journal article·2026-06Open access

Pitting corrosion of copper pipes: The role of water quality and abrasive pre-treatment

Aino Pelto-Huikko, Noora Salonen, Riika Mäkinen, Merja Ahonen, Martti Latva

Abstract

Copper pipes are widely used in drinking water applications. Although copper is considered a corrosion-resistant material, its pitting corrosion has been linked to water quality parameters, such as high concentrations of chloride, aluminium, and sulphate. Additionally, some recent studies have associated the silicate layers on the inner surfaces of copper pipes with corrosion. In this study, the initiation of pitting corrosion in cold and hot water copper pipelines was investigated across six study locations with six different drinking water qualities. Copper pipe samples were taken after 6, 12, and 24 months of use. To study the effect of stagnation on corrosion initiation, one hot-water line in each study location was left unused for 8 weeks after commissioning. Iron residues from abrasive (blast) pre-treatment of the copper pipe inner surface, combined with CO 2 -rich drinking water, were identified as potential contributors to pitting initiation. This mechanism has not previously been demonstrated under field conditions. In waters with low CO 2 , iron residues oxidised and were flushed away without causing damage, suggesting that CO 2 content in water may be a critical but currently unregulated parameter for assessing corrosion risk in new copper installations. Contrary to recent concerns, neither silicate layers on pipe surfaces nor stagnation during commissioning were associated with pitting in any of the six study locations.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Water Treatment and Disinfection · Chemical Analysis and Environmental Impact

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Pitting corrosion of copper tubes in soft drinking waters: corrosion mechanism10.1002/j.1551-8833.2004.tb10742.x ↗
2. Inhibition of copper pitting corrosion in aggressive potable waters10.1155/2012/857823 ↗
3. Copper corrosion mechanisms, influencing factors, and mitigation strategies for water circuits of heat exchangers: critical review and current advances
4. Advancements in corrosion studies and protective measures for copper and copper-based alloys in varied environmental conditions10.1016/j.rineng.2025.105257 ↗
5. Analysis and ranking of corrosion causes for water pipelines: a critical review
6. Role of solution chemistry on corrosion of copper in synthetic solutions: Effect of bicarbonate ion concentration on uniform and localised attack10.1179/bcj.1996.31.2.125 ↗
7. A comprehensive investigation of copper pitting corrosion in a drinking water distribution system10.1016/j.corsci.2010.02.013 ↗
8. Effect of aluminium solids and chlorine on cold water pitting of copper10.1016/j.corsci.2004.05.021 ↗
9. Effects of selected water chemistry variables on copper pitting propagation in potable water10.1016/j.electacta.2011.04.008 ↗
10. Pitting corrosion of copper in waters with high pH and low alkalinity10.1002/j.1551-8833.2008.tb09586.x ↗
11. A new type of silica-induced “moundless” pitting corrosion in copper observed in Japan10.1016/j.heliyon.2022.e10110 ↗
12. Pitting corrosion of copper tubes for drinking water applications due to silicate films10.1149/07501.0137ecst ↗
13. Method for treating the inner surface of a tube
14. S. Välimäki, Method for producing copper tubes, 2000, EP0976845 (A1).
15. Enhancing the oxidation resistance of copper by using sandblasted copper surfaces10.1016/j.apsusc.2015.09.203 ↗
16. A. Korhonen, M. Kuusela, S. Liski-Markkanen, and T. Marjomaa, Kestävä veden käyttö - vedenkäyttöselvitys, 1st ed., vol. TTS:n julkaisuja 453. Työtehoseura ry, 2020. [Online]. Available: www.tts.fi.
17. SFS-EN 1057 + A1, Copper and copper alloys. Seamless, round copper tubes for water and gas in sanitary and heating applications.
18. Exploring the potential of silicate-based corrosion inhibition for copper in dynamic salt water environment10.1016/j.electacta.2025.145956 ↗
19. Inhibition of copper corrosion by corrosion inhibitors in the presence of scale dispersants10.2320/matertrans.MT-D2024004 ↗
20. Corrosion of copper by water of various temperatures and carbon dioxide contents10.1002/maco.19770281102 ↗
21. Cramer · 2005
22. Fonseca · 2024 · 5537767