Influence of backing layers on the interlaminar fracture toughness energy – Mode I – of quasi-unidirectional GFRP
Source abstract
Abstract
Abstract Quasi-unidirectional glass fiber non-crimp fabrics consist of a unidirectional main layer in the 0° direction stabilized by a backing layer in the 90° direction with a significantly lower amount of fibers. It is known that the backing layers impair the fatigue performance of respective reinforced plastics due to their orientation perpendicular to the main load direction. They act as damage initiators for the failure of the load-carrying unidirectional fibers. In the present work, the positive influence of the backing layers on the interlaminar fracture toughness energy – Mode I – G IC is demonstrated by tests in accordance with DIN EN 6033. The presence of backing fibers in the delamination plane can improve the G IC values by up to 43 %. Furthermore, results from evaluation according to DIN EN 6033 and ASTM D5528 are shown to have a good agreement, if the correction factor for large displacements recommended in the ASTM standard is not applied. If it is applied, however, there is a clear gap of up to 19 % between the two standards because the DIN simply does not provide a correction for large deflections.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Mechanical Behavior of Composites · Structural Analysis of Composite Materials · Natural Fiber Reinforced Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
New Materials and Processes , Fraunhofer Institute for Large Structures in Production Engineering IGP , Albert-Einstein-Straße 30 , Rostock 18059 , Germany
New Materials and Processes , Fraunhofer Institute for Large Structures in Production Engineering IGP , Rostock , Germany
Fraunhofer Institute for Large Structures in Production Engineering IGP , Rostock , Germany
References (17)
Show source-provided references
1. K. Vallons, G. Adolphs, P. Lucas, S. V. Lomov, and I. Verpoest, “Quasi-UD glass fibreNCF composites for wind energy applications: a review of requirements and existing fatigue data for blade materials,” Mech. Ind., vol. 14, no. 3, pp. 175–189, 2013, https://doi.org/10.1051/meca/2013045.10.1051/meca/2013045 ↗
2. J. Zangenberg, P. Brøndsted, and J. W. Gillespie, “Fatigue damage propagation in unidirectional glass fibre reinforced composites made of a non-crimp fabric,” J. Compos. Mater., vol. 48, no. 22, pp. 2711–2727, 2014, https://doi.org/10.1177/0021998313502062.10.1177/0021998313502062 ↗
3. K. M. Jespersen, J. Zangenberg, T. Lowe, P. J. Withers, and L. P. Mikkelsen, “Fatigue damage assessment of uni-directional non-crimp fabric reinforced polyester composite using X-ray computed tomography,” Compos. Sci. Technol., vol. 136, pp. 94–103, 2016, https://doi.org/10.1016/j.compscitech.2016.10.006.10.1016/j.compscitech.2016.10.006 ↗
4. K. M. Jespersen and L. P. Mikkelsen, “Three dimensional fatigue damage evolution in non-crimp glass fibre fabric based composites used for wind turbine blades,” Compos. Sci. Technol., vol. 153, pp. 261–272, 2017, https://doi.org/10.1016/j.compscitech.2017.10.004.10.1016/j.compscitech.2017.10.004 ↗
5. K. M. Jespersen, J. A. Glud, J. Zangenberg, A. Hosoi, H. Kawada, and L. P. Mikkelsen, “Uncovering the fatigue damage initiation and progression in uni-directional non-crimp fabric reinforced polyester composite,” Compos. Part A Appl. Sci., vol. 109, pp. 481–497, 2018, https://doi.org/10.1016/j.compositesa.2018.03.002.10.1016/j.compositesa.2018.03.002 ↗
6. S. Korkiakoski, P. Brøndsted, E. Sarlin, and O. Saarela, “Influence of specimen type and reinforcement on measured tension–tension fatigue life of unidirectional GFRP laminates,” Int. J. Fatigue, vol. 85, pp. 114–129, 2016, https://doi.org/10.1016/j.ijfatigue.2015.12.008.10.1016/j.ijfatigue.2015.12.008 ↗
7. D. D. Samborsky, J. F. Mandell, and D. Miller, “The SNL/MSU/DOE fatigue of composite materials database: recent trends,” in 53rd AIAA/ASME/ASCE/AHS/ASC, Structures, Structural Dynamics and Materials Conf, Honolulu, Haiwaii, 2012.10.2514/6.2012-1573 ↗
8. R. Rikards, A. Korjakin, F. G. Buchholz, H. Wang, A. K. Bledzki, and G. Wacker, “Interlaminar fracture toughness of GFRP influenced by fiber surface treatment,” J. Compos. Mater., vol. 32, no. 17, pp. 1528–1559, 1998, https://doi.org/10.1177/002199839803201701.10.1177/002199839803201701 ↗
9. P. Robinson and J. M. Hodgkinson, “Interlaminar fracture toughness,” in Mechanical testing of advanced fibre composites, J. M. Hodgkinson, Ed., Cambridge, England, Boca Raton, FL, USA, Woodhead Publishing Limited, CRC Press, 2000, pp. 170–210. ch. 9.10.1533/9781855738911.170 ↗
10. European Standards, Luft- und Raumfahrt – Kohlenstofffaserverstärkte Kunststoffe – Prüfverfahren – Bestimmung der interlaminaren Energiefreisetzungsrate – Mode I – GIC, DIN EN 6033:2015, Berlin, Germany, DIN Deutsches Institut für Normung e.V., 2016.
11. ASTM International, Standard Test Method for Mode I Interlaminar Fracture Toughness of Unidirectional Fiber-Reinforced Polymer Matrix Composites, ASTM D5528 – 13, West Conshohocken, PA, USA, ASTM International, 2013.
12. ISO - International Organization for Standardization, Fibre-Reinforced Plastic Composites – Determination of Mode I Interlaminar Fracture Toughness, GIC, for Unidirectionally Reinforced Materials, ISO 15024:2001(E), Geneve, Switzerland, ISO International Organization for Standardisation, 2001.
13. T. K. O’Brien, and R. H. Martin, “Round robin testing for mode I interlaminar fracture toughness of composite materials,” J. Compos. Technol. Res., vol. 15, no. 4, pp. 269–281, 1993, https://doi.org/10.1520/CTR10379J.10.1520/CTR10379J ↗
14. D. C. Hartlen, J. Montesano, and D. S. Cronin, “A composite rigid double cantilever beam specimen for assessing the traction–separation response of mode I delamination in composite laminates,” Exp. Mech., vol. 63, no. 8, pp. 1273–1283, 2023, https://doi.org/10.1007/s11340-023-00987-2.10.1007/s11340-023-00987-2 ↗
15. V. Tamuzs, S. Tarasovs, and U. Vilks, “Progressive delamination and fiber bridging modeling in double cantilever beam composite specimens,” Eng. Fract. Mech., vol. 68, pp. 513–525, 2001, https://doi.org/10.1016/S0013-7944(00)00131-4.10.1016/S0013-7944(00)00131-4 ↗
16. E. Farmand-Ashtiani, J. Cugnoni, and J. Botsis, “Specimen thickness dependence of large scale fiber bridging in mode I interlaminar fracture of carbon epoxy composite,” Int. J. Solids Struct., vol. 55, pp. 58–65, 2015, https://doi.org/10.1016/j.ijsolstr.2014.03.031.10.1016/j.ijsolstr.2014.03.031 ↗
17. R. Marat-Mendes and M. Freitas, “DCB, ENF and ECT tests for interlaminar fracture of glass/epoxy unidirectional laminates,” in 10th Portugueses Conf. on Fracture, Braga, Portugal, 2006.