Magnetic Properties of SmFe3-Type Sm–Zr–Fe–Co–Ti Melt-Spun Ribbons
Source abstract
Abstract
The magnetic properties and structures of (Sm,Zr)5(Fe,Co)17−xTix (x = 0–2.0) melt-spun ribbons were investigated in the as-quenched condition and after annealing. The as-quenched (Sm,Zr)5(Fe,Co)17−xTix (x = 0–0.5) specimens consisted of the Sm5Fe17-type and SmFe3-type phases, while the as-quenched (Sm,Zr)5(Fe,Co)17−xTix (x = 1.0–2.0) specimens contained the SmFe3-type phase. These specimens showed low coercivity regardless of the Ti content. Heat treatment of the melt-spun ribbons resulted in a drastic increase in coercivity. The maximum coercivity of 1.11 MAm−1 was achieved in the (Sm,Zr)5(Fe,Co)15.5Ti1.5 specimen annealed at 1073 K. Microstructural studies revealed that the annealed specimen consisted mainly of the SmFe3-type phase. The achieved high coercivity of the annealed specimen was therefore attributed to the existence of the SmFe3-type phase.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Magnetic Properties of Alloys · Magnetic properties of thin films · Metallic Glasses and Amorphous Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Advanced Materials Science and Engineering, Chiba Institute of Technology
Graduate School of Engineering, Chiba Institute of Technology
Institute for Solid State Physics, The University of Tokyo
References (18)
Show source-provided references
1. 1) C. Lin, C.X. Liu, Y.X. Sun and Z.X. Liu: J. Phys. Condens. Matter 9 (1997) 9353–9360.10.1088/0953-8984/9/43/019 ↗
2. 2) N. Kamprath, N.C. Liu, H. Hegde and F.J. Cadieu: J. Appl. Phys. 64 (1988) 5720–5722.10.1063/1.342237 ↗
3. 3) Z. Chu, W.B. Yelom, F.P. Missel and R.K. Murakami: J. Appl. Phys. 87 (2000) 6704–6706.10.1063/1.372814 ↗
4. 4) R.K. Murakami, V. Villas-Boas, J.M. Filho, H.R. Rechenberg and F.P. Missel: J. Alloys Compd. 443 (2007) 1–6.
5. 5) F. Maruyama and Y. Amako: J. Alloys Compd. 474 (2009) 1–3.
6. 6) Y. Luo, D. Yu, H. Li, W. Zhuang, Y. Mao, X. Chen, K. Li and Y. Liu: J. Rare Earths 32 (2014) 960–964.10.1016/S1002-0721(14)60169-1 ↗
7. 7) K. Schnitzke, L. Schultz, J. Wecker and M. Katter: Appl. Phys. Lett. 56 (1990) 587–589.10.1063/1.103306 ↗
8. 8) T. Saito: J. Alloys Compd. 440 (2007) 315–318.10.1016/j.jallcom.2006.09.011 ↗
9. 9) T. Saito: Appl. Phys. Lett. 91 (2007) 072503.10.1063/1.2768908 ↗
10. 10) T. Saito and T. Furutani: J. Alloys Compd. 488 (2009) 13–17.10.1016/j.jallcom.2009.08.074 ↗
11. 11) T. Saito and D. Nishio-Hamane: IEEE Trans. Magn. 49 (2013) 3345–3348.10.1109/TMAG.2013.2245307 ↗
12. 12) K.H.J. Buschow: J. Less Common Met. 25 (1971) 131–134.10.1016/0022-5088(71)90124-X ↗
13. 13) J.F. Herbst and J.J. Croat: J. Appl. Phys. 53 (1982) 4304–4308.10.1063/1.331207 ↗
14. 14) H. Samata, N. Fujiwara, Y. Shimizu, Y. Nagata, T. Uchida and M.D. Lan: Jpn. J. Appl. Phys. 36 (1997) 3492–3496.10.1143/JJAP.36.3492 ↗
15. 15) L. Schultz, K. Schnitzke, J. Wecker and M. Katter: IEEE Trans. Magn. 26 (1990) 1373–1375.10.1109/20.104382 ↗
16. 16) J. Wecker, M. Katter, K. Schnitzke and L. Schultz: J. Appl. Phys. 69 (1991) 5847–5849.10.1063/1.348911 ↗
17. 17) T. Kuno, S. Suzuki, K. Urushibata, K. Kobayashi, N. Sakuma, M. Yano, A. Kato and A. Manabe: AIP Adv. 6 (2016) 025221.10.1063/1.4943051 ↗
18. 18) T. Saito and T. Horita: AIP Adv. 8 (2018) 056228.10.1063/1.5006208 ↗