journal article·2009Open access

Electric Flame-Off Characteristics and Fracture Properties of 20 μm Thin Copper Bonding Wire

Fei-Yi Hung, Truan-Sheng Lui, Li-Hui Chen, Yi-Chang Lin

MATERIALS TRANSACTIONS· Volume 50· Issue 2

Abstract

In the present study, the neck fracture properties of annealed wire with φ=20 μm (0.8 mil) at 225°C for 1 hour and un-annealed wire were compared. In addition, the microstructural characteristics, the mechanical properties and the texture transition using EBSD methods before and after an electric flame-off (EFO) process were also studied. Experimental results indicate that the recrystallization temperature of the as-drawn wire was ∼225°C, and the annealed copper wires possessed a fully annealed structure. Through recrystallization, the matrix structure transferred from long, thin grains to equiaxed grains and a few annealed twins. The microstructure of the free air ball (FAB) after an EFO process consisted of column-like grains, and grew from the heat-affected zone (HAZ) to the Cu ball. For the annealed and un-annealed wires, their preferred orientations on the wire and the neck were 〈100〉||AD. Under the thermal effect of EFO, the orientation of the Cu balls were mainly 〈101〉||AD and 〈111〉||AD for annealed wires. Additionally, the hardness of the Cu balls and the strength of the neck sites of the EFO wires were able to affect the reliability of the copper wire bonding.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Combustion and Detonation Processes · High-Velocity Impact and Material Behavior · Fire effects on concrete materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute of Nanotechnology and Microsystems Engineering, Center for Micro/Nano Science and Technology, National Cheng Kung University

Department of Materials Science and Engineering, National Cheng Kung University

References (15)

Show source-provided references
1. 1) F. Wulff, C. D. Breach and K. Dittmer: J. Mater. Sci. Lett. 22 (2003) 1373–1376.10.1023/A:1025751714880 ↗
2. 2) N. Murali, N. Srikanth and C. J. Vath III: Mater. Res. Bull. 38 (2003) 637–646.10.1016/S0025-5408(03)00004-7 ↗
3. 3) N. Srikanth, S. Murali, Y. M. Wong and C. J. Vath III: Thin Solid Films 462 (2004) 339–345.10.1016/j.tsf.2004.05.116 ↗
4. 4) Properties and Selection: Nonferrous Alloys and Pure Metals, Metals Handbook, Ninth Edition, Volume 2.
5. 5) H. M. Ho, W. Lam, S. Stoukatch, P. Ratchev, C. J. Vath III and E. Beyne: Microelectron. Reliab. 43 (2003) 912–923.10.1016/S0026-2714(03)00074-X ↗
6. 6) S. Murali, N. Srikanth and C. J. Vath III: Mater. Charact. 50 (2003) 39–50.10.1016/S1044-5803(03)00102-5 ↗
7. 7) A. Saboui: IEEE/CHMT IEMT Symposium, (1991) pp. 75–79.
8. 8) F. Y. Hung, T. S. Lui, L. H. Chen and Y. T. Wang: J. Mater. Sci. 42 (2007) 5476–5482.10.1007/s10853-006-0883-0 ↗
9. 9) S. Jakani, T. Baudin, C. H. de Novion and M. H. Mathon: Mater. Sci. Eng. A 456 (2007) 261–269.10.1016/j.msea.2006.11.137 ↗
10. 10) P. Ratchev, S. Stoukatch and B. Swinnen: Microelectron. Reliab. 46 (2006) 1315–1325.10.1016/j.microrel.2005.11.002 ↗
11. 11) F. Wulff, C. D. Breach and K. Dittmer: J. Mater. Sci. Lett. 22 (2003) 1373–1376.10.1023/A:1025751714880 ↗
12. 12) M. R. Koblischka and A. Koblischka-Veneva: Phys. C 392–396 (2003) 545–556.10.1016/S0921-4534(03)00850-5 ↗
13. 13) Z. W. Zhong, H. M. Ho, Y. C. Tan, W. C. Tan, H. M. Goh, B. H. Toh and J. Tan: Microelectron. Eng. 84 (2007) 368–374.10.1016/j.mee.2006.11.003 ↗
14. 14) S. Murali, N. Srikanth and C. J. Vath III: Microelectron. Reliab. 46 (2006) 467–475.10.1016/j.microrel.2005.05.011 ↗
15. 15) F. Wullf, C. D. Breach and K. Dittmer: J. Mater. Sci. Lett. 22 (2003) 1373–1376.10.1023/A:1025751714880 ↗