Abstract

The joining of lead-free Sn-3.0Ag-0.5Cu (SAC305) solder alloy to metal substrate with the addition of a porous Cu interlayer was investigated. Two types of porous Cu interlayers, namely 15 ppi—pore per inch (P15) and 25 ppi (P25) were sandwiched in between SAC305/Cu substrate. The soldering process was carried out at soldering time of 60, 180, and 300 s at three temperature levels of 267, 287, and 307 °C. The joint strength was evaluated by tensile testing. The highest strength for solder joints with addition of P25 and P15 porous Cu was 51 MPa (at 180 s and 307 °C) and 54 MPa (at 300 s and 307 °C ), respectively. The fractography of the solder joint was analyzed by optical microscope (OM) and scanning electron microscopy (SEM). The results showed that the propagation of fracture during tensile tests for solder with a porous Cu interlayer occurred in three regions: (i) SAC305/Cu interface; (ii) inside SAC305 solder alloy; and (iii) inside porous Cu. Energy dispersive X-ray spectroscopy (EDX) was used to identify intermetallic phases. Cu6Sn5 phase with scallop-liked morphology was observed at the interface of the SAC305/Cu substrate. In contrast, the scallop-liked intermetallic phase together with more uniform but a less defined scallop-liked phase was observed at the interface of porous Cu and solder alloy.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Centre of Advanced Manufacturing and Material Processing (AMMP), Department of Mechanical Engineering, University of Malaya, Kuala Lumpur 50603, Malaysia

Department of Metallurgical Engineering, Tokai University, Hiratsuka 259-1292, Japan

Department of Mechanical Engineering, Nagaoka University of Technology, Nagaoka 940-2188, Japan

References (36)

Show source-provided references
1. The Current Status of Lead-Free Soldering
2. High-temperature lead-free solder alternatives10.1016/j.mee.2010.12.072 ↗
3. High-Reliability Low-Ag-Content Sn-Ag-Cu Solder Joints for Electronics Applications10.1007/s11664-012-2145-z ↗
4. Microstructural stability of Sn-1Ag-0.5Cu-xAl (x = 1, 1.5, and 2 wt. %) solder alloys and the effects of high-temperature aging on their mechanical properties10.1016/j.matchar.2013.01.015 ↗
5. Solid state interaction between a Sn-Ag-Cu-In solder alloy and Cu substrate10.1016/j.intermet.2012.12.020 ↗
6. Nanoparticles of the Lead-free Solder Alloy Sn-3.0Ag-0.5Cu with Large Melting Temperature Depression10.1007/s11664-008-0591-4 ↗
7. High Temperature Lead-Free Solder for Microelectronics10.1007/s11837-001-0097-5 ↗
8. Interaction behavior between the additives and Sn in Sn-3.0Ag-0.5Cu-based solder alloys and the relevant joint solderability10.1016/j.jallcom.2008.05.017 ↗
9. High-Temperature Lead-Free Solders: Properties and Possibilities10.1007/s11837-009-0013-y ↗
10. Effects of Fe2NiO4 nanoparticles addition into lead free Sn-3.0Ag-0.5Cu solder pastes on microstructure and mechanical properties after reflow soldering process10.1016/j.matdes.2014.11.025 ↗
11. Microstructure and mechanical properties of Pb-free Sn-3.0Ag-0.5Cu solder pastes added with NiO nanoparticles after reflow soldering process10.1016/j.matdes.2015.10.142 ↗
12. Liu, W., Lee, N.-C., and Bachorik, P. (2013). An innovative composite solder preform for TLP bonding—Microstructure and properties of die attach joints. Electron. Packag. Technol. Conf. EPTC 2013.10.1109/EPTC.2013.6745797 ↗
13. Effects of addition of copper particles of different size to Sn-3.5Ag solder10.1007/s10854-011-0441-7 ↗
14. Degischer, H.P., and Kriszt, B. (2002). Handbook of Cellular Metals: Production, Processing, Applications, Wiley-VCH.10.1002/3527600558 ↗
15. Experimental study of air natural convection on metallic foam-sintered plate10.1016/j.ijheatfluidflow.2012.08.005 ↗
16. Heat transfer performance of lotus-type porous copper heat sink with liquid GaInSn coolant10.1016/j.ijheatmasstransfer.2014.09.058 ↗
17. Bonding of silicon nitride ceramics using Fe-Ni/Cu/Ni/Cu/Fe-Ni interlayers10.1016/S0167-577X(00)00232-9 ↗
18. Vacuum brazing of sapphire with Inconel 600 using Cu/Ni porous composite interlayer for gas pressure sensor application10.1016/j.matdes.2013.08.046 ↗
19. Formation behaviour of reaction layer in Sn-3.0Ag-0.5Cu solder joint with addition of porous Cu interlayer10.1088/1757-899X/61/1/012020 ↗
20. An experimental study on the heat dissipation of LED lighting module using metal/carbon foam10.1016/j.icheatmasstransfer.2013.08.022 ↗
21. Creep-Fatigue Crack Growth Behavior of Pb-Containing and Pb-Free Solders at Room and Elevated Temperatures10.1007/s11664-012-2061-2 ↗
22. Thermal conductivity of porous copper manufactured by the lost carbonate sintering process10.1002/pssa.200723121 ↗
23. Nawaz, K., Bock, J., and Jacobi, A.M. Thermal-Hydraulic Performance of Metal Foam Heat Exchangers. Available online: http://docs.lib.purdue.edu/iracc/1283.
24. Afendi, M., wan Nordin, W.N., Daud, R., and Tokuo, T. (2012, January 27–28). Strength and Fracture Characteristics of Shear Adhesive Dissimilar Joint. Proceedings of the International Conference On Applications and Design in Mechnaical Engineering 2012, Penang, Malaysia.
25. Effects of fourth alloying additive on microstructures and tensile properties of Sn-Ag-Cu alloy and joints with Cu10.1016/S0026-2714(02)00239-1 ↗
26. Joining ceramics to metals using metallic foam10.1016/j.msea.2008.06.007 ↗
27. Effect of Zn addition in Sn-rich alloys on interfacial reaction with Au foils10.1016/S1003-6326(08)60107-7 ↗
28. Microstructural evolution and tensile properties of Sn-5Sb solder alloy containing small amount of Ag and Cu10.1016/j.jallcom.2011.01.109 ↗
29. Development of high strength Sn-0.7Cu solders with the addition of small amount of Ag and In10.1016/j.jallcom.2011.05.119 ↗
30. Lee, C.C., Wang, P.J., and Kim, J.S. (2007). Are intermetallics in solder joints really brittle?. Proc. Electron. Compon. Technol. Conf.10.1109/ECTC.2007.373866 ↗
31. Phase diagrams for lead-free solder alloys10.1007/BF02709189 ↗
32. Effect of iron and indium on IMC formation and mechanical properties of lead-free solder10.1016/j.msea.2012.05.086 ↗
33. Cu6Sn5 precipitation during Sn-based solder/Cu joint solidification and its effects on the growth of interfacial intermetallic compounds10.1016/j.jallcom.2013.08.013 ↗
34. Thermal cycling reliability of lead-free solders (SAC305 and Sn3.5Ag) for high-temperature applications10.1109/TDMR.2011.2134100 ↗
35. Influence of nanoparticle addition on the formation and growth of intermetallic compounds (IMCs) in Cu/Sn-Ag-Cu/Cu solder joint during different thermal conditions10.1088/1468-6996/16/3/033505 ↗
36. Properties of lead-free solder alloys with rare earth element additions10.1016/j.mser.2004.01.001 ↗