Aluminide Coatings Fabricated on Nickel by Aluminium Electrodeposition from DMSO2-Based Electrolyte and Subsequent Annealing

Suguru Shiomi, Masao Miyake, Tetsuji Hirato, Akihiro Sato

MATERIALS TRANSACTIONS· Volume 52· Issue 6

Abstract

A new cost-effective process to fabricate aluminide coatings was developed. Coating layers consisting of nickel aluminides could be formed by electrodeposition of Al layers from a dimethylsulfone-AlCl3 electrolyte on Ni substrates and subsequent annealing in air or vacuum at temperatures of 700–1150°C. Analysis of the intermetallic layers by XRD, SEM and EDX indicated the formation of Al3Ni and Al3Ni2 at 700°C, AlNi at 900°C and 1000°C, and AlNi and AlNi3 at 1150°C. The Annealing atmosphere did not affect the resulting intermetallic products.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Semiconductor materials and interfaces · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Graduate School of Energy Science, Kyoto University

Corporate Research & Development, IHI Corporation

References (20)

Show source-provided references
1. 1) S. Bose: High Temperature Coatings, (Elsevier Butterworth-Heinemann, 2007) pp. 71–97.10.1016/B978-075068252-7/50007-X ↗
2. 2) S. Kobayashi and T. Yakou: Mater. Sci. Eng. A 338 (2002) 44–53.10.1016/S0921-5093(02)00053-9 ↗
3. 3) C. Houngninou, S. Chevalier and J. P. Larpin: Appl. Surf. Sci. 236 (2004) 256–269.10.1016/j.apsusc.2004.04.026 ↗
4. 4) T. S. Hussey, M. J. Koczak, R. W. Smith and S. R. Kalidindi: Mater. Sci. Eng. A 229 (1997) 137–146.10.1016/S0921-5093(97)80109-8 ↗
5. 5) M. S. Chu and S. K. Wu: Acta Mater. 51 (2003) 3109–3120.10.1016/S1359-6454(03)00123-X ↗
6. 6) D. Zhong, J. J. Moore, J. Disam, S. Thiel and I. Dahan: Surf. Coat. Tech. 120–121 (1999) 22–27.10.1016/S0257-8972(99)00334-5 ↗
7. 7) M. Fukumoto, T. Suzuki, M. Hara and T. Narita: Mater. Trans. 50 (2009) 335–340.10.2320/matertrans.MRA2008293 ↗
8. 8) L. Qingfeng, H. A. Hjuler, R. W. Berg and N. J. Bjerrum: J. Electrochem. Soc. 137 (1990) 593–598.10.1149/1.2086512 ↗
9. 9) Q. X. Liu, S. Z. E. Abedin and F. Endres: Surf. Coat. Tech. 201 (2006) 1352–1356.10.1016/j.surfcoat.2006.01.065 ↗
10. 10) J. Fransaer, E. Leunis, T. Hirato and J.-P. Celis: J. Appl. Electrochem. 32 (2002) 123–128.10.1023/A:1014738011603 ↗
11. 11) L. Legrand, A. Tranchant and R. Messina: J. Electrochem. Soc. 141 (1994) 378–382.10.1149/1.2054735 ↗
12. 12) L. Legrand, A. Tranchant, R. Messina, F. Romain and A. Lautie: Inorg. Chem. 35 (1996) 1310–1312.10.1021/ic941455q ↗
13. 13) L. Legrand, E. Chassaing, A. Chausse and R. Messina: Electrochim. Acta 43 (1998) 3109–3115.10.1016/S0013-4686(98)00065-6 ↗
14. 14) T. Jiang, M. J. Chollier Brym, G. Dubé, A. Laisa and G. M. Brisard: Surf. Coat. Tech. 201 (2007) 6309–6317.10.1016/j.surfcoat.2006.11.035 ↗
15. 15) K. Garbala and A. Patejuk: ARCHIVES of FOUNDRY ENGINEERING 10 (2010) 455–458.
16. 16) G. A. López, S. Sommadossi, W. Gust, E. J. Mittermeijer and P. Zieba: Interf. Sci. 10 (2002) 13–19.10.1023/A:1015172710411 ↗
17. 17) T. B. Massalski: Binary Phase Diagram, (ASM International, 1990).
18. 18) M. W. Brumm and H. J. Grabke: Corr. Sci. 34 (1993) 547–561.10.1016/0010-938X(93)90271-H ↗
19. 19) S. Shankar and L. L. Seigle: Metall. Trans. A 9 (1978) 1467–1476.10.1007/BF02661819 ↗
20. 20) S. Kim and Y. A. Chang: Metall. Mater. Trans. A 31 (2000) 1519–1524.10.1007/s11661-000-0162-7 ↗