Oxygen Distribution in Titanium Single Crystal Fabricated by Optical Floating-Zone Method under Extremely Low Oxygen Partial Pressure
Source abstract
Abstract
This study examines the properties of a titanium single crystal fabricated by the floating-zone-melting process in Ar gas flow atmosphere where the partial pressure of oxygen was maintained extremely low at PO2=∼10−23 atm by the newly developed oxygen pump system. The distribution of solute oxygen atoms in the obtained single crystal exhibited a peculiar gradient. In the early stage of the titanium single crystal growth, the oxygen content in the single crystal (approximately 1600 ppm) was higher than that in the mother ingot (980 ppm). However, as the crystal growth progressed, the oxygen content gradually decreases and then reduced to 660 ppm in the final stage of crystal growth. Such a gradient of oxygen composition was not detected in titanium single crystals fabricated under conventional, commercial Ar gas flow atmosphere. Owing to the unique gradient of oxygen content formed under extremely low oxygen partial pressure, the Vickers hardness of the single crystal decreased gradually along the crystal growth direction.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Division of Materials and Manufacturing Science, Graduate School of Engineering, Osaka University
Nanoelectronics Research Institute, National Institute of Advanced Industrial Science and Technology (AIST)
Canon Machinery INC
Department of Materials Processing, Graduate School of Engineering, Tohoku University
References (17)
Show source-provided references
1. 1) J. Murray and H. A. Wriedt: Alloy Phase Diagrams, ASM handbook vol. 3 ed. by H. Baker, (ASM International, Ohio, 1992) pp. 2-324.
2. 2) J. C. Williams and G. Lütjering: Proc. Titanium Science and Technology ed. by G. Lütjering, U. Zwicker and W. Bunk (Deutsche Gesellschaft für Metallkunde, 1985) pp. 2001–2008.
3. 3) For example, Proc. Ti-2007 JIMIC5, ed. by M. Niinomi, S. Akiyama, M. Hagiwara, K. Ikeda and K. Maruyama, (Science and Technology, 2007) pp. 1-1765.
4. 4) S. Naka, A. Lasalmonie, P. Costa and L. P. Kubin: Philo. Mag. A 57 (1988) 717–740.10.1080/01418618808209916 ↗
5. 5) T. H. Okabe, R. O. Suzuki, T. Oishi and K. Ono: Tetsu to Hagane (in Japanese) 77 (1991) 93–99.10.2355/tetsutohagane1955.77.1_93 ↗
6. 6) H. W. Rosenberg and J. E. Green: Proc. Ti-1992, ed. by I. H. Froes and I. L. Caplan, (Science and Technology, 1993) pp. 2371–2376.
7. 7) H. Miyazaki, Y. Yamakoshi and Y. Shindo: Materia Japan (in Japanese) 33 (1994) 51–54.10.2320/materia.33.51 ↗
8. 8) Y. Yoshimura, Y. Shmizu and Z. Imamura: Proc. Ti-1992, (Science and Technology, 1993) pp. 2459–2464.
9. 9) T. Nakano, K. Hagihara, H. Maki, Y. Umakoshi and M. Niinomi: Proc. Ti-2007 JIMIC5, (Science and Technology, 2007) pp. 1437–1439.
10. 10) K. Hagihara, T. Nakano, A. Sonoura, K. Watanabe, Y. Umakoshi and M. Niinomi: Proc. Ti-2007 JIMIC5, (Science and Technology, 2007) pp. 1445–1447.
11. 11) I. Nagai, N. Shirakawa, S. Ikeda, R. Iwasaki, H. Nishimura and M. Kosaka: Appl. Phys. Lett. 87 (2005) 024105.10.1063/1.1992671 ↗
12. 12) W. L. Finlay and J. A. Snyder: Trans. AIME 188 (1950) 277–286.10.1007/BF03399001 ↗
13. 13) C. Ouchi, H. Iizumi and S. Mitao: Mater. Sci. Eng. A 243 (1998) 186–195.10.1016/S0921-5093(97)00799-5 ↗
14. 14) T. Narushima: J. Japan. Soc. Biomaterials (in Japanese) 23-2 (2005) 86–93.
15. 15) Y. Kobayashi and F. Tsukihashi: High Temp. Mater. Process. 19 (2000) 211–218.10.1515/HTMP.2000.19.3-4.211 ↗
16. 16) H. Niiyama, Y. Tajima, F. Tsukihashi and N. Sano: J. Less-common Met. 169 (1991) 209–216.10.1016/0022-5088(91)90069-G ↗
17. 17) M. W. Chase, Jr.: NIST-JANAF Thermochemical Tables, Fourth Edition, (ACS and AIP, 1998) p. 1735.