journal article·2024-06Open access

Effect of Cu content on microstructure and properties of Ti-6Al-4V alloy fabricated by double-wire arc additive manufacturing

Yinbao Tian, Zhetao Liang, Guoyang Zhang, Hongqiang Liu, Zhengyi Jiang, Xin Zhang, Jingling Wang, Jian Han, Xiaoxin Zhao

Abstract

To solve the formation of coarse columnar β grains from Ti-6Al-4 V parts fabricated by wire + arc additive manufacturing , this study adds Cu element for in-situ alloying, effectively suppressing the growth of columnar grains and further enhancing properties. The results show that an addition of Cu element suppresses the lateral growth of β grains, eliminating the columnar structure of β grains. Compared with the Ti-6Al-4 V component, the original β grains in the Ti-6Al-4 V-10Cu component exhibit a refinement of 96 %. With an increase of Cu content, the phase structure of α-Ti transitions from lamellar to needle-like and eventually to equiaxed crystal structure. Moreover, as the Cu content rises, the precipitation of Ti 2 Cu increases, leading to precipitation strengthening and enhancing the microhardness . The average strength of the Ti-6Al-4 V-10Cu, Ti-6Al-4 V-11.7Cu, and Ti-6Al-4 V-15.7Cu walls is increased by 35.5 %, 56.9 %, and 71.6 %, respectively, compared with the Ti-6Al-4 V wall. The ultimate tensile strength is enhanced by 34.9 %, 49.5 %, and −1.4 %, respectively. However, the elongation is reduced by 48.6 %, 63.2 %, and 75.6 %, respectively.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Research on pore closure behavior and microstructure evolution during hot isostatic pressing of Ti6Al4V alloy casting10.1016/j.jmrt.2023.04.027 ↗
2. Regionalization of microstructure and mechanical properties of Ti6Al4V transition area fabricated by WAAM-LMD hybrid additive manufacturing10.1016/j.jallcom.2022.167345 ↗
3. Achieving excellent strength-ductility synergy of Ti6Al4V alloy produced by powder metallurgy and thermo-mechanical treatment10.1016/j.vacuum.2023.112448 ↗
4. Laser-directed energy deposition of ZrH2 particles reinforced Al7075 alloy: Cracks elimination and strength enhancement
5. A review of wire arc additive manufacturing (WAAM) of aluminium composite, process, classification, advantages, challenges, and application
6. Hybrid manufacturing of components from Ti-6Al-4V by metal forming and wire-arc additive manufacturing10.1016/j.jmatprotec.2020.116689 ↗
7. Wire arc additive manufacturing Ti6Al4V aeronautical parts using plasma arc welding: analysis of heat-treatment processes in different atmospheres10.1016/j.jmrt.2020.11.012 ↗
8. β Grain refinement by yttrium addition in Ti-6Al-4V wire-arc additive manufacturing10.1016/j.jallcom.2021.162735 ↗
9. The challenges associated with the formation of equiaxed grains during additive manufacturing of titanium alloys10.4028/www.scientific.net/KEM.770.155 ↗
10. S. Kou, Welding metallurgy, (2nd Ed.)[J].
11. Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti6Al4V by selective electron beam melting10.1016/j.matchar.2013.07.012 ↗
12. Metallurgical modelling of welding
13. A review of the wire arc additive manufacturing of metals: properties, defects and quality improvement10.1016/j.jmapro.2018.08.001 ↗
14. Grain-refinement mechanisms in titanium alloys10.1557/JMR.2008.0002 ↗
15. Beryllium as a grain refiner in titanium alloys10.1016/j.jallcom.2009.03.016 ↗
16. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
17. A study of Cu modified Ti–6Al–4V deposits fabricated by wire-arc directed energy deposition: alloy design, microstructure, and mechanical properties10.1016/j.msea.2023.145750 ↗
18. Microstructure and properties of a Ni–Ti–Cr–Mo–Nb alloy fabricated in situ by dual-wire arc additive manufacturing10.1016/j.msea.2022.143740 ↗
19. Ni50.8Ti49.2 alloy prepared by double-wire + arc additive manufacturing with a substrate heating temperature of 600 °C10.1016/j.jmapro.2023.08.042 ↗
20. High strength Ti alloy fabricated by directed energy deposition with in-situ Cu alloying10.1016/j.jmatprotec.2022.117759 ↗
21. Electrochemical behavior of centrifuged cast and heat treated Ti–Cu alloys for medical applications10.1016/j.electacta.2009.09.016 ↗
22. Effect of the existing form of Cu element on the mechanical properties, bio-corrosion and antibacterial properties of Ti-Cu alloys for biomedical application10.1016/j.msec.2016.08.033 ↗
23. Pushing the limits of the periodic table — A review on atomic relativistic electronic structure theory and calculations for the superheavy elements10.1016/j.physrep.2023.09.004 ↗
24. Glide and cross-slip of a-dislocations in Zr and Ti10.1016/j.actamat.2018.05.038 ↗
25. Microstructural optimization through heat treatment for enhancing the fracture toughness and fatigue crack growth resistance of selective laser melted Ti6Al4V alloy10.1016/j.actamat.2019.03.003 ↗
26. Formation mechanism of the α variant and its influence on the tensile properties of laser solid formed Ti-6Al-4V titanium alloy10.1016/j.msea.2017.03.035 ↗
27. Deformation behavior and microstructure evolution of titanium alloys with lamellar microstructure in hot working process: a review10.1016/j.jmst.2019.07.052 ↗
28. Influence of alpha-case layer on the low cycle fatigue properties of Ti-6Al-2Sn-4Zr-2Mo alloy10.1016/j.msea.2014.01.059 ↗
29. Phase transformations during cooling in α+β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
30. Finite element modeling of the morphology of β to α phase transformation in Ti-6Al-4V alloy10.1007/s11661-002-0204-4 ↗
31. Numerical simulation of microstructure evolution during the solid phase transformation of Ti-6Al-4V Alloy
32. Conjugated precipitation of twin-related α and Ti2Cu phases in a Ti–25V–3Cu alloy10.1016/j.actamat.2014.10.053 ↗
33. The role of prismatic slip dependent dynamic recrystallization in the fabrication of a submicrocrystalline Ti-Cu alloy with high thermostability10.1016/j.matdes.2020.108475 ↗
34. A comparison of the microstructures, thermal and mechanical properties of pressed and sintered Ti–Cu, Ti–Ni and Ti–Cu–Ni alloys intended for dental applications10.1016/j.jallcom.2020.156494 ↗
35. microstructure and corrosion behavior of binary titanium alloys with beta-stabilizing elements
36. Morphological evolution of transformation products and eutectoid transformation(s) in a hyper-eutectoid Ti-12 at% Cu alloy10.1016/j.actamat.2019.01.044 ↗
37. On the selection of Ti–Cu alloys for thixoforming processes: phase diagram and microstructural evaluation10.1007/s10853-015-9367-4 ↗
38. Effect of phase conditions on tensile and antibacterial properties of Ti-Cu alloys with Ti2Cu intermetallic compound10.1016/j.jallcom.2022.166823 ↗
39. The effect of solute elements on the grain refinement of cast Zn10.1007/s11661-013-1861-1 ↗
40. Mechanisms of globularization of Ti-6Al-4V during static heat treatment10.1007/s11661-003-0103-3 ↗
41. Study of the intrinsic mechanisms of nickel additive for grain refinement and strength enhancement of laser aided additively manufactured Ti–6Al–4V10.1088/2631-7990/ac6b61 ↗