journal article·2015-04-30

Influence of the heat treatment on hardness and adhesive wear performance of Ni-P deposit with low phosphorus content

Ulaş Matki, Ramazan Çıtak

Materials Testing· Volume 57· Issue 5
Publisher page

Abstract

Abstract A Ni-P coating with low phosphorus content has been deposited onto an AISI 1020 plain carbon steel. The effect of temperature on the structure of coating was determined by DSC and XRD analysis. To determine the effect of heat treatment on the hardness and wear properties, some of the coated specimens were heat treated at different temperatures as isothermal for 1 h. Pin-on-disc wear tests were carried out on the specimens under loads of 20, 40 and 60 N, respectively. It has been determined that hardness and wear resistance of electroless Ni-P coating increased with the heat treatment. Maximum hardness and wear resistance were obtained for samples heat treated at 400 °C.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Semiconductor materials and interfaces · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Karabük

Ankara , Turkey

References (21)

Show source-provided references
1. 2011
2. The influence of thermal treatment on the microstructure and hardness in electroless Ni–P–W deposit, Thin Solid Films · 2004 · 469–470 · 33310.1016/j.tsf.2004.08.146 ↗
3. Influence of acidic and alkali electroless nickel coating solutions on coating quality of iron based parts produced by powder metallurgy
4. Effect of coating time and heat treatment on structures and corrosion characteristics of electroless Ni-P alloy deposits10.1016/S0257-8972(03)00746-1 ↗
5. Peak-profile analysis of electroless nickel coatings10.1016/S0925-8388(00)01099-9 ↗
6. Crystallization temperature of amorphous electroless nickel–phosphorus alloys10.1016/j.matlet.2004.11.064 ↗
7. Crystallisation kinetics and phase transformation behaviour of electroless nickel–phosphorus deposits with high phosphorus content”10.1016/S0925-8388(01)01798-4 ↗
8. Mechanically assisted electroless barrel-plating Ni-P coatings deposited on carbon steel, J10.1016/S1005-0302(10)60153-3 ↗
9. Hardness evolution of electroless nickel-phosphorus deposits with thermal processing10.1016/S0257-8972(03)00209-3 ↗
10. Crystallisation and phase transformation behaviour of electroless nickel phosphorus platings during continuous heating, Journal of Alloys and Compounds, Volume 358, Issues · 2003 · 1–2 · 11210.1016/S0925-8388(03)00069-0 ↗
12. Crystallization and phase transformation behaviour of electroless nickel-phosphorus deposits with low and medium phosphorus contents under continuous heating10.1023/A:1020641611389 ↗
13. Nanocrystalline Ni-3.6 at.% P and its transformation sequence studied by atom-probe field-ion microscopy10.1016/S1359-6454(99)00371-7 ↗
14. Thermal stability of electroless NiMeP amorphous alloys10.1007/BF02652965 ↗
15. Hardness evolution of electroless nickel-phosphorus deposits with thermal processing10.1016/S0257-8972(03)00209-3 ↗
16. Tribological properties of heat-treated electroless Ni-P coatings on AZ91 alloy10.1016/j.apsusc.2011.06.119 ↗
17. High temperature wear of an electroless Ni-P-BN (h) composite coating, Surface and Coatings Technology · 2003 · 163–164 · 57810.1016/S0257-8972(02)00663-1 ↗
18. 2008 · 620
19. Wear performance and mechanism of electroless Ni-P coating, Surface and Coatings Technology · 1996 · 86–87 · 59810.1016/S0257-8972(96)03086-1 ↗
20. The tribological characteristics of electroless NiP coatings10.1016/S0043-1648(01)00539-7 ↗
21. 2006 · 29