Surface Structural Changes of Feldspathic Ceramics Before and After Immersion in a Corrosive Medium Using Atomic Force Microscopy
Source abstract
Abstract
Abstract Ceramics are attractive dental materials as a result of their supe- rior aesthetics and biocompatibility. However, they are brittle and prone to premature failure, especially at repeated contact strain and in moist environments. The chemical stability of dental ceramics is important, because it directly affects mechanical properties and aesthetic value of restorations. The aim of this study was to investigate the effects of a corrosive agent, i.e. 4% acetic acid, on the surface of glazed and unglazed feldspathic ceramics. Metal-ceramic plates (9.0 × 9.0 × 1.2 mm) composed of a Ni-Cr alloy (Wiron 99, Bego Germany) and glazed or unglazed feldspathic ceramics (IPS Classic, Ivoclar-Vivadent, Schaan, Liechtenstein) were prepared according to the manufacturer‧s instructions. The samples were immersed in the solution at 80 °C and kept there for 16 h (ISO 6872). The surfaces of the samples before and after immersion in the corrosive medium were examined by atomic force microscopy (AFM). The pre- and post- corrosion AFM images of the surfaces of the feldspathic ceramics samples clearly show that the glazed surfaces are much less prone to deterioration by corrosion than the unglazed ones.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Bone Tissue Engineering Materials · Dental Implant Techniques and Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Zagreb, Croatia
References (25)
Show source-provided references
1. Degradability of dental ceramics10.1177/08959374920060012201 ↗
2. Dental ceramics: Current thinking and trends10.1016/j.cden.2004.01.003 ↗
3. A review of the strength properties of dental ceramics10.1016/0022-3913(92)90602-7 ↗
4. 1993
5. Kemijska degradacija dentalne keramike
6. Corrosion behavior of alumina ceramics in aqueous HCL and H2SO4 solutions10.1016/j.corsci.2007.10.008 ↗
7. Measurement of ion elution from dental ceramics10.1016/j.jeurceramsoc.2005.03.242 ↗
8. 2004 · 9910.1002/jbm.b.30066 ↗
9. Estimation of chemical resistance of dental ceramics by neural network10.1016/j.dental.2007.01.008 ↗
10. Sintering of dental porcelain: Effect of time and temperature on appearance and porosity10.1016/S0109-5641(01)00038-0 ↗
11. Comparative evaluation of four finishing systems on one ceramic surface
12. Protein characterisation of salivary and plasma biofilms formed in vitro on non-corroded and corroded dental ceramic materials. Biomaterials · 2001 · 22 · 2545
13. Ultrastructure of dental enamel afflicted with hypoplasia: An atomic force microscopic study10.1007/s00223-002-1045-2 ↗
14. ISO 6872 · 1995
15. Surface corrosion of dental ceramics in vitro10.1016/S0142-9612(98)00223-3 ↗
16. Use of contact testing in the characterization and design of all-ceramic crownlike layer structures: A review10.1067/mpr.2001.119581 ↗
17. AFM and SEM study of the effects of etching on IPS Empress 2 dental ceramics10.1016/S0039-6028(01)01301-2 ↗
18. Ion leaching from dental ceramics during static in vitro corrosion testing10.1002/jbm.10109 ↗
19. Strength, fracture toughness and microstructure of a selection of all-ceramic materials – Part I: Pressable and alumina glass-infiltrated ceramics10.1016/j.dental.2003.05.003 ↗
20. 1985 · 152
21. Resistance to staining, flexural strength and chemical solubility of core porcelains for all-ceramic crown
22. In vivo plaque formation on cast ceramic (Dicor) and conventional ceramic
23. Effects of various treatment and glazing (coating) techniques on the roughness and wettability of ceramic dental restorative surfaces10.1016/j.colsurfb.2006.09.016 ↗
24. Porcelain refinishing with two different polishing systems after orthodontic debonding10.2319/081307-374.1 ↗
25. Wear resistance of Chromium-Nitride and Diamond-like Carbon thin hard coatings10.3139/120.100892 ↗