journal article·2006Open access

A Study on the Low Temperature Internal Friction Relaxation Peak in a Ti49.8Ni50.2 Alloy

Shyi-Kaan Wu, Hsin-Chih Lin, Tung-Sheng Chou

MATERIALS TRANSACTIONS· Volume 47· Issue 3

Abstract

The low temperature relaxation peak appearing around 200 K in Ti49.8Ni50.2 shape memory alloy is a multiple relaxation process with activation energy Q=0.39 eV and frequency factor f0=6.2×109 s−1 and is associated with the interaction of dislocations with pinning vacancies. Due to the increase of dislocation density and the annihilation of quenched-in vacancies after thermal cycling, the height of relaxation peak PR decreases with increasing the number of thermal cycling. Higher amounts of dislocation-vacancy reaction cause a higher relaxation damping under the condition of higher quenching temperature. The quenched-in vacancies can have a significant effect on the transformation rate, and thus the heights of transformation peaks PH1 and PC1 decrease with increasing quenching temperature. Dislocations introduced by both thermal cycling and quenching from high temperature will depress the martensitic transformation, and hence decrease the peak temperatures of PH1 and PC1.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Shape Memory Alloy Transformations · Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials Science and Engineering, National Taiwan University

Silitech Technology Corporation

References (14)

Show source-provided references
1. 1) K. Iwasaki and R. Hasiguti: Trans. JIM 28 (1987) 363.10.2320/matertrans1960.28.363 ↗
2. 2) N. Y. Chui and Y. T. Huang: Scr. Met. 21 (1987) 447.10.1016/0036-9748(87)90178-5 ↗
3. 3) S. K. Wu, H. C. Lin and T. S. Chou: Acta Met. 38 (1990) 95.10.1016/0956-7151(90)90137-6 ↗
4. 4) H. C. Lin, S. K. Wu and T. S. Chou: Acta Met. 39 (1991) 2069.10.1016/0956-7151(91)90177-3 ↗
5. 5) J. S. Zhu, R. Schaller and W. Benoit: Phys. Lett. A 141 (1989) 177.10.1016/0375-9601(89)90784-6 ↗
6. 6) J. S. Kochler: Imperfections in Nearly Perfect Crystals, (Wiley, New York, 1952) Chap. 7.
7. 7) A. V. Granato and K. Lücke: J. Appl. Phys. 52 (1981) 7136.10.1063/1.328687 ↗
8. 8) T. S. Chou, S. K. Wu and H. C. Lin: Scr. Mater. 38 (1998) 363.10.1016/S1359-6462(97)00502-2 ↗
9. 9) S. H. Chang and S. K. Wu: Scr. Mater. 50 (2004) 937.10.1016/j.scriptamat.2004.01.009 ↗
10. 10) A. S. Nowick and B. S. Berry: Anelastic Relaxation in Crystalline Solids, (Academic Press, New York, 1972) pp. 52.
11. 11) H. C. Lin, S. K. Wu and T. S. Chou: J. Alloys Compd. 355 (2003) 90.10.1016/S0925-8388(03)00283-4 ↗
12. 12) I. Yoshida and K. Otsuka: Program of 2nd International Symp. on High Damping Materials 2005 (HDM-2, 2005), Kyoto, Japan, pp. 18.
13. 13) S. Miyazaki, Y. Igo and K. Otsuka: Acta Met. 34 (1986) 2045.10.1016/0001-6160(86)90263-4 ↗
14. 14) J. F. Delorme, R. Schmid, M. Robin and P. Gobin: J. De Physique 32 (1971) C2-101.10.1051/jphyscol:1971221 ↗