Effect of deformation speed on microstructure evolution and mechanical property of Mg-Gd alloys
Source abstract
Abstract
Abstract The effect of deformation speed on microstructure and mechanical property was investigated in Mg1Gd and Mg3Gd alloys, and annealing of high-speed deformed samples was studied. Twinning was a dominant deformation mechanism after low-speed and high-speed compressions, while twin variant and type diversities were observed. Low-speed and high-speed deformed samples showed difference in twin amounts instead of twin types. Low-speed deformed samples exhibited more 10 1 ¯ 2 tension twins (including unusual tension twins), while amount of 10 1 ¯ 2 - 10 1 ¯ 2 twin boundaries soared in high-speed deformed samples that contained less tension twins. 10 1 ¯ 1 contraction twins and 10 1 ¯ 1 - 10 1 ¯ 2 double twins were relatively less activated after both low-speed and high-speed deformations. During annealing, hardness fluctuated because of competition between twin boundary segregation and recovery, while a higher alloying content would lead to a higher hardening rate as well as an extended hardening stage.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Weight loss with magnesium alloys10.1126/science.1182848 ↗
2. The origins of high hardening and low ductility in magnesium10.1038/nature15364 ↗
3. Precipitation strengthening in an ultralight magnesium alloy10.1038/s41467-019-08954-z ↗
4. Linear complexions confined chemical and structural states at dislocations10.1126/science.aab2633 ↗
5. Achieving high strength and ductility in magnesium alloys via densely hierarchical double contraction nanotwins10.1021/acs.nanolett.7b02641 ↗
6. Study of deformed microstructures near the impact crater in pure copper targets10.1016/j.msea.2004.05.029 ↗
7. Strain rates in crashworthiness
8. High speed forming of the light-weight wrought alloys
9. Anomalous effects of strain rate on the room-temperature ductility of a cast Mg-Gd-Y-Zr alloy10.1016/j.actamat.2018.08.013 ↗
10. High strain rate deformation behavior of an AZ91 magnesium alloy at elevated temperatures10.1016/j.matlet.2005.01.012 ↗
11. Dynamic tensile properties and microstructural evolution of extruded EW75 magnesium alloy at high strain rates10.1016/j.jma.2020.02.013 ↗
12. Deformation and spallation of a magnesium alloy under high strain rate loading10.1016/j.msea.2016.03.009 ↗
13. Dynamic compressive property and failure behavior of extruded Mg-Gd-Y alloy under high temperatures and high strain rates10.1016/j.jma.2015.04.003 ↗
14. Deformed microstructure evolution in AM60B Mg alloy under hypervelocity impact at a velocity of 5kms−110.1016/j.matdes.2010.03.010 ↗
15. Characterization of adiabatic shear bands in AM60B magnesium alloy under ballistic impact10.1016/j.matchar.2011.03.003 ↗
16. Twinning behavior and lattice rotation in a Mg–Gd–Y–Zr alloy under ballistic impact10.1016/j.jallcom.2015.08.020 ↗
17. Influence of twinning-induced recrystallization on texture evolution in a high strain rate compressed Mg-Zn alloy10.1016/j.matchar.2020.110192 ↗
18. Twinning-induced negative strain rate sensitivity in wrought Mg alloy AZ3110.1016/j.msea.2011.04.059 ↗
19. Grain refinement of ZK60 magnesium alloy during low temperature deformation
20. Periodic segregation of solute atoms in fully coherent twin boundaries10.1126/science.1229369 ↗
21. Chakrabarty · 2005
22. Microstructural evolution of pure magnesium under high strain rate loading10.1016/j.actamat.2014.12.030 ↗
23. Global strain generated by shuffling-dominated {10-12}<10-1-1> twinning10.1016/j.scriptamat.2013.10.002 ↗
24. Microstructures and textures of pure magnesium deformed in plane-strain compression10.1016/j.scriptamat.2004.07.002 ↗
25. High-strain-Rate deformation: mechanical behavior and deformation substructures induced10.1146/annurev-matsci-070511-155034 ↗
26. Fabrication of strong and ductile AZ31 magnesium alloy using high strain rate multiple forging in a wide temperature range10.3390/met10060729 ↗
27. Deformation mechanism of fine grained Mg–7Gd–5Y–1.2Nd–0.5Zr alloy under high temperature and high strain rates10.1016/j.jma.2020.02.017 ↗
28. The High strain rate deformation behavior of high purity magnesium and AZ31B magnesium alloy
29. Strain-rate sensitivity and microstructural evolution in a Mg–Al–Zn alloy10.1016/j.scriptamat.2010.06.047 ↗
30. Hazeli · 2018
31. Effects of gadolinium and neodymium addition on young’s modulus of magnesium-based binary alloys
32. The effect of high yttrium solute concentration on the twinning behaviour of magnesium alloys10.1016/j.actamat.2014.09.022 ↗
33. Strain-induced nano recrystallization in AZ31 magnesium: TEM characterization10.1016/j.jallcom.2016.12.424 ↗
34. Self-patterning Gd nano-fibers in Mg-Gd alloys10.1038/srep38537 ↗
35. Orientational analysis of static recrystallization at compression twins in a magnesium alloy AZ3110.1016/j.msea.2009.03.045 ↗