journal article·2026-02-01

Effects of Al and Si Additives on the Passivation Behavior of 11Cr Stainless Steels

Masatoshi Abe, Akinori Kawano, Toru Matsuhashi, Nobuhiko Hiraide, Jun-ichi Hamada, Akira Nagaoka, Eri Hoshiba, Akihiro Fujimura, Koji Fushimi

MATERIALS TRANSACTIONS· Volume 67· Issue 2
Publisher page

Abstract

In sulfate or chloride ion environments, the current density in the active/passive transition in Fe-11 mass% Cr steels decreases with the addition of 2 mass% Al or Si. This reduced current density lowers passivation pH; consequently, the corrosion resistance of the Al/Si-added Fe-11 mass% Cr steel is superior to that of the Fe-11 mass% Cr steel. The Al (or Si) content in the passive film formed on Fe-11 mass% Cr-2 mass% Al (or -2 mass% Si), is higher than that in the substrate. The excellent corrosion resistance of the Al-added low-Cr stainless steel is attributed to the generation of Al(III) hydroxides, which dominates over that of Fe(II) and Cr(III). By contrast, the excellent corrosion resistance of the Si-added low-Cr stainless steel is ascribed to the formation of Si oxides.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Electrodeposition and Electroless Coatings

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

NIPPON STEEL Stainless Steel Corporation

NIPPON STEEL TECHNOLOGY Co., Ltd.

Graduate School of Chemical Sciences and Engineering, Hokkaido University

Faculty of Engineering, Hokkaido University

References (35)

Show source-provided references
1. 1) S. Morioka: Corrosion-resistant steel materials part 1, Boshoku Gijutsu (presently Corrosion Engineering) 9 (1960) 274–278. doi:10.3323/jcorr1954.9.6_27410.3323/jcorr1954.9.6_274 ↗
2. 2) N. Hiraide, H. Matsuyama, T. Matsuhashi, H. Kajimura and N. Hara: Effect of Sn for ferritic stainless steels on corrosion resistance in sulfuric acid solutions, Zairyo-to-Kankyo (presently Corrosion Engineering) 66 (2017) 361–368. doi:10.3323/jcorr.66.36110.3323/jcorr.66.361 ↗
3. 3) ISO 15510: Stainless steels – Chemical composition, (ISO, 2010).
4. 4) Elements, Terrestrial Abundance, [Accessed March 24, 2025].
5. 5) H. Ike, H. Okabe and E. Tsuji: The oxidation behavior of Fe-14Cr alloys with low Al contents at high temperatures, J. Jpn. Inst. Met. Mater. 42 (1978) 509–517. doi:10.2320/jinstmet1952.42.5_50910.2320/jinstmet1952.42.5_509 ↗
6. 6) G.C. Wood, J.A. Richardson, M.G. Hobby and J. Boustead: The identification of thin healing layers at the base of oxide scales on Fe-Cr base alloys, Corros. Sci. 9 (1969) 659–671. doi:10.1016/S0010-938X(69)80097-110.1016/S0010-938X(69)80097-1 ↗
7. 7) Y. Shoji, S. Akiyama, M. Kisaichi, K. Nagatoshi and H. Hoshi: Effects of Cr and Si contents and rare earth metal additions on the high temperature oxidation resistance of high Si austenitic stainless steels, Tetsu-to-Hagané 63 (1977) 700–714. doi:10.2355/tetsutohagane1955.63.5_70010.2355/tetsutohagane1955.63.5_700 ↗
8. 8) D. Schaepers and H. Strehblow: Surface analytical investigations of electrochemically formed passive layers on binary Fe/Al alloys, J. Electrochem. Soc. 142 (1995) 2210–2218. doi:10.1149/1.204427710.1149/1.2044277 ↗
9. 9) D. Schaepers and H. Strehblow: An XPS and ISS investigation of passive layers on binary Fe-Al alloys, Corros. Sci. 39 (1997) 2193–2213. doi:10.1016/S0010-938X(97)00103-010.1016/S0010-938X(97)00103-0 ↗
10. 10) J. Peng, F. Moszner, J. Rechmann, D. Vogel, M. Palm and M. Rohwerder: Influence of Al content and pre-oxidation on the aqueous corrosion resistance of binary Fe-Al alloys in sulphuric acid, Corros. Sci. 149 (2019) 123–132. doi:10.1016/j.corsci.2018.12.04010.1016/j.corsci.2018.12.040 ↗
11. 11) O. Tajima, K. Nakao, M. Matsuda and H. Miyamae: Studies on the characteristics of Fe-Si alloys in potentiostatic polarization, J. Soc. Mater. Sci. Jpn. 17 (1968) 737–742. doi:10.2472/jsms.17.73710.2472/jsms.17.737 ↗
12. 12) H. Mitani and M. Onishi: Anodic behaviors of iron-silicon alloys fundamental studies on corrosion behaviors of iron-silicon alloys (part 1), J. Met. Finish. Soc. Jpn. 18 (1967) 225–229. doi:10.4139/sfj1950.18.22510.4139/sfj1950.18.225 ↗
13. 13) M. Onishi and H. Mitani: Anodic polarization behavior of iron-silicon alloys, Trans. Jpn. Inst. Met. 11 (1970) 62–67. doi:10.2320/matertrans1960.11.6210.2320/matertrans1960.11.62 ↗
14. 14) K. Hio, Y. Hosoi, M. Tsutsui and M. Okabe: Effects of Al and Si on the anodic polarization charaeteristics of Fe-10Cr alloys, J. Japan Inst. Metals 63 (1999) 1248–1254. doi:10.2320/jinstmet1952.63.10_124810.2320/jinstmet1952.63.10_1248 ↗
15. 15) K. Hio, T. Adachi, T. Yamada, Y. Tsuchida, K. Nakajima and Y. Hosoi: Effects of Al, Si and Mo on passivation characteristics of Fe-10Cr alloys, J. Japan Inst. Metals 64 (2000) 1148–1155. doi:10.2320/jinstmet1952.64.12_114810.2320/jinstmet1952.64.12_1148 ↗
16. 16) K. Hio, T. Yamada, Y. Tsuchida, K. Nakajima and Y. Hosoi: Effect of chromium content on anodic polarization characteristics of Fe-Cr-Al and Fe-Cr-Si alloys, Corrosion 58 (2002) 124–131. doi:10.5006/1.327731210.5006/1.3277312 ↗
17. 17) I.M. Wolff, L.E. Iorio, T. Rumpf, P.V.T. Scheers and J.H. Potgieter: Oxidation and corrosion behaviour of Fe–Cr and Fe–Cr–Al alloys with minor alloying additions, Mater. Sci. Eng. A 241 (1998) 264–276. doi:10.1016/S0921-5093(97)00500-510.1016/S0921-5093(97)00500-5 ↗
18. 18) A. Nagaoka, K. Nose, R. Matsuhashi, K. Matsuoka and H. Kajimura: The effect of chloride ion and dissolved oxygen concentration on passivation pH of SUS304 stainless steel, Zairyo-to-Kankyo (presently Corrosion Engineering) 69 (2020) 49–57. doi:10.3323/jcorr.69.4910.3323/jcorr.69.49 ↗
19. 19) JIS G 0579: Method of anodic polarization curves measurement for stainless steels, (JIS, 2007).
20. 20) JASO M 610-92: Cosmetic corrosion test method for automotive parts, (JASO, 1992).
21. 21) G. Okamoto: Passive film of 18-8 stainless steel structure and its function, Corros. Sci. 13 (1973) 471–489. doi:10.1016/0010-938X(73)90031-010.1016/0010-938X(73)90031-0 ↗
22. 22) O.E. Barcia, O.R. Mattos and B. Tribollet: Anodic dissolution of iron in acid sulfate under mass transport control, J. Electrochem. Soc. 139 (1992) 446–453. doi:10.1149/1.206923810.1149/1.2069238 ↗
23. 23) M. Bojinov, I. Betova, G. Fabricius, T. Laitinen and R. Raicheff: Passivation mechanism of iron in concentrated phosphoric acid, J. Electroanal. Chem. 475 (1999) 58–65. doi:10.1016/S0022-0728(99)00343-510.1016/S0022-0728(99)00343-5 ↗
24. 24) J.O’M. Bockris, M. Genshaw and V. Brusic: Mechanism of film growth and passivation of iron as indicated by transient ellipsometry, Symp. Faraday Soc. 4 (1970) 177–191. doi:10.1039/sf970040017710.1039/sf9700400177 ↗
25. 25) E.J. Kelly: The active iron electrode I. Iron dissolution and hydrogen evolution reactions in acidic sulfate solutions, J. Electrochem. Soc. 112 (1965) 124–131. doi:10.1149/1.242348010.1149/1.2423480 ↗
26. 26) R.M. Smith and A.E. Martell: Critical Stability Constants, (Plenum Press, New York, 1976) pp. 5–7.10.1007/978-1-4757-5506-0 ↗
27. 27) L.G. Sillèn and A.E. Martell: Stability Constants of Metal-ion Complexes, (The Chemical Society, London, 1964) pp. 48–280.
28. 28) R.T. Foley and T.H. Nguyen: The chemical nature of aluminum corrosion V. energy transfer in aluminum dissolution, J. Electrochem. Soc. 129 (1982) 464–467. doi:10.1149/1.212388110.1149/1.2123881 ↗
29. 29) D. Dobos: Electrochemical Data, (Elsevier, 1975) pp. 205–209.
30. 30) A. Fujimura, S. Shoji, Y. Kitagawa, Y. Hasegawa, T. Doi and K. Fushimi: Investigation of the dissolution/passivation mechanisms on Fe-Cr alloys in acidic Na2SO4 solution using online ICP-OES, Electrochim. Acta 463 (2023) 142843. doi:10.1016/j.electacta.2023.14284310.1016/j.electacta.2023.142843 ↗
31. 31) T.J. Swift and R.E. Connick: NMR-relaxation mechanisms of O17 in aqueous solutions of paramagnetic cations and the lifetime of water molecules in the first coordination sphere, J. Chem. Phys. 37 (1962) 307–320. doi:10.1063/1.170132110.1063/1.1701321 ↗
32. 32) D. Fiat and R.E. Connick: Oxygen-17 magnetic resonance studies of ion solvation. The hydration of aluminum (III) and gallium (III) ions, J. Am. Chem. Soc. 90 (1968) 608–615. doi:10.1021/ja01005a00910.1021/ja01005a009 ↗
33. 33) J.A. Jackson, J.F. Lemons and H. Taube: Nuclear magnetic resonance studies on hydration of cations, J. Chem. Phys. 32 (1960) 553–555. doi:10.1063/1.173073310.1063/1.1730733 ↗
34. 34) J.P. Hunt and R.A. Plane: The kinetics of the exchange of water between Cr(H2O)6+3 and solvent, J. Am. Chem. Soc. 76 (1954) 5960–5962. doi:10.1021/ja01652a01810.1021/ja01652a018 ↗
35. 35) R.A. Plane and J.P. Hunt: Photochemical exchange of water between Cr(H2O)6+3 and solvent, J. Am. Chem. Soc. 79 (1957) 3343–3346. doi:10.1021/ja01570a01010.1021/ja01570a010 ↗