journal article·2004Open access

Effect of Ni Addition on Fatigue Properties of Bulk Glassy Zr50Cu40Al10 Alloys

Yoshihiko Yokoyama, Kenzo Fukaura, Akihisa Inoue

MATERIALS TRANSACTIONS· Volume 45· Issue 5

Abstract

We examined Wöhler curves of Zr50Cu40Al10 and Zr50Cu30Ni10Al10 bulk glassy alloys (BGAs) using a rotating-beam fatigue test to evaluate the effect of addition Ni on fatigue strength. As a result, we found that the fatigue limit was increased from 250 MPa to 500 MPa by adding 10 at% Ni instead of Cu to a Zr50Cu40Al10 BGA. Zr50Cu40Al10 BGAs exhibit wider fatigue-fractured region with striation-like marks than that of Zr50Cu30Ni10Al10 BGAs. Additive Ni element limits the fatigue-fractured region to half of the whole fractured surface. We also measured dimensions of fatigue-fracture area of Zr50Cu40Al10 and Zr50Cu30Ni10Al10 BGAs to estimate the value of fatigue-fracture toughness. Especially, the fatigue fracture toughness decreases suddenly around 103 ∼ 104 cycles, similar to the Wöhler curves. The significant decrease of fatigue-fracture toughness originates from embrittlement/hardening in front of the fatigue crack tip during fatigue test.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Glass properties and applications · Surface Roughness and Optical Measurements

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Faculty of Engineering, Himeji Institute of Technology

Institute for Materials Research, Tohoku University

References (23)

Show source-provided references
1. 1) H.S. Chen and T.T. Wang: J. Appl. Phys. 41 (1970) 5338-5339.10.1063/1.1658675 ↗
2. 2) C.C. Hays, C.P. Kim and W.L. Johnson: Phys. Rev. Lett. 84 (2000) 2901-2904.10.1103/PhysRevLett.84.2901 ↗
3. 3) For example, A. Inoue: Bulk Amorphous Alloys, (trans tech publication, Zuerich, 1998).
4. 4) H. Kakiuchi, A. Inoue, M. Onuki, Y. Takano and T. Yamaguchi: Mater. Trans. 42 (2001) 678-681.10.2320/matertrans.42.678 ↗
5. 5) W.L. Johnson: JOM 3 (2002) 40-43.10.1007/BF02822619 ↗
6. 6) Y. Yokoyama and A. Inoue: Collected Abstractus of the 2001 Autumn Meeting of the Japan Inst. Matals, p.280.
7. 7) Y. Yokoyama, A. Kobayashi, K. Fukaura and A. Inoue: Mater. Trans. 43 (2002) 571-574.10.2320/matertrans.43.571 ↗
8. 8) Y. Yokoyama, K. Fukaura and A. Inoue: Intermetallics 10 (2002) 1113-1124.10.1016/S0966-9795(02)00141-3 ↗
9. 9) C.J. Gilbert, J.M. Lippmann and R.O. Ritchie: Scr. Mater. 38 (1998) 537-542.10.1016/S1359-6462(97)00522-8 ↗
10. 10) R.O. Ritchie, C.J. Gilbert and V. Schroeder: Proc. Inter. Conf. on “Advanced Technology in Experimental Mechanics '99”, JSME-MMD, Vol.1 (1999) 9-16.
11. 11) Y. Yokoyama, K. Fukaura and H. Sunada: Mater. Trans. 41 (2000) 675-680.10.2320/matertrans1989.41.675 ↗
12. 12) A. Gebert, J. Eckert and L. Schultz: Acta Mater. 46 (1998) 5475-5482.10.1016/S1359-6454(98)00187-6 ↗
13. 13) Y. Yokoyama, K. Inoue and K. Fukaura: Mater. Trans. 43 (2002) 2316-2319.10.2320/matertrans.43.2316 ↗
14. 14) Y. Yokoyama, K. Inoue and K. Fukaura: Mater. Trans. 43 (2002) 3199-3205.10.2320/matertrans.43.3199 ↗
15. 15) B. Yang, P.K. Liaw, G. Wang, M. Morrison, C.T. Liu, R.A. Buchanan and Y. Yokoyama: Proc. Inter. Conf. on “Bulk Metallic Glasses III”, (2003) in press.
16. 16) H. French: Trans. ASTM 21 (1933) 899.
17. 17) Y. Murakami: Stress Intensity Factors Handbook, (Maruzen, Tokyo, 1987) 657-658.
18. 18) For example, M. Kawada: Data Book of Fatigue Design, (Maruzen, Tokyo, 1961) p.44.
19. 19) For example, M. Kawada: Data Book of Fatigue Design, (Maruzen, Tokyo, 1961) p.95.
20. 20) D.A. Meyn: Trans. ASM 61 (1968) 52-61.
21. 21) R.M.N. Pelloux: Trans. ASM 62 (1969) 281-285.
22. 22) K. Fujita, T. Zhang and A. Inoue: Mater. Trans. 42 (2001) 1502-1508.10.2320/matertrans.42.1502 ↗
23. 23) W.H. Peter, P.K. Liaw, R.A. Buchanan, C.T. Liu, C.R. Brooks, J.A. Horton Jr., C.A. Carmichael Jr. and J.L. Wright: Intermetallics 10 (2002) 1125-1129.10.1016/S0966-9795(02)00152-8 ↗