Abstract
The purpose of this study is to investigate the influence of chunky graphite on the characteristics of fatigue crack propagation in heavy section spheroidal graphite cast iron. Samples containing and not containing chunky graphite were cut from a large ingot of spheroidal graphite cast iron. The fatigue crack propagation test conformed to ASTM. Stress ratio R was 0.1, and the specimen used was of the 1CT type with a thickness of 12.5 mm, and humidity RH = 0%.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fatigue and fracture mechanics · Engineering Applied Research · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Graduate Student, Tokyo City University
Faculty of Engineering, Tokyo City University
Toshiba Machine Co. LTD.
References (26)
Show source-provided references
1. 1) S. Yamada and S. Tsukahara: Heat Treatment and Mechanical Properties of Cast Iron, (AGNE Gijutsu Center, Tokyo, 2004) p. 2.
2. 2) Y. Yamada, T. Nishio, K. Yasue, Y. Kondo, H. Takeo and M. Kawai: IMONO 65 (1993) 237–242.
3. 3) K. Ohji: Fracture Strength, (Ohmsha, Tokyo, 1985) p. 194.
4. 4) Y. Sugiyama, K. Asami and S. Tabata: IMONO 66 (1994) 833–839.
5. 5) Y. Sugiyama, K. Asami and S. Tabata: IMONO 67 (1995) 190–196.10.1515/9783486782967-020 ↗
6. 6) H. Usami, Y. Sugiyama, N. Shiraki and M. Funamoto: J. JFS 74 (2002) 714–719.
7. 7) N. Shiraki and Y. Atsumi: J. JFS 79 (2007) 83–89.
8. 8) N. Shiraki and T. Kanno: J. JFS 82 (2010) 86–91.10.1177/003172171009100421 ↗
9. 9) N. Shiraki and K. Morita: Mater. Trans. 56 (2015) 1226–1232.10.2320/matertrans.F-M2015812 ↗
10. 10) H. Nakae and H. Kiyosuke: IMONO 55 (1983) 603–608.
11. 11) O. Tsumura: J. JFS 76 (2004) 125–129.10.1055/s-2004-818740 ↗
12. 12) H. Nakae, H.-C. Shin, M. Hara and Y. Harada: J. JFS 75 (2003) 337–343.
13. 13) H. Nakae: J. JFS 76 (2004) 107–113.
14. 14) S. Kiguchi: J. JFS 76 (2004) 114–118.10.1002/cite.200403279 ↗
15. 15) S. Kiguchi, M. Sintani, H. Sumimoto and K. Nakamura: J. JFS 72 (2000) 311–316.
16. 16) H. Itofuji and A. Masutani: J. JFS 76 (2004) 98–106.
17. 17) R. Fujimoto, S. Hiratsuka, H. Horie and T. Hareyama: J. JFS 86 (2014) 712–718.
18. 18) S. Kiguchi, T. Ishikawa, H. Sumimoto and K. Nakamura: J. JFS 73 (2001) 173–177.
19. 19) Y. Nagai, R. Morimoto, H. Hirahara, Y. Naya, H. Kage and H. Kato: J. JFS 76 (2004) 86–92.
20. 20) JIS Z 2241: Metallic materials-Tensile testing-Method of test at room temperature (2011).
21. 21) ASTM E647-81 (1981).
22. 22) J.E. Srawley: Int. J. Fract. 12 (1976) 475–476.10.1007/BF00032844 ↗
23. 23) J.E. Newman: ASTM Spec. Tech. Publ. 560 (1974) 105–121.
24. 24) S. Harada, T. Kobayashi, T. Noguchi, H. Suzuki and M. Yano: Strength Evaluation of Spheroidal Graphite Cast Iron, (AGNE Gijutsu Center, Tokyo, 1999) p. 147.
25. 25) M. Jono and J. Song: Fatigue Crack Crack Opening and Closing and Propagation Rate Estimation Method, (Osaka University Press, Osaka, 2005) p. 17.
26. 26) T. Chin: Metal Fatigue Strength Fatigue Crack Generation and Propagation, (Uchida Rokakuho, Tokyo, 2015) p. 100.