Correlation of nanoscale interface debonding and multimode fracture in polymer carbon composites with long-term hygrothermal effects
Source abstract
Abstract
Abstract The correlation between nanoscale interface debonding and crack energy release rate for modes I, II, and I/II for extended exposure to hygrothermal conditions in polymer matrix composites (PMCs) needs to be understood. In this study, the effects on PMCs for two years of exposure, to a heat of 60 °C and relative humidity of 90%, were investigated. The interphase properties were studied using PF QNM. During hygrothermal treatment, the interphase region's thickness around the crack tip increases, and the morphology of the interphase changes. Nanoscale debonding of the fiber and matrix in artificially aged samples is a mix of cohesive and adhesive failure. Degradation at the nanoscale interphase and the macroscale crack initiation toughness slows after one year of aging. Interface debonding and nanoscale cracks cause intralaminar cracks, fiber bridging, and an increase in crack energy. Toughness in mode I fracture was increased in the artificially aged samples.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Mechanical Behavior of Composites · Polymer crystallization and properties · Smart Materials for Construction
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Effect of hydrothermal ageing on the thermal and delamination fracture CFRP composites
2. Damage characterization in composite materials using acoustic emission signal-based and parameter-based data10.1016/j.compositesb.2019.107469 ↗
3. Comparative effects of humid tropical weathering and artificial ageing on a model composite properties from nano- to macro-scale
4. Interfacial microstructure and mechanical properties of carbon fiber composite modified with carbon dots10.1016/j.compscitech.2019.107856 ↗
5. Probing elastic properties of soft materials with AFM: data analysis for different tip geometries10.1016/j.polymer.2016.02.020 ↗
6. Study of the relationship between the crystal structure and micro-nano morphology of anodized stainless steels10.1016/j.elecom.2019.02.021 ↗
7. Non-smooth mode I fracture of fibre-reinforced composites: an experimental, numerical and analytical study10.1098/rsta.2011.0381 ↗
8. Application of the effective crack method to mode I and mode II interlaminar fracture of carbon/epoxy unidirectional laminates10.1016/j.compositesa.2006.09.001 ↗
9. Effect of contact deformations on the adhesion of particles10.1016/0021-9797(75)90018-1 ↗
10. Comparison of nanoindentation and AFM methods for the determination of mechanical properties of polymers10.1016/j.polymertesting.2013.01.011 ↗
11. Characterization of the interphase in carbon fiber/polymer composites using a nanoscale dynamic mechanical imaging technique10.1016/j.carbon.2010.05.008 ↗
12. Structuring the thermoplastic interleaf with lotus-leaf-like structure and its interlaminar toughening for CFRPs10.1016/j.compscitech.2019.107825 ↗
13. Analysis of properties of fiber composites with anisotropic constituents10.1115/1.3424603 ↗
14. Nano-indentation and nano-scratch of polymer/glass interfaces. II: model of interphases in water aged composite materials10.1016/S0032-3861(01)00029-5 ↗
15. Effect of hygrothermal ageing on tribological behaviour of PTFE-based composites
16. A review of interphase formation and design in fibre-reinforced composites10.1163/016942409X12579497420609 ↗
17. Rate dependence of mode I fracture behavior in carbon fiber epoxy composite laminates10.1016/S0266-3538(97)00176-0 ↗
18. Novel carbon-fibre powder-epoxy composites: interface phenomena and interlaminar fracture behaviour10.1016/j.compositesb.2019.107012 ↗
19. The effects of manufacturing-induced and in-service related bonding quality reduction on the mode-I fracture toughness of composite bonded joints for aeronautical use10.1016/j.compositesb.2012.05.052 ↗
20. Characterization of the interlaminar fracture toughness of a laminated carbon/epoxy composite10.1016/j.compscitech.2006.07.035 ↗
21. Effect of prepreg storage humidity on the mixed-mode fracture toughness of a co-cured composite joint10.1016/j.compositesa.2012.09.010 ↗
22. Mode I fracture toughness of co-cured and secondary bonded composite joints10.1016/j.ijadhadh.2014.02.008 ↗
23. Interphase formation and fiber matrix adhesion in carbon fiber reinforced epoxy resin: influence of carbon fiber surface chemistry10.1080/09276440.2017.1267513 ↗
24. Novel three-dimensional interphase characterisation of polymer nanocomposites using nanoscaled topography10.1088/1361-6528/aacd5d ↗
25. Mechanical mapping of the interphase in carbon fiber reinforced poly(ether-ether-ketone) composites using peak force atomic force microscopy: interphase shrinkage under coupled ultraviolet and hydro-thermal exposure10.1016/j.polymertesting.2016.09.008 ↗
26. Investigation of the interphase structures and properties of carbon fiber reinforced polymer composites exposed to hydrothermal treatments using peak force quantitative nanomechanics technique10.1002/pc.24245 ↗
27. O'Brien · 1983 · 192
28. Olsen · 2007 · 5
29. Pittenger
30. CNT/polymer interface in polymeric composites and its sensitivity study at different environments10.1016/j.cis.2016.12.008 ↗
31. Water-induced degradations in MWCNT embedded glass fiber/epoxy composites: an emphasis on aging temperature10.1002/app.45987 ↗
32. Mechanical performance of CNT-filled glass fiber/epoxy composite in in-situ elevated temperature environments emphasizing the role of CNT content10.1016/j.compositesa.2016.02.020 ↗
33. Spring constant calibration of atomic force microscope cantilevers of arbitrary shape10.1063/1.4757398 ↗
34. Study on the performance of different nano-species used for surface modification of carbon fiber for interface strengthening10.1016/j.compositesa.2019.105509 ↗
35. Novel method for improving fatigue behavior of carbon fiber reinforced epoxy composite10.1016/j.compositesb.2018.08.062 ↗
36. Investigation of reactive polymer-polymer interface using nanomechanical mapping10.1021/ma100799s ↗
37. Visualization and quantification of the chemical and physical properties at a diffusion-induced interface using AFM nanomechanical mapping10.1021/ma500099b ↗
38. The use of the PeakForceTM quantitative nanomechanical mapping AFM-based method for high-resolution Young's modulus measurement of polymers10.1088/0957-0233/22/12/125703 ↗
39. Effect of elevated operating temperature on the dynamic mechanical performance of E-glass/epoxy composite10.1016/j.compositesb.2019.106937 ↗
40. Investigation of the long term effects of moisture on carbon fibre and epoxy matrix composites10.1016/j.compscitech.2012.01.010 ↗
41. Following the morphological and thermal properties of PLA/PEO blends containing carbon nanotubes (CNTs) during hydrolytic degradation10.1016/j.compositesb.2019.107132 ↗