Investigation of the hydrogen embrittlement susceptibility of steel components during thin-film hot-dip galvanizing
Source abstract
Abstract
Abstract With regard to the application of thin-film hot-dip galvanizing to a welded steel tube structure in vehicle construction, several test series were carried out to investigate the potential for hydrogen embrittlement caused by the pretreatment media used in the galvanizing process. Here, C-ring specimens were produced from the materials E355 and C75 in different tempering states, treated in a hydrochloric acid-based operational pickle, and then tested under constant strain rate or constant load. The results show that under the investigated pickling conditions, no hydrogen-induced embrittlement effect occurs up to a hardness of 470 HV in the case of material E355 and 500 HV in the case of material C75. Only in the case of 550 HV and 600 HV, both for C75, was a tendency to embrittlement observed; this effect was more pronounced after treatment with the freshly prepared pickle than in the operating pickles. The two test methods used showed consistent results.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
ZINQ Technologie GmbH , Gelsenkirchen , Germany
iChemAnalytics GmbH , Detmold , Germany
Mercedes-Benz AG , Sindelfingen , Germany
References (15)
Show source-provided references
1. DIN 50997, Zinc-aluminium Coatings Applied by Thin Film Galvanizing of Steel – Requirements and Testing, Berlin, Germany, Beuth, 2020, in German.
2. ASTM A1072/A1072M, Standard Specification for Zinc-5 % Aluminum (Hot-dip) Coatings on Iron and Steel Products, West Conshohocken, Pennsylvania, USA, ASTM International, 2015.
3. I. M. Robertson, P. Sofronis, A. Nagao, et al.., “Hydrogen embrittlement understood,” Metall. Mater. Trans. B, vol. 46, no. 6, pp. 1085–1103, 2015, https://doi.org/10.1007/s11663-015-0325-y.10.1007/s11663-015-0325-y ↗
4. S. Lynch, “Hydrogen embrittlement phenomena and mechanisms,” Corros. Rev., vol. 30, nos. 3–4, pp. 105–123, 2012, https://doi.org/10.1515/corrrev-2012-0502.10.1515/corrrev-2012-0502 ↗
5. T. Neeraj, R. Srinivasan, and J. Li, “Hydrogen embrittlement of ferritic steels: observations on deformation microstructure, nanoscale dimples and failure by nanovoiding,” Acta Mater., vol. 60, no. 8, pp. 5160–5171, 2012, https://doi.org/10.1016/j.actamat.2012.06.014.10.1016/j.actamat.2012.06.014 ↗
6. S. Serebrinsky, E. A. Carter, and M. Ortiz, “A quantum-mechanically informed continuum model of hydrogen embrittlement,” J. Mech. Phys. Solid., vol. 52, no. 10, pp. 2403–2430, 2004, https://doi.org/10.1016/j.jmps.2004.02.010.10.1016/j.jmps.2004.02.010 ↗
7. M. M. Hall, “Effect of variable stress intensity factor on hydrogen environment assisted cracking,” Metall. Mater. Trans. A, vol. 42, pp. 304–318, 2011, https://doi.org/10.1007/s11661-010-0226-2.10.1007/s11661-010-0226-2 ↗
8. H. Yu, J. S. Olsen, A. Alvaro, V. Olden, J. Hey, and Z. Zhang, “A uniform hydrogen degradation law for high strength steels,” Eng. Fract. Mech., vol. 157, pp. 56–71, 2016, https://doi.org/10.1016/j.engfracmech.2016.02.001.10.1016/j.engfracmech.2016.02.001 ↗
9. W. S. Walston, I. M. Bernstein, and A. W. Thompson, “The effect of internal hydrogen on a single-crystal nickel-base superalloy,” Metall. Trans. A, vol. 23, pp. 1313–1322, 1992, https://doi.org/10.1007/BF02665063.10.1007/BF02665063 ↗
10. A. Barnoush, B. Yang, and H. Vehoff, “Effect of hydrogen and grain boundaries on dislocation nucleation and multiplication e with a NI-AFM,” Adv. Solid State Phys., vol. 47, pp. 253–269, 2008, https://doi.org/10.1007/978-3-540-74325-5_20.10.1007/978-3-540-74325-5_20 ↗
11. DIN 50969, Prevention of Hydrogen-Induced Brittle Fracture of High-Strength Steel Building Elements, Teil 2, Berlin, Germany, Beuth, 2013, in German.
12. J.-U. Riedel and V. Lipp, Hydrogen Embrittlement in Galvanic Processes Part III, ZVOreport 2, Hilden, Germany, Zentralverband Oberflächentechnik e.V., 2020, in German.
13. DBL 8461, Hot-dip Galvanized Prefabricated Parts (Batch Galvanizing), Stuttgart, Germany, Mercedes-Benz Factory Standard, 2019, in German.
14. DIN EN 10305, Steel Tubes for Precision Applications – Technical Delivery Conditions, Part 2, Berlin, Germany, Beuth, 2016.
15. DIN EN ISO 18265, Metallic Materials – Conversion of Hardness Values, Berlin, Germany, Beuth, 2014.