journal article·2004Open access

Oxidation Resistance of TiAl Improved by Ion Implantation of Beta-Former Elements

Shigeji Taniguchi, Michiko Yoshihara, Kazuhisa Fujita

MATERIALS TRANSACTIONS· Volume 45· Issue 5

Abstract

TiAl coupon specimens were implanted with Fe, Mo, Ta or W ions and then cyclically oxidised with temperature varying between room temperature and 1200 K in a flow of purified oxygen under atmospheric pressure. The surface modification by the ion implantation was characterised by glancing angle X-ray diffractometry (GAXRD), Auger electron spectroscopy (AES) and transmission electron microscopy (TEM). The oxidised specimens were examined by AES, GAXRD, X-ray diffractometry, scanning electron microscopy and electron probe microanalysis. The oxidation resistance of TiAl is significantly improved by the implantation of Mo, Ta or W ions with a dose of 1021 ions·m&minus2; at acceleration voltages ranging from 50 to 340 kV. The acceleration voltage has a small influence. The oxide scales consist predominantly of α-Al2O3 and are very adherent to the substrates even after 20 cycles (400 h). On the other hand, the implantation of Fe has a little effect. The significant effect brought about by the implantation is attributable to the formation of a thin β-Ti phase layer in the modified area. Therefore, a possible explanation for the improved oxidation resistance is the formation of β-Ti phase, which is a solid solution where diffusion of Al seems much faster than in γ-TiAl which has an ordered structure. The enhanced Al diffusion results in the formation of a thin but continuous Al2O3-rich layer in the scale during the initial oxidation stages. The enrichment of Al relative to Ti by the implantation was thought playing some role. The so-called doping effect of Mo, Ta and W is also contributing to the early formation of Al2O3-rich layers by retarding TiO2 growth.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Energetic Materials and Combustion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials Science and Processing, Graduate School of Engineering, Osaka University

Department of Mechanical Engineering and Materials Science, Yokohama National University

3rd Project Research Laboratory, Ion Engineering Research Institute Corporation

References (15)

Show source-provided references
1. 1) T. Noda: Intermetallics 6 (1998) 709-713.10.1016/S0966-9795(98)00060-0 ↗
2. 2) T. Tetsui and S. Ono: Intermetallics 7 (1999) 689-697.10.1016/S0966-9795(98)00085-5 ↗
3. 3) Y.-W. Kim, R. Wagner and M. Yamaguchi: Proc. Gamma Titanium Aluminides, (TMS, 1995).
4. 4) Y.-W. Kim, D.M. Dimiduk and M.H. Loretto: Proc. Gamma Titanium Aluminides, (TMS, 1999).
5. 5) J.S. Williams and J.M. Poate: Ion Implantation and Beam Processing, (Academic Press, New York, 1984).
6. 6) H. Ryssel and I. Ruge: Ion Implantation, (John Wiley & Sons, New York, 1986).
7. 7) S. Taniguchi, K. Uesaki, Y.-C. Zhu, H.-X. Zhang and T. Shibata: Mater. Sci. Eng. A249 (1998) 223-232.10.1016/S0921-5093(98)00567-X ↗
8. 8) S. Taniguchi, Y.-C. Zhu, K. Fujita and N. Iwamoto: Oxid. Met. 58 (2002) 375-390.10.1023/A:1020115006816 ↗
9. 9) S. Taniguchi, T. Shibata and S. Itoh: Mater. Trans., JIM 32 (1991) 151-156.10.2320/matertrans1989.32.151 ↗
10. 10) S. Becker, A. Rahmel, M. Schorr and M. Schütze: Oxid. Met. 38 (1992) 425-464.10.1007/BF00665663 ↗
11. 11) K. Hashimoto, M. Miura and Y. Mizuhara: Intermetallics 6 (1998) Issues 7-8, pp.667-672.10.1016/S0966-9795(98)00048-X ↗
12. 12) N. Zheng, W. Fischer, H. Grubmeier, V. Shemet and W.J. Quadakkers: Scr. Metall. Mater. 33 (1995) 47-53.10.1016/0956-716X(95)00155-O ↗
13. 13) M. Koiwa, H. Nakajima and T. Ito: Bull. Japan Inst. Metals 28 (1989) 723-731. (in Japanese)10.2320/materia1962.28.723 ↗
14. 14) H. Nakajima and M. Koiwa: ISIJ Inter. 31 (1991) 757-766.10.2355/isijinternational.31.757 ↗
15. 15) K. Hauffe: Progress in Metal Physics. 4, (Pergamon Press, London, 1953) 88-89.10.1016/0502-8205(53)90015-X ↗