Effect of austempering on wear resistance of GGG50 nodular cast iron
Source abstract
Abstract
Abstract In this research, nodular cast iron (GGG50) with 0.2 wt.% Cr and 0.8 wt.% Mo was subjected to austenization at 900, and 950 °C for 45 min, and 1 h. Then, austempering was performed at 200, 250, 300, 350 and 400 °C for periods of 30–720 min. The microstructure of the austempered samples at varying temperatures was defined using an optical and scanning electron microscope. Phases and compounds were analyzed through X-ray diffraction. Hardness tests were conducted on the samples. Wear performances were assessed using a pin-on-disc wear apparatus. The friction coefficients of the materials were detected. The worn surfaces of the samples were examined by scanning electron microscope (SEM). The microstructure of the casting was comprised of ferrite and pearlite. In contrast, the annealed sample contained a blend of acicular ferrite and carbon-enriched annealed iron, referred to as “ausferrite.” As the austempering temperature increased, the structure became coarser and the hardness values declined. As the annealing temperature increased, wear resistance was observed to decrease. The coefficient of friction diminished as the austempering temperature raised.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Tribology and Wear Analysis · Advanced machining processes and optimization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Tekirdağ Namık Kemal University , Faculty of Engineering , Department of Mechanical Engineering , Corlu , Tekirdağ 59160 , Türkiye
Sivas Cumhuriyet University , Faculty of Technology , Department of Manufacturing Engineering , Sivas , Türkiye
References (24)
Show source-provided references
1. S. Panneerselvam, C. J. Martis, S. K. Putatunda, and J. M. Boileau, “An investigation on the stability of austenite in austempered ductile cast iron (ADI),” Mater. Sci. Eng. A, vol. 626, pp. 237–246, 2015, https://doi.org/10.1016/j.msea.2014.12.038.10.1016/j.msea.2014.12.038 ↗
2. S. K. Putatunda, “Development of austempered ductile cast iron (ADI) with simultaneous high yield strength and fracture toughness by a novel two-step austempering process,” Mater. Sci. Eng. A, vol. 315, nos. 1–2, pp. 70–80, 2001, https://doi.org/10.1016/S0921-5093(01)01210-2.10.1016/S0921-5093(01)01210-2 ↗
3. N. Zhang, J. Zhang, L. Lu, M. Zhang, D. Zeng, and Q. Song, “Wear and friction behavior of austempered ductile iron as railway wheel material,” Mater. Des., vol. 89, pp. 815–822, 2016, https://doi.org/10.1016/j.matdes.2015.10.037.10.1016/j.matdes.2015.10.037 ↗
4. P. P. Rao and S. K. Putatunda, “Investigations on the fracture toughness of austempered ductile irons austenitized at different temperatures,” Mater. Sci. Eng. A, vol. 349, nos. 1–2, pp. 136–149, 2003, https://doi.org/10.1016/S0921-5093(02)00633-0.10.1016/S0921-5093(02)00633-0 ↗
5. O. Erić, M. Jovanović, L. Šid, D. Rajnović, and S. Zec, “The austempering study of alloyed ductile iron,” Mater. Des., vol. 27, no. 7, pp. 617–622, 2006, https://doi.org/10.1016/j.matdes.2004.11.028.10.1016/j.matdes.2004.11.028 ↗
6. M. H. Sohi, M. N. Ahmadabadi, and A. B. Vahdat, “The role of austempering parameters on the structure and mechanical properties of heavy section ADI,” J. Mater. Process. Technol., vols. 153–154, pp. 203–208, 2004, https://doi.org/10.1016/j.jmatprotec.2004.04.308.10.1016/j.jmatprotec.2004.04.308 ↗
7. X. Chen, et al., “Effects of niobium alloying on microstructure, toughness and wear resistance of austempered ductile iron,” Mater. Sci. Eng. A, vol. 760, pp. 186–194, 2019, https://doi.org/10.1016/j.msea.2019.05.100.10.1016/j.msea.2019.05.100 ↗
8. Y. J. Kim, H. Shin, H. Park, and J. D. Lim, “Investigation into mechanical properties of austempered ductile cast iron (ADI) in accordance with austempering temperature,” Mater. Lett., vol. 62, no. 3, pp. 357–360, 2008, https://doi.org/10.1016/j.matlet.2007.05.028.10.1016/j.matlet.2007.05.028 ↗
9. L. F. V. Guerra, A. B. Jacuinde, I. Mejia, J. Zuno, and C. Maldonado, “Effects of boron addition and austempering time on microstructure, hardness, and tensile properties of ductile irons,” Mater. Sci. Eng. A, vol. 648, pp. 193–201, 2015, https://doi.org/10.1016/j.msea.2015.09.066.10.1016/j.msea.2015.09.066 ↗
10. J. Cui and L. Chen, “Microstructure and abrasive wear resistance of an alloyed ductile iron subjected to deep cryogenic and austempering treatments,” J. Mater. Sci. Technol., vol. 33, no. 12, pp. 1549–1554, 2017, https://doi.org/10.1016/j.jmst.2017.08.003.10.1016/j.jmst.2017.08.003 ↗
11. Y. Zhu, J. Chen, J. Du, Y. Fan, and J. Zheng, “Tribological behavior of laser textured nodular cast iron surface,” Ind. Lubr. Tribol., vol. 71, no. 7, pp. 949–955, 2019, https://doi.org/10.1108/ILT-08-2018-0327.10.1108/ILT-08-2018-0327 ↗
12. J. F. Dias, G. O. Ribeiro, D. J. Carmo, and J. J. Vilela, “The effect of reducing the austempering time on the fatigue properties of austempered ductile iron,” Mater. Sci. Eng. A, vol. 556, pp. 408–413, 2012, https://doi.org/10.1016/j.msea.2012.07.005.10.1016/j.msea.2012.07.005 ↗
13. S. Panneerselvam, S. K. Putatunda, R. Gundlach, and J. Boileau, “Influence of intercritical austempering on the microstructure and mechanical properties of austempered ductile cast iron (ADI),” Mater. Sci. Eng. A, vol. 694, pp. 72–80, 2017, https://doi.org/10.1016/j.msea.2017.03.096.10.1016/j.msea.2017.03.096 ↗
14. T. Teker, S. O. Yilmaz, and E. Bulus, “Influence of austempering temperatures on microstructure and wear performance of solution strengthened ferritic ductile irons,” Pract. Metallogr., vol. 61, no. 6, pp. 356–369, 2024, https://doi.org/10.1515/pm-2022-1031.10.1515/pm-2022-1031 ↗
15. S. O. Yilmaz, T. Teker, and B. Atik, “Improved Gx40CrNi25-20 grade austenitic stainless steel,” Mater. Test, vol. 66, no. 4, pp. 493–502, 2024, https://doi.org/10.1515/mt-2023-0366.10.1515/mt-2023-0366 ↗
16. B. Wang, G. C. Barber, F. Qiu, Q. Zou, and H. Yang, “A review: phase transformation and wear mechanisms of single-step and dual-step austempered ductile irons,” J. Mater. Res. Technol., vol. 9, no. 1, pp. 1054–1069, 2020, https://doi.org/10.1016/j.jmrt.2019.10.074.10.1016/j.jmrt.2019.10.074 ↗
17. R. Upadhyaya, K. K. Singh, R. Kumar, and M. S. Chandran, “Study on the effect of austempering temperature on the structure-properties of thin wall austempered ductile iron,” Mater. Today: Proc., vol. 5, no. 5, pp. 13472–13477, 2018, https://doi.org/10.1016/j.matpr.2018.02.342.10.1016/j.matpr.2018.02.342 ↗
18. T. Teker and S. O. Yilmaz, “Investigation on mechanical properties of austempered and solution strengthened ferritic ductile irons,” Int. J. Mater. Res., vol. 111, no. 12, pp. 976–982, 2020, https://doi.org/10.3139/146.111963.10.3139/146.111963 ↗
19. T. Teker, S. O. Yilmaz, and S. Ö. Eruslu, “Effect of austempering treatment on metallurgical structure of Ce inoculated X210Cr12 cold work tool steel,” Mater. Test, vol. 64, no. 1, pp. 78–87, 2022, https://doi.org/10.1515/mt-2021-2014.10.1515/mt-2021-2014 ↗
20. H. Zhang, Y. Wu, Q. Li, and X. Hong, “Mechanical properties and rolling-sliding wear performance of dual phase austempered ductile iron as potential metro wheel material,” Wear, vols. 406–407, pp. 156–165, 2018, https://doi.org/10.1016/j.wear.2018.04.005.10.1016/j.wear.2018.04.005 ↗
21. J. Zimba, M. Samandi, D. Yu, T. Chandra, E. Navara, and D. J. Simbi, “Un-lubricated sliding wear performance of unalloyed austempered ductile iron under high contact stresses,” Mater. Des., vol. 25, no. 5, pp. 431–438, 2004, https://doi.org/10.1016/j.matdes.2003.11.004.10.1016/j.matdes.2003.11.004 ↗
22. K. H. S. Silva, J. R. Carneiro, R. S. Coelho, H. Pinto, and P. Brito, “Influence of shot peening on residual stresses and tribological behavior of cast and austempered ductile iron,” Wear, vols. 440–441, p. 203099, 2019, https://doi.org/10.1016/j.wear.2019.203099.10.1016/j.wear.2019.203099 ↗
23. B. Wang, M. He, G. C. Barber, J. D. Schall, C. Tao, and X. Sun, “Rolling contact fatigue resistance of austempered ductile iron processed at various austempering holding times,” Wear, vol. 398, no. 399, pp. 41–46, 2018, https://doi.org/10.1016/j.wear.2017.11.022.10.1016/j.wear.2017.11.022 ↗
24. T. Engelke and A. Esderts, “Analytical strength assessments of austempered ductile iron components,” Mater. Test, vol. 60, no. 10, pp. 940–944, 2018, https://doi.org/10.3139/120.111235.10.3139/120.111235 ↗