journal article·2021-04-21Open access

Effect of Cooling Rate on Hardness and Phase Transformation of a Pd-Ag-Based Metal–Ceramic Alloy with or without Ice-Quenching

Hye-Jeong Shin, Yong-Hoon Kwon, Hyo-Joung Seol

Metals· Volume 11· Issue 5

Abstract

The aim of this study was to investigate the effect of cooling rate on the hardness and phase transformation of a Pd-Ag-based metal–ceramic alloy with or without ice-quenching. A total of 28 test specimens, in an as-cast state, were fabricated. A multiple firing simulation was performed on the randomly selected specimens (n = 3/group) in a porcelain furnace; each firing was followed by cooling at the relatively low or high cooling rate. In addition, ice-quenching after oxidation was introduced before the normal firing process (n = 3/group). Microhardness, microstructure, phase transformation and elemental distribution were observed. Oxidation followed by ice-quenching allowed the alloy to be in a homogenized state. On the other hand, the oxidation-treated specimens followed by cooling at relatively high or low cooling speeds showed much higher hardness than the ice-quenched specimen after oxidation, which was resulted from the formation of the metastable precipitates based on the InPd3 phase with tetragonal structure. The hardness of ice-quenched alloy after oxidation was recovered in the very next firing step at both the relatively high and low cooling rates. In all specimens, the Pd-rich matrix and the InPd3-based precipitates were observed. The hardness of a Pd-Ag-based metal–ceramic alloy with and without ice-quenching depended on the cooling rate during the firing process.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Metallic Glasses and Amorphous Alloys · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Dental Materials, Dental and Life Science Institute, School of Dentistry, Pusan National University, Beomeo-Ri, Mulgeum-Eup, Yangsan 626-814, Korea

Funding

National Research Foundation of Korea

References (25)

Show source-provided references
1. Fracture reasons in ceramic-fused-to-metal restorations10.1046/j.1365-2842.2003.01038.x ↗
2. Metallurgical aspects of palladium-silver porcelain-bonding alloys10.1016/0300-5712(89)90140-1 ↗
3. The effect of repeated porcelain firings on corrosion resistance of different dental alloys10.4047/jap.2013.5.1.44 ↗
4. Effect of pretreatments on the metal-ceramic bonding strength of a Pd-Ag alloy10.1016/j.jdent.2013.11.020 ↗
5. Potentiodynamic polarization study of the corrosion behavior of palladium-silver dental alloys10.1016/j.prosdent.2017.06.026 ↗
6. New high-palladium casting alloys: Part 2. Effects of heat treatment and burnout temperature
7. Study of Pd-Ag dental alloys: Examination of effect of casting porosity on fatigue behavior and microstructural analysis10.1007/s10856-010-4116-3 ↗
8. Effect of ice-quenching on the change in hardness of a Pd-Au-Zn alloy during porcelain firing simulation10.4012/dmj.2016-279 ↗
9. Effect of ice quenching after oxidation with or without vacuum on the hardness of Pd-Ag–Au–In alloy during porcelain firing simulation10.1016/j.jmbbm.2019.03.006 ↗
10. Effect of cooling rate on hardness and microstructure of Pd-Ag–In–Sn–Ga alloy during porcelain firing simulation10.1016/j.jmbbm.2020.103728 ↗
11. Comparative study of two precision overdenture attachment designs10.1016/S0022-3913(96)90298-X ↗
12. Recommendations for analysis of repeated-measures designs: Testing and correcting for sphericity and use of manova and mixed model analysis10.1111/opo.12399 ↗
13. Effect of ice-quenching after Oxidation treatment on hardening of a Pd-Cu-Ga-Zn alloy for bonding porcelain10.1016/j.jmbbm.2017.12.014 ↗
14. Porter, D.A., Easterling, K.E., and Sherif, M.Y. (2009). Phase Transformations in Metals and Alloys, CRC Press/Taylor and Francis Group. [3rd ed.]. Chapter 5.5.1.
15. Early stage of ordering in stoichiometric AuCu alloy10.2320/matertrans1989.39.87 ↗
16. Age-hardening behavior in a palladium-base dental porcelain-fused alloy10.1016/1044-5803(90)90008-8 ↗
17. Age-hardening associated with precipitation reaction and spinodal decomposition in a commercial dental low-carat Au-Ag-Cu-Pd alloy10.1023/A:1018572614570 ↗
18. Age-hardening reactions in a type III dental gold alloy10.1016/S0142-9612(00)00301-X ↗
19. Transmission electron microscopic investigate on of a Pd-Ag-In-Sn dental alloy10.1016/S0142-9612(02)00564-1 ↗
20. Isothermal age-hardening behaviour in commercial dental gold alloys containing palladium10.4012/dmj.3.253 ↗
21. Annealing study of palladium-silver dental alloys: Vickers hardness measurements and SEM microstructural observations10.1007/s10856-006-0668-7 ↗
22. Stress-relieving and porcelain firing cycle influence on marginal fit of commercially pure titanium and titanium–aluminum–vanadium copings10.1016/S0109-5641(03)00014-9 ↗
23. Mitra, F., Rashin, G., and Amin, A.R. (2018). The effect of multiple firings on the shear bond strength of porcelain to a new millable alloy and a conventional casting alloy. Materials, 11.10.3390/ma11040478 ↗
24. Massalski, T.B. (1990). Binary Alloy Phase Diagrams, ASM International. [2nd ed.].
25. Three distinguishable phase changes during slow cooling in commercial dental alloys for porcelain bonding10.4012/dmj.6.54 ↗