journal article·2025-01

New findings on reduced solidification brittle temperature range in epitaxially grown CMSX-4 superalloy welds via varestraint testing

Min-Chang Shin, Eun-Joon Chun

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Microstructural and compositional design of Ni-based single crystalline superalloys ― a review10.1016/j.jallcom.2018.01.224 ↗
2. Alloy design for aircraft engines10.1038/nmat4709 ↗
3. The temperature dependence of γ′ volume fraction in a Ni-based single crystal superalloy from resistivity measurements10.1016/S1359-6462(00)00662-X ↗
4. Development of strong, oxidation and corrosion resistant nickel-based superalloys: critical review of challenges, progress and prospects10.1080/09506608.2018.1516713 ↗
5. Advanced characterization techniques for turbine blade wear and damage10.1016/j.procir.2016.09.005 ↗
6. Welding of Single Crystal Superalloy CMSX-4: Experiments and Modeling, in: TMS
7. Joining of nickel base superalloy single crystals10.1179/136217104225017080 ↗
8. Stray grain formation, thermomechanical stress and solidification cracking in single crystal nickel base superalloy welds10.1179/136217104225021841 ↗
9. Stray Grain Formation and Solidification Cracking Susceptibility of Single Crystal Ni-Base Superalloy CMSX-4
10. Comparison of single crystal Ni based superalloy repair by gas tungsten arc and electron beam processes10.1179/026708310X12701095964405 ↗
11. Metallographic and OIM study of weld cracking in GTA weld build-up of polycrystalline, directionally solidified and single crystal Ni based superalloys10.1179/136217108X370290 ↗
12. Solidification crack free welding strategy via ultra high precision laser scanning at a single grain of directionally solidified and single crystal superalloys10.5781/JWJ.2023.41.4.4 ↗
13. Effect of substrate cooling on the epitaxial growth of Ni-based single-crystal superalloy fabricated by direct energy deposition10.1016/j.jmst.2020.05.041 ↗
14. Single-crystal height extension by laser metal deposition of CMSX-410.1016/j.procir.2020.09.057 ↗
15. Hot cracking behavior and mechanism of a third-generation Ni-based single-crystal superalloy during directed energy deposition
16. Single-crystal laser deposition of superalloys: processing–microstructure maps10.1016/S1359-6454(00)00367-0 ↗
17. Laser repair of superalloy single crystals with varying substrate orientations10.1007/s11661-007-9172-z ↗
18. Quantifying susceptibility to solidification cracking in oscillated CM247LC superalloy welds via Varestraint Testing10.1007/s12540-022-01250-4 ↗
19. Effects of Hf and carbides formation behavior on the weld solidification cracking susceptibility of 247LC superalloy10.1016/j.matchemphys.2024.129147 ↗
20. DuPont · 2009
21. A new hot-tearing criterion10.1007/s11661-999-0334-z ↗
22. Last-stage solidification of alloys: theoretical model of dendrite-arm and grain coalescence10.1007/s11661-003-0083-3 ↗