Preparation of White Heart Malleable Cast Iron in Na2O–SiO2 Oxide Molten Salt
Source abstract
Abstract
The preparation process of white heart malleable cast iron in Na2O–SiO2 oxide molten salts was studied. We investigated the effect of the molten salt composition on the decarburization of white cast iron. A specimen of white cast iron (φ8mm×8mm) containing 3.34 mass% carbon was immersed in a Na2O–SiO2 molten salt at 1323 K for 24–72 h. After the heat treatment of white cast iron in Na2O–SiO2 (64–36 mol%) at 1323 K for 48 h, low-carbon surface layer had a thickness of about 100 μm and contained 0.53 mass% carbon. This surface layer was formed as a result of the reaction of carbon in white cast iron with free oxygen in the oxide molten salt. However, no decarburized layer was observed on the specimen surface after the heat treatment in the Na2O–SiO2 (38–62 mol%) molten salt. As the Na2O composition increased within the limit of 41 < Na2O (mol%) ≤ 65, the thickness of the decarburized layer also increased. It was found that white heart malleable cast iron could be prepared from white cast iron in Na2O–SiO2 oxide molten salts, and the degree of decarburization depended on the composition of the molten salts.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Materials Engineering and Processing · Glass properties and applications · Pigment Synthesis and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials Science and Chemistry, Graduate School of Engineering, University of Hyogo
References (17)
Show source-provided references
1. 1) S. Tanaka, M. Isakawa and H. Nagasaki: Kensagijutsu 10 (2005) 50–54.
2. 2) The Iron and Steel Institute of Japan: Handbook of Iron and Steel 3rd edition V, (Maruzen, Tokyo, 1982) pp. 116.
3. 3) The Japan Institute of Materials: KinzokuBinran 5th edition, (Maruzen, Tokyo, 1990) pp. 595.
4. 4) K. Monma: Tekkouzairyougaku, (Jikkyo shuppan, Tokyo, 1992) pp. 524.
5. 5) R. S. Roth, T. Negas and L. P. Cook: PHASE DIAGRAMS FOR CERAMISTS VOLUME IV, (THE AMERICAN CERAMIC SOCIETY, Columbus, 1981) pp. 87.
6. 6) J. Loeffler: Glastech. Ber. 42 (1969) 92–96.10.1093/forestry/42.1.92 ↗
7. 7) K. Morinaga, H. Yoshida and H. Takebe: J. Am. Ceram. Soc. 77 (1994) 3113–3118.10.1111/j.1151-2916.1994.tb04557.x ↗
8. 8) J. A. Duffy and M. D. Ingram: J. Am. Chem. Soc. 93 (1971) 6448–6454.10.1021/ja00753a019 ↗
9. 9) G. W. Toop and C. S. Samis: Trans. Met. Soc. AIME 224 (1962) 878–887.
10. 10) T. Yokogawa and K. Niwa: Trans. JIM 10 (1969) 3–7.10.2320/matertrans1960.10.3 ↗
11. 11) M. Susa: Bull. Iron Steel Inst. Jpn. 3 (1998) 595–601.
12. 12) H. Lux: Z. Elektrochem. 45 (1939) 303–309.10.1002/bbpc.19390450405 ↗
13. 13) H. Flood and T. Forland: Acta Chem. Scand. 1 (1947) 592–604.10.3891/acta.chem.scand.01-0592 ↗
14. 14) B. E. Warren and A. G. Pincus: J. Am. Ceram. Soc. 23 (1940) 301–304.10.1111/j.1151-2916.1940.tb14194.x ↗
15. 15) Y. Suginohara, T. Yanagase and H. Ito: Trans. JIM 3 (1962) 227–233.10.2320/matertrans1960.3.227 ↗
16. 16) T. Yanagase and Y. Suginohara: TETSU-TO-HAGANE 57 (1971) 142–157.10.2355/tetsutohagane1955.57.1_142 ↗
17. 17) Y. Waseda and H. Suito: Trans. ISIJ 17 (1977) 82–91.10.2355/isijinternational1966.17.82 ↗