Microstructures in Heat Treated LPBF Ti-6Al-4V Alloys after α′ phase Decomposition and their Mechanical Properties
Source abstract
Abstract
Alloys formed by laser power bed fusion (LPBF) contain high residual stress and strain due to the cyclic heating process, which decreases ductility. Therefore, many researchers have investigated heat treatments to improve ductility by removing residual stress and forming α + β phase structures. However, in this study the ductility of some heat-treated samples was found to decrease below that of as-built samples. This study investigated the heat treatment of LPBF at different temperatures to decompose α′ grains to α grains and understand the resulting microstructure and mechanical properties. Specifically, the influence of microstructural factors on ductility was examined. In the samples heat treated at 500°C, α′ was found to decompose into α with elevated strain and finer β grains, which increased yield strength at the cost of ductility. Meanwhile, in the samples heat treated at 700°C, coarser β phase was precipitated, and greater ductility was supported by the transfer of the slip deformation between α phase grains.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Surface Treatment and Residual Stress
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Dept. of Mechanical Engineering, Graduate School of Engineering, the University of Osaka
Joining and Welding Research Institute, the University of Osaka
School of Materials Science and Engineering, Xi’an University of Technology
Institute of Process Engineering, Chinese Academy of Sciences
References (15)
Show source-provided references
1. 1) N. Singh, H. Siddiqui, B.S.R. Koyalada, A. Mandal, V. Chauhan, S. Natarajan, S. Kumar, M. Goswami and S. Kumar: Recent Advancements in Additive Manufacturing (AM) Techniques: A Forward-Looking Review, Met. Mater. Int. 29 (2023) 2119–2136. doi:10.1007/s12540-022-01380-910.1007/s12540-022-01380-9 ↗
2. 2) M.K. Thompson, G. Moroni, T. Vaneker, G. Fadel, R.I. Campbell, I. Gibson, A. Bernard, J. Schulz, P. Graf, B. Ahuja and F. Martina: Design for Additive Manufacturing: Trends, opportunities, considerations, and constraints, CIRP Ann. 65 (2016) 737–760. doi:10.1016/j.cirp.2016.05.00410.1016/j.cirp.2016.05.004 ↗
3. 3) C. Zhang, Y. Li, W. Kang, X. Liu and Q. Wang: Current advances and future perspectives of additive manufacturing for functional polymeric materials and devices, SusMat 1 (2021) 127–147. doi:10.1002/sus2.1110.1002/sus2.11 ↗
4. 4) C.Y. Yap, C.K. Chua, Z.L. Dong, Z.H. Liu, D.Q. Zhang, L.E. Loh and S.L. Sing: Review of selective laser melting: Materials and applications, Appl. Phys. Rev. 2 (2015) 041101. doi:10.1063/1.493592610.1063/1.4935926 ↗
5. 5) K.S. Al-Rubaie, S. Melotti, A. Rabelo, J.M. Paiva, M.A. Elbestawi and S.C. Veldhuis: Machinability of SLM-produced Ti6Al4V titanium alloy parts, J. Manuf. Process. 57 (2020) 768–786. doi:10.1016/j.jmapro.2020.07.03510.1016/j.jmapro.2020.07.035 ↗
6. 6) T. Vilaro, C. Colin and J.D. Bartout: As-Fabricated and Heat-Treated Microstructures of the Ti-6Al-4V Alloy Processed by Selective Laser Melting, Metall. Mater. Trans. A 42 (2011) 3190–3199. doi:10.1007/s11661-011-0731-y10.1007/s11661-011-0731-y ↗
7. 7) B. Vrancken, L. Thijs, J. Kruth and J. Humbeeck: Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties, J. Alloy. Compd. 541 (2012) 177–185. doi:10.1016/j.jallcom.2012.07.02210.1016/j.jallcom.2012.07.022 ↗
8. 8) J. Sarma, R. Kumar, A.K. Sahoo and A. Panda: Enhancement of material properties of titanium alloys through heat treatment process: A brief review, Mater. Today Proc. 23 (2020) 561–564. doi:10.1016/j.matpr.2019.05.40910.1016/j.matpr.2019.05.409 ↗
9. 9) F.F. Dear, P. Kontis, B. Gault, J. Ilavsky, D. Rugg and D. Dye: Mechanisms of Ti3Al precipitation in hcp α-Ti, Acta Mater. 212 (2021) 116811. doi:10.1016/j.actamat.2021.11681110.1016/j.actamat.2021.116811 ↗
10. 10) C. Cayron: Diffraction artefacts from twins and stacking faults, and the mirage of hexagonal, polytypes or other superstructures, Scr. Mater. 194 (2021) 113629. doi:10.1016/j.scriptamat.2020.11.01410.1016/j.scriptamat.2020.11.014 ↗
11. 11) K. Kondoh, E. Ichikawa, A. Issariyapat, K. Shitara, J. Umeda, B. Chen and S. Li: Tensile property enhancement by oxygen solutes in selectively laser melted titanium materials fabricated from pre-mixed pure Ti and TiO2 powder, Mater. Sci. Eng. A 795 (2020) 139983. doi:10.1016/j.msea.2020.13998310.1016/j.msea.2020.139983 ↗
12. 12) M.A. Galindo-Fernández, K. Mumtaz, P.E.J. Rivera-Díaz-del-Castillo, E.I. Galindo-Nava and H. Ghadbeigi: A microstructure sensitive model for deformation of Ti-6Al-4V describing Cast-and-Wrought and Additive Manufacturing morphologies, Mater. Des. 160 (2018) 350–362. doi:10.1016/j.matdes.2018.09.02810.1016/j.matdes.2018.09.028 ↗
13. 13) K. Sato, H. Matsumoto, A. Chiba and T.J. Konno: Aging Effect on Microstructure of Cold Groove-Rolled α′-Type Ti–12 mass%V–2 mass%Al Alloys Studied by Transmission Electron Microscopy, Mater. Trans. 55 (2014) 763–767. doi:10.2320/matertrans.M201346310.2320/matertrans.M2013463 ↗
14. 14) S. Cao, R. Chu, X. Zhou, K. Yang, Q. Jia, C. Lim, A. Huang and X. Wu: Role of martensite decomposition in tensile properties of selective laser melted Ti-6Al-4V, J. Alloy. Compd. 744 (2018) 357–363. doi:10.1016/j.jallcom.2018.02.11110.1016/j.jallcom.2018.02.111 ↗
15. 15) M. Simonelli, Y.Y. Tse and C. Tuck: Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V, Mater. Sci. Eng. A 616 (2014) 1–11. doi:10.1016/j.msea.2014.07.08610.1016/j.msea.2014.07.086 ↗