, “Boronizing for erosion resistance,” Thin Solid Films, vol. 45, pp. 341–347, 1977, https://doi.org/10.1016/0040-6090(77)90267-X.10.1016/0040-6090(77)90267-X ↗
18. P. Topuz, E. G. İş, E. Gümüş, and E. Gümüş, “The fracture toughness of Fe2B formed on boronized AISI 304 stainless steel,” Mater. Test., vol. 56, no. 9, pp. 690–693, 2014, https://doi.org/10.3139/120.110621.10.3139/120.110621 ↗
19. M. Kulka, “Trends in thermochemical techniques of boriding,” in Current Trends in Boriding, Engineering Materials, Cham, Springer, 2019.10.1007/978-3-030-06782-3 ↗
20. R. J. Fischer, “Thermochemical treatment in powdered media,” in Proceedings of the Eighth International Conference on Chemical Vapor Deposition, J. M. Blocher, V. E. Guy, and G. Wahl, Eds., USA, Electrochemical Society, 1981, pp. 509–510.
21. D. Tkalich, V. Yastrebov, G. Cailletaud, and A. Kane, “Multiscale modeling of cemented tungsten carbide in hard rock drilling,” Int. J. Solids Struct., vol. 128, pp. 282–295, 2017, https://doi.org/10.1016/j.ijsolstr.2017.08.034.10.1016/j.ijsolstr.2017.08.034 ↗
22. W. J. Wolfgong, A. S. H. Makhlouf, and M. Aliofkhazraei, “Chemical analysis techniques for failure analysis: chapter 14, Part 1, common instrumental methods,” in Handbook of Materials Failure Analysis with Case Studies from the Aerospace and Automotive Industries, A. S. H. Makhlouf and M. Aliofkhazraei, Eds., Butterworth-Heinemann, 2016, pp. 279–307.
23. Available at: http://www.metallographic.com/Etchants/Etchants.htm [accessed: Jan. 13, 2021].
24. G. Voort, E. Manilova, and J. Michael, “A study of selective etching of carbides in steel,” Microsc. Microanal., vol. 10, no. S02, pp. 1–5, 2004. https://doi.org/10.1017/S1431927604883375.10.1017/S1431927604883375 ↗
25. E. N. Avdeenko, E. I. Zamulaeva, A. A. Zaitsev, I. Y. Konyashin, and E. A. Levashov, “Structure and properties of coarse-grained WC–Co alloys with an especially homogeneous microstructure,” Russ. J. Non-Ferrous Metals, vol. 60, pp. 542–548, 2019, https://doi.org/10.3103/S1067821219050055.10.3103/S1067821219050055 ↗
26. Available at: https://www.destinytool.com/carbide-substrate.html [accessed: Oct. 08, 2020].
27. P. Topuz, “Development of boronizing parameters and boronizing of different steels in fluidized bed furnace,” Ph.D. thesis, Institute of Science, Marmara University, İstanbul, Turkey, 2009.
28. Ö. Aydın, P. Topuz, and T. Aydoğmuş, “Kinetic characterization of boride layers formed on AISI 316 stainless steel,” Mater. Test., vol. 62, no. 6, pp. 652–656, 2020, https://doi.org/10.3139/120.111530.10.3139/120.111530 ↗