Fatigue Property of Ti-5Al-13Ta Alloy Dental Castings in 0.9% NaCl Solution
Source abstract
Abstract
The purpose of this study was to evaluate the fatigue property of Ti-5Al-13Ta alloy castings for dental application since dental prostheses are used under repetitive stress condition. Dumbbell-shaped cast specimens were prepared with a centrifugal casting machine and a magnesia-based mold material. Fatigue test was performed at 310 K in 0.9% NaCl solution under repetitive loading condition with the maximum cycles at 107. As a result, fatigue limit of Ti-5Al-13Ta alloy castings in NaCl solution was about 220 MPa, which was higher than those of CP-Ti, Ti-6Al-4V and Ti-6Al-7Nb alloys, previously reported. Clear striation was observed at the crack propagation area on the fracture surface. The ratio of fatigue limit to UTS was suggested to be 30% for Ti-5Al-13Ta alloy castings; this value was higher than those for Ti-6Al-4V and Ti-6Al-7Nb alloys. It was concluded that Ti-5Al-13Ta alloy castings showed good fatigue property in 0.9% NaCl solution as an α+β high-strength titanium alloy for dental prostheses.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Dental materials and restorations · Orthopaedic implants and arthroplasty
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Institute of Biomaterials and Bioengineering, Tokyo Medical and Dental University
Department of Materials Engineering, The University of Tokyo
References (29)
Show source-provided references
1. 1) R. Strietzel, A. Hosch, H. Kalbfleisch and D. Buch: Biomaterials 19 (1998) 1495–1499.10.1016/S0142-9612(98)00065-9 ↗
2. 2) M. Koike and H. Fujii: Biomaterials 22 (2001) 2931–2936.10.1016/S0142-9612(01)00040-0 ↗
3. 3) D. Iijima, T. Yoneyama, H. Doi, H. Hamanaka and N. Kurosaki: Biomaterials 24 (2003) 1519–1524.10.1016/S0142-9612(02)00533-1 ↗
4. 4) ISO 5832-2, (International Organization for Standardization, Geneva, 1999) pp. 1–3.
5. 5) ISO 5832-3, (International Organization for Standardization, Geneva, 1996) pp. 1–2.
6. 6) ISO 5832-11, (International Organization for Standardization, Geneva, 1994) pp. 1–2.
7. 7) E. P. Lautenschlager and P. Monaghan: Int. Dent. J. 43 (1993) 245–253.
8. 8) P. G. Laing: ASTM STP. 684 (1979) 199–211.10.1520/STP35945S ↗
9. 9) M. F. Semlitsch, H. Weber, R. M. Streicher and R. Schon: Biomaterials 13 (1992) 781–788.10.1016/0142-9612(92)90018-J ↗
10. 10) E. Kobayashi, T. J. Wang, H. Doi, T. Yoneyama and H. Hamanaka: J. Mater. Sci. Mater. Med. 9 (1998) 567–574.10.1023/A:1008909408948 ↗
11. 11) T. J. Wang, E. Kobayashi, H. Doi and T. Yoneyama: J. Med. Dent. Sci. 46 (1999) 13–19.
12. 12) H. Matsumura, T. Yoneyama and S. Shimoe: J. Prosthet. Dent. 88 (2002) 636–639.10.1067/mpr.2002.129996 ↗
13. 13) V. Srimaneepong, T. Yoneyama, N. Wakabayashi, E. Kobayashi, T. Hanawa and H. Doi: Dent. Mater. J. 23 (2004) 497–503.10.4012/dmj.23.497 ↗
14. 14) A. S. Aronson, N. Jonsson and P. Alberius: Skeletal Radiol. 14 (1985) 207–211.10.1007/BF00355566 ↗
15. 15) H. Zitter and H. Plenk Jr.: J. Biomed. Mater. Res. 21 (1987) 881–896.10.1002/jbm.820210705 ↗
16. 16) J. D. Cotton, J. F. Bingert, P. S. Dunn and R. A. Patterson: Metall. Mater. Trans. A 25 (1994) 461–472.10.1007/BF02651588 ↗
17. 17) H. Doi, T. Yoneyama, E. Kobayashi and H. Hamanaka: J. Jpn. Dent. Mater. 17 (1998) 247–252.
18. 18) T. Mizumoto, M. Niinomi, Y. Nakano, T. Akahori and H. Fukui: Mater. Trans. 43 (2002) 3160–3166.10.2320/matertrans.43.3160 ↗
19. 19) T. Akahori, M. Niinomi, H. Fukui and A. Suzuki: Mater. Trans. 45 (2004) 1540–1548.10.2320/matertrans.45.1540 ↗
20. 20) Y. Okazaki, E. Gotoh, H. Nakada and K. Kobayashi: Mater. Trans. 46 (2005) 1545–1550.10.2320/matertrans.46.1545 ↗
21. 21) Gunawarman, M. Niinomi, T. Akahori, T. Souma, M. Ikeda, H. Toda and K. Terashima: Mater. Trans. 46 (2005) 1570–1577.10.2320/matertrans.46.1570 ↗
22. 22) Y. Okazaki and H. Gotoh: Mater. Trans. 43 (2002) 2949–2955.10.2320/matertrans.43.2949 ↗
23. 23) N. Maruyama, K. Nakazawa and T. Hanawa: Mater. Trans. 43 (2002) 3118–3121.10.2320/matertrans.43.3118 ↗
24. 24) N. Maruyama, S. Hiromoto, M. Ohnuma and T. Hanawa: Mater. Trans. 45 (2004) 1233–1238.10.2320/matertrans.45.1233 ↗
25. 25) H. Doi: J. Jpn. Dent. Mater. 18 (1999) 368–374.
26. 26) E. J. Czryca and D. Taylor: ASM Handbook, Vol. 8, (ASM International, Materials Park, Ohio, USA, 1985) pp. 686–708.
27. 27) ISO 13782, (International Organization for Standardization, Geneva, 1996) pp. 1–2.
28. 28) P. Ducheyne, D. Kohn and T. S. Smith: Biomaterials 8 (1987) 223–227.10.1016/0142-9612(87)90068-8 ↗
29. 29) J. Kasuga, T. Yoneyama, E. Kobayashi, T. Hanawa and H. Doi: Mater. Trans. 46 (2005) 1555–1563.10.2320/matertrans.46.1555 ↗