journal article·2003-09

Determination of the Interlaminar Fracture Toughness of Glass-Fiber-Reinforced Plastics on Ring Segments

V. I. Solodilov, S. L. Bazhenov, Yu. A. Gorbatkina, A. M. Kuperman

Mechanics of Composite Materials· Volume 39· Issue 5
Publisher page

Abstract

A method is developed which allows one to estimate the fracture toughness GIc of fiber-reinforced plastics using ring segment specimens. It is shown that this method reduces to the so-called “angle method.” The approach developed was tested on segments of glass-fiber-reinforced plastic (GFRP) rings based on an EDT-10 epoxy matrix and RVMPN 10-1200-14 glass fibers. The crack was set by a polyimide film placed in the specimen midlayer at the winding stage. The ring thickness was 1 to 4.5 mm. The fracture toughness GIc was also calculated from force F-displacement D diagrams. It was found that the values of GIc determined by both methods agreed well. For δ ≥2 mm thick segments with long (L ≥30 mm) cracks, GIc was practically independent of L and δ, and, for the GFRP examined, it could be regarded as a material constant.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Mechanical Behavior of Composites · Material Properties and Failure Mechanisms · Ultrasonics and Acoustic Wave Propagation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. A. A. Griffith, “Theory of rupture,” in: Proc. 1st Int. Conf. Appl. Mech., Delft, Holland (1924), p. 55.
2. J. W. Obreimoff, “The splitting strength of mica,” Proc. Royal Soc. London, A127, 290–297 (1930).
3. A. I. Bailey, “The adhesion of mica crystals surfaces,” in: 2nd Int. Congr. Surf. Act. Vol. 3, (1957), pp. 406–417.
4. J. J. Gilman, “Direct measurements of the surface energies of crystals,” J. Appl. Phys., 31, 2208–2218 (1960).10.1063/1.1735524 ↗
5. A. J. Smiley and R. B. Pipes, “Rate effects on mode I interlaminar fracture toughness in composite materials,” J. Compos.Mater., 21, 670–687 (1987).10.1177/002199838702100706 ↗
6. W. P. Bascom, J. L. Bitner, R. J. Moulton, and A. R. Siebert, “The interlaminar fracture of organic matrix, woven reinforcement composites,” Composites, 11, 9–18 (1980).10.1016/0010-4361(80)90016-6 ↗
7. N. Sela and O. Ishai, “Interlaminar fracture toughness and toughening of laminated composite materials: a review,” Composites, 20, 423–435 (1989).10.1016/0010-4361(89)90211-5 ↗
8. P. G. Babaevskii and S. G. Kulik, Crack Resistance of Cured Polymer Compositions [in Russian], Khimiya, Moscow (1991).
9. J. G. Williams, “Large displacement and end block effects in the DCB interlaminar test in mode I and II,” J. Compos. Mater., 21, 330–338 (1987).10.1177/002199838702100403 ↗
10. S. L. Bazhenov, K. Selitty, A. Hiltner, and E. Baer, “Delamination mechanism in multilayer polycarbonate-styrene-acrylonitrile copolymer composites,” Vysokomol. Soed., 36A, 466–474 (1994).
11. S. Bazhenov, “Interlaminar and intralaminar fracture modes in 0°/90° cross-ply glass/epoxy laminate,” Composites, 26, 125–133 (1995).10.1016/0010-4361(95)90412-S ↗
12. H. T. Corten, “Mechanics of composite fracture,” in: Fracture. Vol. 7. Fracture of Nonmetals and Composites, Academic Press, New York–London (1972).
13. S. Hashemi, A. J. Kinloch, and J. G. Williams, “The effect of geometry, rate and temperature on the Mode I, Mode II and mixed-Mode I/II interlaminar fracture of carbon-fibre/poly(ether-ether ketone) composites,” J. Compos. Mater., 24, 918–956 (1990).10.1177/002199839002400902 ↗
14. B. F. Sorensen and T. K. Jacobsen, “Large-scale bridging in composites: R-curves and bridging laws,” Composites, 29A, Pt. A, 1443–1451 (1998).10.1016/S1359-835X(98)00025-6 ↗
15. T. K. Jacobsen and B. F. Sorensen, “Mode I intra-laminar crack growth in composites–modelling of R-curves from measured bridging laws,” Composites, 32, Pt. A, 1–11 (2001).10.1016/S1359-835X(00)00139-1 ↗