Abstract
9CrMoW steel tubes were welded in multiple passes by gas-tungsten arc welding. The reheated microstructures in the Gr. 92 weld metal (WM) of a multiple-pass weld were simulated with an infrared heating system. Simulated specimens after tempering at 760 °C/2 h were subjected to constant load creep tests either at 630 °C/120 MPa or 660 °C/80 MPa. The simulated specimens were designated as the over-tempered (OT, below AC1, i.e., WT-820T) and partially transformed (PT, below AC3, i.e., WT-890T) samples. The transmission electron microscope (TEM) micrographs demonstrated that the tempered WM (WT) displayed coarse martensite packets with carbides along the lath and grain boundaries. Cellular subgrains and coarse carbides were observed in the WT-820T sample. A degraded lath morphology and numerous carbides in various dimensions were found in the WT-890T sample. The grain boundary map showed that the WT-820T sample had the same coarse-grained structure as the WT sample, but the WT-890T sample consisted of refined grains. The WT-890T samples with a fine-grained structure were more prone to creep fracture than the WT and WT-820T samples were. Intergranular cracking was more likely to occur at the corners of the crept samples, which suffered from high strain and stress concentration. As compared to the Gr. 91 steel or Gr. 91 WM, the Gr. 92 WM was more stable in maintaining its original microstructures under the same creep condition. Undegraded microstructures of the Gr. 92 WM strained at elevated temperatures were responsible for its higher resistance to creep failure during the practical service.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Optoelectronics and Materials Technology, National Taiwan Ocean University, Keelung 20224, Taiwan
Nuclear Fuels and Materials Division, Institute of Nuclear Energy Research, Taoyuan 32546, Taiwan
Department of Materials Science and Engineering, National Taiwan University, Taipei 10617, Taiwan
Center of Excellence for Ocean Engineering, National Taiwan Ocean University, Keelung 20224, Taiwan
Funding
Ministry of Science and Technology
References (22)
Show source-provided references
1. Program on Materials Technology for Ultra-Supercritical Coal Power Plants
2. Enhanced mechanical properties induced by refined heat treatment for 9Cr–0.5Mo–1.8W martensitic heat resistant steel10.1016/j.matdes.2013.01.072 ↗
3. Analysis of the microstructure near the crack tip of ASME Gr.92 steel after creep crack growth10.1016/j.matchar.2010.07.003 ↗
4. Phase evolution in P92 and E911 weld metals during ageing10.1016/j.msea.2007.07.036 ↗
5. Review of type IV cracking of weldments in 9–12%Cr creep strength enhanced ferritic steels10.1179/1743280412Y.0000000016 ↗
6. Formation Mechanism of Type IV Failure in High Cr Ferritic Heat-Resistant Steel-Welded Joint10.1007/s11661-013-1801-0 ↗
7. The Influence of Thermal Cycles on the Microstructure of Grade 92 Steel10.1007/s11661-017-4306-4 ↗
8. Microstructural Characterization of the Heat-Affected Zones in Grade 92 Steel Welds: Double-Pass and Multipass Welds10.1007/s11661-017-4446-6 ↗
9. Microstructure evolution in HAZ and suppression of Type IV fracture in advanced ferritic power plant steels10.1016/j.ijpvp.2010.08.005 ↗
10. Metallurgy of Type IV fracture in advanced ferritic power plant steels10.3184/096034011X13056166748234 ↗
11. Role of Boundary Strengthening on Prevention of Type IV Failure in High Cr Ferritic Heat-Resistant Steels10.1007/s11661-013-2072-5 ↗
12. Effect of microstructural evolution on high-temperature strength of 9Cr–3W–3Co martensitic heat resistant steel under different aging conditions10.1016/j.msea.2013.09.033 ↗
13. Suppression of grain refinement in heat-affected zone of 9Cr–3W–3Co–VNb steels10.1016/j.msea.2015.12.095 ↗
14. Microstructure and type IV cracking behavior of HAZ in P92 steel weldment10.1016/j.msea.2012.05.076 ↗
15. Experimental investigation of specimen size effect on creep crack growth behavior in P92 steel welded joint10.1016/j.matdes.2013.12.062 ↗
16. Alternative PWHT to Improve High-Temperature Mechanical Properties of Advanced 9Cr Steel Welds10.1007/s11665-018-3736-5 ↗
17. Microstructural characterization of weld joints of 9Cr reduced activation ferritic martensitic steel fabricated by different joining methods10.1016/j.matchar.2014.08.013 ↗
18. Peng, Y.Q., Chen, T.C., Chung, T.J., Jeng, S.L., Huang, R.T., and Tsay, L.W. (2017). Creep Rupture of the Simulated HAZ of T92 Steel Compared to that of a T91 Steel. Materials, 10.10.3390/ma10020139 ↗
19. Wu, T.J., Liao, C.C., Chen, T.C., Shiue, R.K., and Tsay, L.W. (2019). Microstructural Evolution and Short-Term Creep Rupture of the Simulated HAZ in T92 Steel Normalized at Different Temperatures. Metals, 9.10.3390/met9121310 ↗
20. Effects of simulated microstructure on the creep rupture of the modified 9Cr-1Mo steel10.1007/s11665-016-2270-6 ↗
21. Wu, H.W., Wu, T.J., Shiue, R.K., and Tsay, L.W. (2018). The Effect of Normalizing Temperature on the Short-Term Creep Rupture of the Simulated HAZ in Gr. 91 Steel Welds. Metals, 8.10.3390/met8121072 ↗
22. Liao, C.C., Wang, C.C., Chen, T.C., Shiue, R.K., and Tsay, L.W. (2020). Effects of Thermal Simulation on the Creep Fracture of the Mod. 91 Weld Metal. Metals, 10.10.3390/met10091181 ↗