Thermal Fatigue Behavior of Flip-chip Joints with Lead-free Solders
Source abstract
Abstract
Thermal cycle tests were performed for flip-chip joints with several lead-free solders in order to research the thermal fatigue behavior of the joints. A joint with Sn–3.5Ag solder was ruptured by solder cracking in the neighborhood of the joint interface. A joint with Sn–3.5Ag–0.76Cu solder was ruptured by interfacial cracking at the Al/Ni interface, and the lifetime before the rupture was shorter than that of the Sn–3.5Ag solder. Although the rupture modes were different, both joints showed a sufficient fatigue life to tolerate the alignment stress in the flip-chip bonding process. In the case of a joint with Sn–1.9Ag–0.52Cu–7.6Bi solder, an interfacial crack was observed in the joint immediately after reflow soldering. Bi segregation was found in the cracked interface. The cracked microstructure was similar to the structure of lifted-off joints often observed when soldering through-hole circuits with Bi-bearing solder. These thermal cycle test results with Sn–3.5Ag and Sn–3.5Ag–0.76Cu solders demonstrate that there is a possibility of using flip-chip joints with these solders for conventional electronic applications.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Faculty of Engineering, Gunma University
IBM Japan
Graduate School of Engineering, Osaka University
References (13)
Show source-provided references
1. 1) I. Shohji, F. Mori, S. Fujiuchi and M. Yamashita: Journal of Japan Institute of Electronics Packaging 4 (2001) 133–137.10.5104/jiep.4.133 ↗
2. 2) I. Shohji, F. Mori, S. Fujiuchi and M. Yamashita: Journal of Japan Institute of Electronics Packaging 4 (2001) in printing.10.5104/jiep.4.289 ↗
3. 3) L. F. Miller: IBM Journal of Research and Development 13 (1969) 239–250.10.1147/rd.133.0239 ↗
4. 4) Y. Tsukada, S. Tsuchida and Y. Mashimoto: Proc. of the 7th International Microelectronics Conference, (The Microelectronics Society-Japan, 1992) pp. 252–258.
5. 5) I. Shohji, T. Yamada and H. Kimura: Proc. of the 9th International Microelectronics Conference, (The Microelectronics Society-Japan, 1996) pp. 314–317.
6. 6) I. Shohji, Y. Orii and K. F. Kobayashi: Quarterly Journal of Japan Welding Society 16 (1998) 215–222.10.2207/qjjws.16.215 ↗
7. 7) I. Shohji, S. Fujiwara, S. Kiyono and K. F. Kobayashi: Scr. Mater. 40 (1999) 815–820.10.1016/S1359-6462(99)00007-X ↗
8. 8) P. Villars, A. Prince and H. Okamoto: Handbook of Ternary Alloy Phase Diagrams 4 (1995) 9819–9837.
9. 9) K. Suganuma: Scr. Mater. 38 (1998) 1333–1340.10.1016/S1359-6462(98)00059-1 ↗
10. 10) Y. Kariya and M. Otsuka: J. Electron. Mater. 27 (1998) 866–870.10.1007/s11664-998-0111-6 ↗
11. 11) Y. Kariya, H. Kagawa and M. Otsuka: Proc. of 4th Symposium on “Microjoining and Assembly Technology in Electronics”, (Japan Welding Society, 1998) 259–264.
12. 12) K. C. Norris and A. H. Landzberg: IBM Journal of Research and Development 13 (1969) 266–271.10.1147/rd.133.0266 ↗
13. 13) M. Sakane, T. Yamamoto, M. Ohnami and T. Yamada: Mechanics and Materials for Electronic Packaging 187 (1994) 51–56.