Ultrathin zwitterionic polymeric interphases for stable lithium metal anodes
Source abstract
Abstract
Summary Lithium metal electrodeposits in the form of irregular morphological features, loosely termed dendrites, on planar anode substrates. The deposits may lead to rapid battery failure and safety concerns. Due to the highly reducing nature of Li (−3.04 V versus standard hydrogen electrode [SHE]), a solid electrolyte interphase (SEI) inevitably forms at the electrode/electrolyte interface, which regulates the subsequent electrodeposition of Li. Rational design of the chemical, mechanical, and ion transport properties of SEI plays an important role in determining the morphology of electrodeposited metals. We report on using initiated chemical vapor deposition (iCVD) to create ultrathin conformal zwitterionic polymeric interphases with precise thicknesses in the range of 10–500 nm. It was found that zwitterionic moieties are able to tune the solvation environment of the lithium cation at the electrode/electrolyte interface, enabling compact, planar deposition of the lithium metal. These findings provide new directions for designing ionic polymeric interphases for metal anodes.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Reviving the lithium metal anode for high-energy batteries10.1038/nnano.2017.16 ↗
2. Toward safe lithium metal anode in rechargeable batteries: a review10.1021/acs.chemrev.7b00115 ↗
3. Design principles for electrolytes and interfaces for stable lithium-metal batteries10.1038/nenergy.2016.114 ↗
4. Dendrite-free lithium deposition via self-healing electrostatic shield mechanism10.1021/ja312241y ↗
5. Lithium fluoride additives for stable cycling of lithium batteries at high current densities10.1002/aelm.201500246 ↗
6. Electrolyte additive enabled fast charging and stable cycling lithium metal batteries10.1038/nenergy.2017.12 ↗
7. Recent progress in understanding solid electrolyte interphase on lithium metal anodes10.1002/aenm.202003092 ↗
8. A review of solid electrolyte interphases on lithium metal anode10.1002/advs.201500213 ↗
9. Electroless formation of hybrid lithium anodes for fast interfacial ion transport10.1002/anie.201707754 ↗
10. Elastic and Li-Ion–Percolating hybrid membrane stabilizes Li metal plating10.1073/pnas.1809187115 ↗
11. Dendrite-free Li-metal battery enabled by a thin asymmetric solid electrolyte with engineered layers10.1021/jacs.7b10864 ↗
12. Universal chemomechanical design rules for solid-ion conductors to prevent dendrite formation in lithium metal batteries10.1038/s41563-020-0655-2 ↗
13. Suppression of lithium dendrite growth using cross-linked polyethylene/poly(ethylene oxide) electrolytes: a new approach for practical lithium-metal polymer batteries10.1021/ja502133j ↗
14. Achieving uniform lithium electrodeposition in cross-linked poly(ethylene oxide) networks: “soft” polymers prevent metal dendrite proliferation10.1021/acs.macromol.0c00475 ↗
15. High lithium transference number electrolytes via creation of 3-dimensional, charged, nanoporous networks from dense functionalized nanoparticle composites10.1021/cm303091j ↗
16. Designing solid-state electrolytes for safe, energy-dense batteries10.1038/s41578-019-0165-5 ↗
17. High rate and stable cycling of lithium metal anode10.1038/ncomms7362 ↗
18. A localized high-concentration electrolyte with optimized solvents and lithium difluoro(Oxalate)Borate additive for stable lithium metal batteries10.1021/acsenergylett.8b00935 ↗
19. Localized high-concentration sulfone electrolytes for high-efficiency lithium-metal batteries10.1016/j.chempr.2018.05.002 ↗
20. Nonpolar alkanes modify lithium-ion solvation for improved lithium deposition and stripping10.1002/aenm.201902116 ↗
21. The intrinsic behavior of lithium fluoride in solid electrolyte interphases on lithium10.1073/pnas.1911017116 ↗
22. Polymer–inorganic solid–electrolyte interphase for stable lithium metal batteries under lean electrolyte conditions10.1038/s41563-019-0305-8 ↗
23. Effects of polymer coatings on electrodeposited lithium metal10.1021/jacs.8b06047 ↗
24. Lithium metal anodes with an adaptive “solid-liquid” interfacial protective layer10.1021/jacs.6b13314 ↗
25. A dynamic, electrolyte-blocking, and single-ion-conductive network for stable lithium-metal anodes10.1016/j.joule.2019.07.025 ↗
26. Designing artificial solid-electrolyte interphases for single-ion and high-efficiency transport in batteries10.1016/j.joule.2017.06.002 ↗
27. Solid-state polymer electrolytes for high-performance lithium metal batteries
28. Designing polymeric interphases for stable lithium metal deposition10.1021/acs.nanolett.0c01501 ↗
29. Dendrite suppression by a polymer coating: a coarse-grained molecular study
30. Ultrathin conformal polycyclosiloxane films to improve silicon cycling stability10.1126/sciadv.aaw4856 ↗
31. Vapor-deposited biointerfaces and bacteria: an evolving conversation10.1021/acsbiomaterials.9b01496 ↗
32. Zwitterionic antifouling coatings for the purification of high-salinity shale gas produced water10.1021/acs.langmuir.5b02795 ↗
33. Molecular fouling resistance of zwitterionic and amphiphilic initiated chemically vapor-deposited (ICVD) thin films10.1080/09205063.2014.951245 ↗
34. Kinetics of all-dry free radical polymerization under nanoconfinement10.1021/acs.macromol.0c01534 ↗
35. A cation-tethered flowable polymeric interface for enabling stable deposition of metallic lithium10.1021/jacs.0c09649 ↗
36. The zwitterion effect in high-conductivity polyelectrolyte materials10.1038/nmat1044 ↗
37. Gleason · 2015 · 1
38. Investigating the electrochemical windows of ionic liquids10.1016/j.jiec.2012.07.011 ↗
39. Ultrathin antifouling coatings with stable surface zwitterionic functionality by initiated chemical vapor deposition (ICVD)10.1021/la302059s ↗
40. Surface-tethered zwitterionic ultrathin antifouling coatings on reverse osmosis membranes by initiated chemical vapor deposition10.1021/cm1031392 ↗
41. Synergistic prevention of biofouling in seawater desalination by zwitterionic surfaces and low-level chlorination10.1002/adma.201304386 ↗
42. Ultrathin zwitterionic coatings for roughness-independent underwater superoleophobicity and gravity-driven oil-water separation10.1002/admi.201400489 ↗
43. Nanoindentation of high-purity vapor deposited lithium films: the elastic modulus10.1557/jmr.2018.83 ↗
44. The electrochemical stability of ionic liquids and deep eutectic solvents10.1007/s11426-016-5566-3 ↗
45. Exploring electrochemical windows of room-temperature ionic liquids: a computational study10.1021/jp303915c ↗
46. Surface-based Li+ complex enables uniform lithium deposition for stable lithium metal anodes10.1021/acsaem.9b00929 ↗
47. Theory of chemical kinetics and charge transfer based on nonequilibrium thermodynamics10.1021/ar300145c ↗
48. Morphological stability during electrodeposition10.1557/mrc.2017.38 ↗
49. Strong texturing of lithium metal in batteries10.1073/pnas.1708224114 ↗
50. Insight into the critical role of exchange current density on electrodeposition behavior of lithium metal
51. Transient voltammetry with ultramicroelectrodes reveals the electron transfer kinetics of lithium metal anodes10.1021/acsenergylett.0c00031 ↗
52. Stabilizing electrodeposition in elastic solid electrolytes containing immobilized anions10.1126/sciadv.1600320 ↗
53. Morphological instability during steady electrodeposition at overlimiting currents10.1103/PhysRevE.92.052310 ↗
54. Nanoscale Nucleation and Growth of Electrodeposited Lithium Metal