Monitoring the Early Stage of Degradation of Epoxy-Coated Steel for Ballast Tank by Electrochemical Impedance Spectroscopy
Source abstract
Abstract
The early stages of the degradation of thick epoxy-coated steels used for water ballast tanks were monitored by electrochemical impedance spectroscopy (EIS). 200-μm-thick epoxy-coated steels were exposed to accelerated corrosion tests containing humid air at 70℃ for 246 days before immersion in a NaCl solution at 70℃ for 79 days. They were removed from the corrosion test chamber during the test so that EIS measurements could be performed in order to determine the coating resistance (Rf) and the coating capacitance (Cf). In addition, the water volume fraction (XV) and the diffusion coefficient (DH2O) in the coating were determined from the Cf vs. t1/2 curves during the water desorption process. These parameters were compared with the degradation morphology of the coated steel after a pull-off test. Only “physical aging” of coating was observed for first 80 days. After 190th day, Rf decreasing, Cf and XV increasing started. Underlying corrosion also initiated between 80th and 190th day. On the other hand DH2O did not indicate the clear change associated with the degradation. The changes in Rf, Cf, and XV were closely correlated with the progress of the degradation of the coated steels.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
National Maritime Research Institute, National Institute of Maritime, Port and Aviation Technology
Graduate School of Science & Engineering, Tokyo Institute of Technology
References (23)
Show source-provided references
1. 1) H. Emi, M. Yuasa, A. Kumano, N. Yamamoto, T. Arima and M. Umino: J. Soc. Nav. Arch. Jpn. 174 (1993) 735–744. 10.2534/jjasnaoe1968.1993.174_73510.2534/jjasnaoe1968.1993.174_735 ↗
2. 2) M. Asari, T. Tsuru and S. Haruyama: Corros. Eng. (Jpn.) 36 (1987) 134–141.
3. 3) H. Hayashibara, E. Tada and A. Nishikata: ISIJ Int. 56 (2016) 2029–2036. 10.2355/isijinternational.ISIJINT-2016-22810.2355/isijinternational.ISIJINT-2016-228 ↗
4. 4) E.P.M. van Westing, G.M. Ferrari and H.W. de Wit: Corros. Sci. 36 (1994) 979–994. 10.1016/0010-938X(94)90198-810.1016/0010-938X(94)90198-8 ↗
5. 5) L. Valentinelli, J. Vogelsang, H. Ochs and L. Fedrizzi: Prog. Org. Coat. 45 (2002) 405–413. 10.1016/S0300-9440(02)00137-610.1016/S0300-9440(02)00137-6 ↗
6. 6) D.M. Brasher and A.H. Kingsbury: J. Appl. Chem. 4 (1954) 62–72. 10.1002/jctb.501004020210.1002/jctb.5010040202 ↗
7. 7) T. Morozumi and C. Fujiyama: Shikizai 44 (1971) 161–167.
8. 8) E.P.M. van Westing, G.M. Ferrari and J.H.W. de Wit: Corros. Sci. 36 (1994) 957–977. 10.1016/0010-938X(94)90197-X10.1016/0010-938X(94)90197-X ↗
9. 9) M. Hattori: Ph.D Thesis, (Tokyo Institute of Technology, 2011) p.41.
10. 10) K.N. Allahar, B.R. Hinderliter, G.P. Bierwagen, D.E. Tallman and S.G. Croll: Prog. Org. Coat. 62 (2008) 87–95. 10.1016/j.porgcoat.2007.09.01810.1016/j.porgcoat.2007.09.018 ↗
11. 11) B.R. Hinderliter, K.N. Allahar, G.P. Bierwagen, D.E. Tallman and S.G. Croll: J. Electrochem. Soc. 155 (2008) C93–C100. 10.1149/1.282299110.1149/1.2822991 ↗
12. 12) N. Fredj, S. Cohendoz, S. Mallarino, X. Feaugas and S. Touzain: Prog. Org. Coat. 67 (2010) 287–295. 10.1016/j.porgcoat.2009.11.00110.1016/j.porgcoat.2009.11.001 ↗
13. 13) D. Nguyen Dang, B. Peraudeau, S. Cohendoz, S. Mallarino, X. Feaugas and S. Touzain: Electrochim. Acta 124 (2014) 80–89. 10.1016/j.electacta.2013.08.11110.1016/j.electacta.2013.08.111 ↗
14. 14) IMO: Resolution MSC.215(82), Performance standard for protective coatings of dedicated seawater ballast tanks on all new ships and of double-side skin spaces of bulk carriers, (IMO, London, 2006) p.14.
15. 15) F.R. Bichowsky: Heat. Piping Air Cond. 12 (1940) 627–632.
16. 16) J. Li, C.S. Jeffcoate, G.P. Bierwagen, D.J. Mills and D.E. Tallman: Corrosion 54 (1998) 763–771. 10.5006/1.328479710.5006/1.3284797 ↗
17. 17) ISO 20340, Paint and Varnishes–Performance Requirements for Protective Paint Systems for Offshore and Related Structure, (ISO, Geneva, 2009) p.15.
18. 18) C.A. Schiller and W. Strunz: Electrochim. Acta 46 (2001) 3619–3625. 10.1016/S0013-4686(01)00644-210.1016/S0013-4686(01)00644-2 ↗
19. 19) S. Amand, M. Musiani, M.E. Orazem, N. Pébère, B. Tribollet and V. Vivier: Electrochim. Acta 87 (2013) 693–700. 10.1016/j.electacta.2012.09.06110.1016/j.electacta.2012.09.061 ↗
20. 20) H. Katayama, K. Yagi, A. Nishikata and T. Turu: J. Jpn. Inst. Metals 59 (1995) 50–56. 10.2320/jinstmet1952.59.1_5010.2320/jinstmet1952.59.1_50 ↗
21. 21) P. Musto, L. Mascia, G. Ragosta, G. Scarinzi and P. Villano: Polymer 41 (2000) 565–574. 10.1016/S0032-3861(99)00210-410.1016/S0032-3861(99)00210-4 ↗
22. 22) ISO 12944-6, Paints and Varnishes - Corrosion Protection of Steel Structures by Protective Paint Systems - Part 6: Laboratory Performance Test Methods (ISO, Geneva, 1998) p.6.
23. 23) J. Scheirs: Compositional and Failure Analysis of Polymers: A Practical Approach, 1st ed., (John Wiley & Sons, Chichester, 2000) p.330.