The use of polyolefins-based hot melts for wood bonding
Source abstract
Abstract
The shear strength of three-layer birch veneer/polyolefin/birch veneer lap joints has been investigated. It was found that the optimum technological parameters for producing three-layer laminated systems (plywood) at 180°C were a pressure time of 1-3 min (plus 3-min preheating) and pressure of 5-10 MPa. All the systems investigated exhibited relatively high values of shear strength, which were higher than those of the industrially produced plywood based on phenol-formaldehyde glues (3.5-5 MPa). It is shown that the use of interfacial modifiers can increase the shear strength by 50% compared with its initial values. The high shear resistance is explained by the high mechanical adhesion between the hot melts and the wood substrate. After a prolonged moisture influence (70 days at relative air humidity of 80%), all the systems investigated showed a considerable (up to 25%) increase in the shear strength. This can be explained by swelling of birch veneer, which gives rise to additional resistance forces between the hot melt and the substrate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Natural Fiber Reinforced Composites · Wood Treatment and Properties · Lignin and Wood Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. A. Knilock, Adhesion and Adhesive Science and Technology, Chapman and Hill, New York (1987).
2. F. Beand, P. Niemz, and A. Pizzi, “Structure properties relationships in one-component polyurethane adhesives for wood: sensitivity to low moisture content,” J. Appl. Polym. Sci., 101, 4181-4192 (2006).10.1002/app.24334 ↗
3. Young-Jun Park and Hyun-Joong Kim, “Hot melt adhesive properties of EVA-aromatic hydrocarbon resin blend,” Int. J. Adhes. Adhes., 23, No. 5, 383-392 (2003).10.1016/S0143-7496(03)00069-1 ↗
4. Pentti K. Jarvela, Outi Tervala, and Pirkko A. Jarvela, “Coating plywood with thermoplastic,” Int. J. Adhes. Adhes., 19, Iss. 4, No. 8, 295-301 (1999).
5. I. Aydin, “Activation of wood surfaces for glue bonds by mechanical pretreament and its effects on some properties of veneer surfaces and plywood panels,” Appl. Surface Sci., 233, Iss. 1-4, No. 6, 268-274 (2004).
6. M. J. Smith, H. Dai, and K. Ramani, “Wood-thermoplastic adhesive interface-method of characterization and results,” Int. J. Adhes. Adhes., 22, Iss. 3, 197-204 (2002).10.1016/S0143-7496(01)00055-0 ↗
7. Z. Mezey and T. Czigany, “Mechanical investigation of hemp fiber reinforced polypropylene with different types of MAPP compatibilizer,” Mater. Sci. Forum, 537-538, 223-229 (2007).10.4028/www.scientific.net/MSF.537-538.223 ↗
8. Burhanettin, “Usual bonding strength and dimensional stability of laminated veneer lumbers manufactured by using different adhesives after the steam test,” Int. J. Adhes. Adhes., 25, 395-403 (2005).10.1016/j.ijadhadh.2004.11.005 ↗
9. Syed H. Imam, Gordon Sherald H., Liju Mao, and Liang Chen, “Environmentally friendly wood adhesive from renewable plant polymer: characteristics and optimization,” Polym. Degrad. Stab., 73, 529-533 (2001).10.1016/S0141-3910(01)00114-8 ↗