journal article·2026-03-26

Effects of hydrogen absorption on the mechanical and fatigue strength of high-strength bolts for a propulsion motor

Changwan Han, Jaehyeok Doh

Materials Testing· Volume 68· Issue 3
Publisher page

Abstract

Abstract This study examined the effects of hydrogen-related degradation on the static and dynamic fatigue strength of high-strength bolts for propulsion motors during electro-galvanization. Two-bolt types were prepared with different baking treatments: B 0h (no baking) and B 8h (baking at 200 °C for 8 h). Baking did not significantly affect the mechanical strength ( p < 0.01) but did increase the elongation of B 8h by 25.3 %. In high-cycle fatigue tests, B 8h exhibited a fatigue life of up to 6.3 times longer than that of B 0h . These results indicate that baking effectively mitigates hydrogen-related degradation and enhances the high-cycle fatigue life, ductility, and toughness of electro-galvanized 42CrMo4 steel bolts.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Combustion and Detonation Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Mobility Design Engineering , Gyeongkuk National University , Gyeongsangbuk-do , South Korea

School of Aerospace Engineering , College of Space and Aerospace, Gyeongsang National University , Gyeongsangnam-do , South Korea

References (31)

Show source-provided references
1. Y. Wang et al.., “Mechanical behavior of high-strength bolted joints fabricated from fire-resistant steel at elevated temperatures,” Adv. Mater. Sci. Eng., vol. 2022, no. 1, p. 8265019, 2022, https://doi.org/10.1155/2022/8265019.10.1155/2022/8265019 ↗
2. J. Chakhari, A. Daidié, Z. Chaib, and J. Guillot, “Numerical model for two-bolted joints subjected to compressive loading,” Finite Elem. Anal. Des., vol. 44, no. 4, pp. 162–173, 2008, https://doi.org/10.1016/j.finel.2007.11.010.10.1016/j.finel.2007.11.010 ↗
3. N. Garipova, C. Batigün, and C. H. Gür, “Numerical and experimental determination of the residual stress state in multipass welded API 5L X70 plates,” Mater. Test., vol. 56, no. 10, pp. 831–836, 2014, https://doi.org/10.3139/120.110637.10.3139/120.110637 ↗
4. S. Gündüz, H. Karabulut, M. A. Erden, and M. Türkmen, “Microstructural effects on fatigue behaviour of a forged medium carbon microalloyed steel,” Mater. Test., vol. 55, nos. 11–12, pp. 865–870, 2013, https://doi.org/10.3139/120.110511.10.3139/120.110511 ↗
5. X. Shen, L. Lu, and D. Zeng, “Fatigue failure analysis of high strength bolts used for high-speed railway vehicle braking discs,” Eng. Fail. Anal., vol. 115, p. 104661, 2020, https://doi.org/10.1016/j.engfailanal.2020.104661.10.1016/j.engfailanal.2020.104661 ↗
6. F. Tan, D. Xuan, Z. Zheng, P. Zhang, and H. Shen, “Experimental study on fatigue performance of high strength bolts of rail vehicles under axial alternating load,” IOP Conf. Ser.: Earth Environ. Sci., vol. 714, no. 3, p. 032055, 2021, https://doi.org/10.1088/1755-1315/714/3/032055.10.1088/1755-1315/714/3/032055 ↗
7. B. H. Choe et al.., “Hydrogen induced crack propagation in bainitic X70 steel in hydrogen pressured tensile test,” Korean J. Met. Mater., vol. 56, no. 1, pp. 1–7, 2018, https://doi.org/10.3365/KJMM.2018.56.1.1.10.3365/KJMM.2018.56.1.1 ↗
8. E. H. Hwang, H. G. Seong, and S. J. Kim, “Effect of carbon contents on corrosion and hydrogen diffusion behaviors of ultra-strong steels for automotive applications,” Korean J. Met. Mater., vol. 56, no. 8, pp. 570–579, 2018, https://doi.org/10.3365/KJMM.2018.56.8.570.10.3365/KJMM.2018.56.8.570 ↗
9. S. I. Lee et al.., “Tensile and fracture behaviors of austenitic high-manganese steels subject to different hydrogen embrittlement test methods,” Mater. Sci. Eng. A, vol. 766, p. 138367, 2019, https://doi.org/10.1016/j.msea.2019.138367.10.1016/j.msea.2019.138367 ↗
10. I. Yoo, J. M. Lee, H. S. Lim, J. Y. Suh, J. Lee, and B. Hwang, “Comparative study of hydrogen embrittlement of three heat-resistant Cr–Mo steels subjected to electrochemical and gaseous hydrogen charging,” Metall. Mater. Trans. A, vol. 51, no. 5, pp. 2118–2125, 2020, https://doi.org/10.1007/s11661-020-05704-5.10.1007/s11661-020-05704-5 ↗
11. D. H. Shim, T. Lee, J. Lee, H. J. Lee, J. Y. Yoo, and C. S. Lee, “Increased resistance to hydrogen embrittlement in high-strength steels composed of granular bainite,” Mater. Sci. Eng. A, vol. 700, pp. 473–480, 2017, https://doi.org/10.1016/j.msea.2017.06.043.10.1016/j.msea.2017.06.043 ↗
12. S. Brahimi, K. Sriraman, and S. Yue, “Hydrogen embrittlement characteristics of two tempered martensitic steel alloys for high-strength bolting,” Proc. Inst. Mech. Eng. Part C J. Mech. Eng. Sci., vol. 231, no. 17, pp. 3214–3227, 2017, https://doi.org/10.1177/0954406216642476.10.1177/0954406216642476 ↗
13. S. V. Brahimi, S. Yue, and K. R. Sriraman, “Alloy and composition dependence of hydrogen embrittlement susceptibility in high-strength steel fasteners,” Philos. Trans. R. Soc. A, vol. 375, no. 2098, p. 20160407, 2017, https://doi.org/10.1098/rsta.2016.0407.10.1098/rsta.2016.0407 ↗
14. O. Barrera et al.., “Understanding and mitigating hydrogen embrittlement of steels: A review of experimental, modelling and design progress from atomistic to continuum,” J. Mater. Sci., vol. 53, no. 9, pp. 6251–6290, 2018, https://doi.org/10.1007/s10853-017-1978-5.10.1007/s10853-017-1978-5 ↗
15. K. Park, D. H. Cho, M. H. Park, and C. W. Yang, “Effects of molybdenum on HIC susceptibility in normalized pressure vessel steels for sour service applications,” Korean J. Met. Mater., vol. 57, no. 7, pp. 405–411, 2019, https://doi.org/10.3365/KJMM.2019.57.7.405.10.3365/KJMM.2019.57.7.405 ↗
16. T. Neeraj, R. Srinivasan, and J. Li, “Hydrogen embrittlement of ferritic steels: Observations on deformation microstructure, nanoscale dimples and failure by nanovoiding,” Acta Mater., vol. 60, no. 13, pp. 5160–5171, 2012, https://doi.org/10.1016/j.actamat.2012.06.014.10.1016/j.actamat.2012.06.014 ↗
17. E. Hillier and M. Robinson, “Hydrogen embrittlement of high strength steel electroplated with zinc–cobalt alloys,” Corros. Sci., vol. 46, no. 3, pp. 715–727, 2004, https://doi.org/10.1016/S0010-938X(03)00180-X.10.1016/S0010-938X(03)00180-X ↗
18. M. Nagumo, Fundamentals of Hydrogen Embrittlement, Tokyo, Japan, Springer, 2016.10.1007/978-981-10-0161-1 ↗
19. X. Wu, H. Zhang, M. Yang, W. Jia, Y. Qiu, and L. Lan, “From the perspective of new technology of blending hydrogen into natural gas pipelines transmission: Mechanism, experimental study, and suggestions for further work of hydrogen embrittlement in high-strength pipeline steels,” Int. J. Hydrogen Energy, vol. 47, no. 12, pp. 8071–8090, 2022, https://doi.org/10.1016/j.ijhydene.2021.12.108.10.1016/j.ijhydene.2021.12.108 ↗
20. H. F. Alesary et al.., “Influence of additives on the electrodeposition of zinc from a deep eutectic solvent,” Electrochim. Acta, vol. 304, pp. 118–130, 2019, https://doi.org/10.1016/j.electacta.2019.02.090.10.1016/j.electacta.2019.02.090 ↗
21. M. Hino, S. Mukai, T. Shimada, K. Okada, and K. Horikawa, “Effect of baking on hydrogen embrittlement for high strength steel treated with various zinc based electroplating from a sulfate bath,” Mater. Trans., vol. 61, no. 12, pp. 2302–2306, 2020, https://doi.org/10.2320/matertrans.MT-M2020245.10.2320/matertrans.MT-M2020245 ↗
22. F. M. Rivas-Esquivel, G. M. Brisard, R. Ortega-Borges, G. Trejo, and Y. Meas, “Zinc electrochemical deposition from ionic liquids and aqueous solutions onto indium tin oxide,” Int. J. Electrochem. Sci., vol. 12, no. 3, pp. 2026–2041, 2017, https://doi.org/10.20964/2017.03.58.10.20964/2017.03.58 ↗
23. S. Lynch, “Hydrogen embrittlement phenomena and mechanisms,” Corros. Rev., vol. 30, nos. 3–4, pp. 105–123, 2012, https://doi.org/10.1515/corrrev-2012-0502.10.1515/corrrev-2012-0502 ↗
24. Q. Liu and A. Atrens, “A critical review of the influence of hydrogen on the mechanical properties of medium-strength steels,” Corros. Rev., vol. 31, nos. 3–4, pp. 85–103, 2013, https://doi.org/10.1515/corrrev-2013-0023.10.1515/corrrev-2013-0023 ↗
25. S. Takagi, Y. Toji, M. Yoshino, and K. Hasegawa, “Hydrogen embrittlement resistance evaluation of ultra high strength steel sheets for automobiles,” ISIJ Int., vol. 52, no. 2, pp. 316–322, 2012, https://doi.org/10.2355/isijinternational.52.316.10.2355/isijinternational.52.316 ↗
26. M. Koyama et al.., “Hydrogen-assisted quasi-cleavage fracture in a single crystalline type 316 austenitic stainless steel,” Corros. Sci., vol. 75, pp. 345–353, 2013, https://doi.org/10.1016/j.corsci.2013.06.018.10.1016/j.corsci.2013.06.018 ↗
27. E. Akiyama and S. Matsuoka, “Hydrogen visualization in steels using Ag decoration method,” Mater. Trans., vol. 56, no. 6, pp. 793–797, 2015, https://doi.org/10.2320/matertrans.M2014431.10.2320/matertrans.M2014431 ↗
28. J. J. Venezuela, Q. Liu, M. Zhang, Q. Zhou, and A. Atrens, “A review of hydrogen embrittlement of martensitic advanced high-strength steels,” Corros. Rev., vol. 34, no. 3, pp. 153–186, 2016, https://doi.org/10.1515/corrrev-2016-0006.10.1515/corrrev-2016-0006 ↗
29. B. Meng et al.., “Hydrogen effects on X80 pipeline steel in high-pressure natural gas/hydrogen mixtures,” Int. J. Hydrogen Energy, vol. 42, no. 11, pp. 7404–7412, 2017, https://doi.org/10.1016/j.ijhydene.2016.05.145.10.1016/j.ijhydene.2016.05.145 ↗
30. J. Hack and G. Leverant, “The influence of microstructure on the susceptibility of titanium alloys to internal hydrogen embrittlement,” Metall. Trans. A, vol. 13, no. 10, pp. 1729–1738, 1982, https://doi.org/10.1007/BF02647828.10.1007/BF02647828 ↗
31. S. W. Ko, J. M. Lee, Y. N. Kwon, and B. Hwang, “Effect of annealing treatment on microstructure and hydrogen embrittlement of Ti-6Al-4V alloys subject to electrochemical hydrogen charging,” Trans. Mater. Process., vol. 29, no. 4, pp. 211–217, 2020, https://doi.org/10.5228/KSTP.2020.29.4.211.