The Oxide Scale Formation and Evolution on Detonation Gun Sprayed NiCrAlY Coatings during Isothermal Oxidation
Source abstract
Abstract
NiCrAlY coatings were prepared by the newly-developed detonation gun spray process. The oxide scale formation and evolution on these coatings during isothermal oxidation in air at 1100°C were investigated. It was found that semi-molten particles, particle debris and pores, are present in the surface layer of the as-sprayed coating. During 100 h oxidation, the particle debris and some semi-molten particles gradually change into oxide mixture consisting of spinel, chromia and nickel oxides. However, after removal of the surface layer of the coating by a grinding treatment, a dense and single-layer α-Al2O3 scale forms on the surface of the coating during the oxidation. The mechanisms governing the oxide scale formation and evolution are discussed in terms of atomic diffusion and thermodynamic stability. In addition, thermogravimetric analysis showed that the oxidation rate of the ground NiCrAlY coating at 1100°C is much lower than that of the as-sprayed one. The residual stress in thermally grown oxide scales was investigated using photo-stimulated luminescence spectroscopy.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences
Department of Intelligent Mechanical Engineering, Fukuoka Institute of Technology
References (28)
Show source-provided references
1. 1) W. J. Brindley: J. Therm. Spray Technol. 6 (1997) 85–90.10.1007/BF02646316 ↗
2. 2) W. Brandl, H. J. Grabke, D. Toma and J. Kruger: Surf. Coat. Technol. 86–87 (1996) 41–47.10.1016/S0257-8972(96)03039-3 ↗
3. 3) M. Jinnestrand and H. Brodin: Mater. Sci. Eng. A 379 (2004) 45–57.10.1016/j.msea.2003.12.063 ↗
4. 4) Y. N. Wu, F. H. Wang, W. G. Hua, J. Gong, C. Sun and L. S. Wen: Surf. Coat. Technol. 166 (2003) 189–194.10.1016/S0257-8972(02)00783-1 ↗
5. 5) F. H. Yuan, Z. W. Huang, Z. G. Wang, C. Sun and S. J. Zhu: J. Mater. Sci. Technol. 20 (2004) 85–88.
6. 6) Y. N. Wu, P. L. Ke, Q. M. Wang, C. Sun and F. H. Wang: Corros. Sci. 46 (2004) 2925–2935.10.1016/j.corsci.2004.04.003 ↗
7. 7) E. A. G. Shillington and D. R. Clarke: Acta Mater. 47 (1999) 1297–1305.10.1016/S1359-6454(98)00407-8 ↗
8. 8) A. G. Evans, D. R. Mumm, J. W. Hutchinson, G. H. Meier and F. S. Pettit: Prog. Mater. Sci. 46 (2001) 505–553.10.1016/S0079-6425(00)00020-7 ↗
9. 9) H. Choi, B. Yoon, H. Kim and C. Lee: Surf. Coat. Technol. 150 (2002) 297–308.10.1016/S0257-8972(01)01557-2 ↗
10. 10) F. Tang, L. Ajdelsztajn and J. M. Schoenung: Scripta Mater. 51 (2004) 25–29.10.1016/j.scriptamat.2004.03.026 ↗
11. 11) M. Shibata, S. Kuroda, H. Murakami, M. Ode, M. Watanabe and Y. Sakamoto: Mater. Trans. 47 (2006) 1638–1642.10.2320/matertrans.47.1638 ↗
12. 12) D. R. Clarke, J. R. Christensen and V. K. Tolpygo: Surf. Coat. Technol. 94–95 (1997) 89–93.10.1016/S0257-8972(97)00483-0 ↗
13. 13) T. Tomimatsu, S. J. Zhu and Y. Kagawa: Acta Mater. 51 (2003) 2397–2405.10.1016/S1359-6454(03)00046-6 ↗
14. 14) T. Tomimatsu, S. J. Zhu and Y. Kagawa: Scripta Mater. 50 (2004) 137–141.10.1016/j.scriptamat.2003.09.005 ↗
15. 15) H. Singh, S. Prakash and D. Puri: Mater. Sci. Eng. A 444 (2007) 242–250.10.1016/j.msea.2006.08.080 ↗
16. 16) X. Ren, F. H. Wang and X. Wang: Surf. Coat. Technol. 198 (2005) 425–431.10.1016/j.surfcoat.2004.10.108 ↗
17. 17) D. Utu, G. Marginean, W. Brandl and I. Cartis: Solid State Sci. 7 (2005) 459–464.10.1016/j.solidstatesciences.2005.01.003 ↗
18. 18) H. E. Evans and M. P. Taylor: Oxid. Met. 55 (2001) 17–34.10.1023/A:1010369024142 ↗
19. 19) K. Messaoudi, A. M. Huntz and B. Lesage: Mater. Sci. Eng. A 247 (1998) 248–262.10.1016/S0921-5093(97)00711-9 ↗
20. 20) M. J. Stiger, N. M. Yanar, M. G. Topping, F. S. Pettit and G. H. Meier: Z. Metallkd. 90 (1999) 1069–1078.10.1515/ijmr-1999-901218 ↗
21. 21) T. Teratani, H. Yamano, N. Mifune, K. Tani, Y. Harada and M. Okazaki: J. Jap. Inst. Metals 68 (2004) 1060–1067.10.2320/jinstmet.68.1060 ↗
22. 22) D. Strauss, G. Muller, G. Schumacher, V. Engelko, W. Stamm, D. Clemens and W. J. Quaddakers: Surf. Coat. Technol. 135 (2001) 196–201.10.1016/S0257-8972(00)00916-6 ↗
23. 23) Y. N. Wu, G. Zhang, Z. C. Feng, B. C. Zhang, Y. Liang and F. J. Liu: Surf. Coat. Technol. 138 (2001) 56–60.10.1016/S0257-8972(00)01102-6 ↗
24. 24) H. B. Guo, H. B. Xu, S. K. Gong and F. S. Liu: Rare Met. Mater. Eng. 30 (2001) 314–317.
25. 25) D. Monceau, F. Crabos, A. Malie and B. Pieraggi: Mater. Sci. Forum 369–372 (2001) 607–614.10.4028/www.scientific.net/MSF.369-372.607 ↗
26. 26) C. Piehl, Zs. Toekei and H. J. Grabke: Mater. High Temp. 17 (2000) 243–246.10.1179/mht.2000.17.2.010 ↗
27. 27) B. Wang, C. Sun, J. Gong, R. F. Huang and L. S. Wen: Corros. Sci. 46 (2004) 519–528.10.1016/S0010-938X(03)00184-7 ↗
28. 28) A. Aubry, F. Armanet, G. Beranger, J. L. Lebrun and G. Maeder: Acta Metall. 36 (1988) 2779–2786.10.1016/0001-6160(88)90124-1 ↗