The Effect of Low-Temperature Annealing and Long-Term Operation of Nuclear Power Plant Components on the Corrosion Resistance of 08CH18N10T Steel
Source abstract
Abstract
Extending the service life of nuclear power plant components beyond their originally designed operational period requires a detailed understanding of the microstructural stability of the materials used. This study focuses on low-temperature precipitation in the austenitic stainless steel 08CH18N10T, which is employed in the main circulation piping of pressurized water reactors. During long-term operation in the temperature range of 100–320 °C, secondary phases such as M23C6 carbides and intermetallic phase sigma (σ) can precipitate, which can lead to local chromium depletion at grain boundaries, subsequent sensitization of the steel, and susceptibility to intergranular corrosion. The research includes the analysis of samples taken from the decommissioned V1 unit of the Jaslovské Bohunice Nuclear Power Plant, which has been in operation for 28 years. The samples were subjected to thermal aging under laboratory conditions, with an emphasis on evaluating microstructural changes and their impact on corrosion resistance. Based on the experimental results, it can be concluded that the thermal stability of all tested materials is suitable for the operation of the main circulation piping, as the service temperatures to which the main circulation piping is exposed during operation remain below the activation of precipitation that would lead to sensitization and, consequently, susceptibility to intergranular corrosion. Activation of low-temperature precipitation was observed only at 450 °C, while at temperatures up to 400 °C, the structural stability of the material was confirmed, demonstrating its suitability for operation within the specified temperature range of the nuclear power plants’ main circulation piping.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Faculty of Materials Science and Technology in Trnava, Slovak University of Technology in Bratislava, 811 07 Bratislava, Slovakia
Funding
international Horizon-Euratom project “Lifetime Extension and Its Impact on Safety and Perfor-mance of Structural Materials—Long-Term Operation without Safety Compromises · Slovak Research and Development Agency
References (42)
Show source-provided references
1. JAVYS (2026, March 01). Jadrové Zariadenia—História. Available online: https://www.javys.sk/sk/jadrove-zariadenia/jadrova-elektraren-v1/historia.
2. Critical analysis of the primary circuit components important to LTO’s safe operation of NPP VVER-440 and VVER-100010.1063/5.0235147 ↗
3. Jirková, H., Janda, T., Růžička, J., Mach, J., and Volkmannová, J. (2020). Effect of holding time at stabilization annealing on properties of 08CH18N10T austenitic stainless steel. Proceedings of the 29th International Conference on Metallurgy and Materials, Tanger Ltd.10.37904/metal.2020.3498 ↗
4. A review of stress corrosion cracking of austenitic stainless steels in PWR primary water10.1016/j.jnucmat.2023.154815 ↗
5. VVER long-term operation—A review based on the material studies results from past and ongoing EU-supported research projects10.1016/j.nucengdes.2025.113949 ↗
6. Effect of aging on the low cycle fatigue performance of a low alloy steel10.1016/j.prostr.2023.12.002 ↗
7. Low cycle thermomechanical fatigue of VVER-440 reactor pressure vessel steels: Investigation of fatigue kinetics and development of a life assessment model10.1016/j.prostr.2016.06.271 ↗
8. Effects of cold-working and annealing at 700 °C on hardness of 08Ch18N10T steel10.1016/j.prostr.2020.01.124 ↗
9. Fatigue tests of austenitic stainless steel AISI 321 and the weld metal ER308L in air and high-temperature water environment10.1016/j.prostr.2025.11.066 ↗
10. Precipitation behavior of the M23C6 phase on the coherent twin boundary of 25Cr-20Ni-Nb-N steel10.1016/j.matlet.2024.136277 ↗
11. Microstructural investigation and identification of intermetallic σ phase in solution annealed 316L type austenitic stainless steel10.1016/j.matchar.2021.111524 ↗
12. Investigation of the corrosion behavior of bulk nanocrystalline 316L austenitic stainless steel in NaCl solution10.1049/mnl.2012.0162 ↗
13. Correlation between grain boundary strength determined by impact test of miniature specimens and stress corrosion cracking resistance of irradiated austenitic steels used for internals of WWER type and PWR type nuclear reactors10.1016/j.engfailanal.2021.105544 ↗
14. Influence of final turning on SCC susceptibility and corrosion properties of austenitic stainless steel 08Ch18N10T10.1088/1742-6596/2931/1/012014 ↗
15. Understanding the effect of decreasing C content and increasing solid solution time on intergranular corrosion resistance of 304 austenitic stainless steel10.1016/j.jmrt.2024.04.132 ↗
16. Susceptibility to intergranular corrosion in sensitized austenitic stainless steel characterized via crystallographic characteristics of grain boundaries10.1016/j.corsci.2021.109946 ↗
17. Intergranular corrosion in sensitized austenitic stainless steel subjected to tensile loading and unloading in the elastic plastic region10.1016/j.corsci.2024.111896 ↗
18. Effect of grain size and grain boundary type on intergranular stress corrosion cracking of austenitic stainless steel: A phase field study10.1016/j.corsci.2024.112557 ↗
19. A new method for predicting susceptibility of austenitic stainless steels to intergranular stress corrosion cracking10.1016/j.matdes.2019.108368 ↗
20. Microstructures and intergranular corrosion resistance of hot rolled austenitic stainless steel-clad plates10.1016/j.jmrt.2023.07.192 ↗
21. New insights into the intergranular corrosion resistance mechanism of type 304 austenitic stainless steel by adjusting carbon content10.1016/j.jmrt.2023.07.220 ↗
22. Mechanical criterion for nucleation of intergranular stress corrosion cracking in austenitic stainless steel10.1016/j.finmec.2021.100013 ↗
23. Raman spectroscopy study on intergranular corrosion sensitivity of 304 austenitic stainless steel10.1016/j.corcom.2024.03.004 ↗
24. The importance of steel chemistry and thermal history on the sensitization behavior in austenitic stainless steels: Experimental and modeling assessment10.1016/j.mtcomm.2020.101088 ↗
25. Corrosion behavior of metastable AISI 321 austenitic stainless steel: Effect of grain size and prior plastic deformation on degradation in saline media10.1038/s41598-019-48594-3 ↗
26. Carbide forming special features and fracture mechanisms under the austenitic chromium-nickel 304 steel post-life ageing
27. (2021). Standard Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels (Standard No. ASTM A262). Annual Book of ASTM Standards.
28. (2010). Corrosion of Metals and Alloys–Electrochemical Potentiokinetic Reactivation Measurement Using the Double Loop Method (DL-EPR) (Standard No. BS EN ISO 12732).
29. On the development of the electrochemical potentiokinetic method10.1016/S0013-4686(01)00674-0 ↗
30. Číhal, V. (1984). Intergranular Corrosion of Steels and Alloys, Elsevier. Materials Science Monographs 18.
31. Double Loop Electrochemical Potentiokinetic Reactivation Test optimization for assessing duplex stainless steel intergranular corrosion susceptibility10.1007/s11661-004-0187-4 ↗
32. Application of Double Loop Electrochemical Potentio kinetic Reactivation for characterizing the intergranular corrosion susceptibility of stainless steels and Ni based alloys in solar nitrate salts used in CSP systems10.1016/j.engfailanal.2021.105717 ↗
33. Microstructure degradation of austenitic stainless steels after 45 years of operation as VVER 440 reactor internals10.1016/j.jnucmat.2020.152124 ↗
34. Effect of carbon content on the low temperature sensitization of 304L stainless steel and its corrosion resistance in simulated groundwater10.1016/j.matchemphys.2019.01.019 ↗
35. Janda, T., Jenicek, S., Kucerova, L., Letak, R., Jandova, D., and Jirkova, H. (2023). Influence of higher stabilization temperatures on the microstructure and mechanical properties of austenitic stainless steel 08Ch18N10T. Metals, 13.10.3390/met13050975 ↗
36. Liu, G., Liu, Y., Cheng, Y., Li, J., and Jiang, Y. (2019). Intergranular corrosion susceptibility of metastable austenitic Cr–Mn–Ni–N–Cu high strength stainless steel under various heat treatments. Materials, 12.10.3390/ma12091385 ↗
37. Fang, K., Luo, K., and Wang, L. (2022). Effect of microstructure on mechanical properties of 316LN austenitic stainless steel. Coatings, 12.10.3390/coatings12101461 ↗
38. Dong, Y., Zhang, Z., Yang, Z., Zheng, R., and Chen, X. (2022). Effect of annealing temperature on the microstructure and mechanical properties of high-pressure torsion produced 316LN stainless steel. Materials, 15.10.3390/ma15010181 ↗
39. Corrosion behaviors of random and special grain boundaries in sensitized 304 stainless steels10.1016/S1006-706X(08)60107-7 ↗
40. Formation of M23C6 type precipitates and chromium depleted zones in austenitic stainless steel10.1016/j.scriptamat.2011.06.010 ↗
41. Sigma phase evolution and nucleation mechanisms revealed by atom probe tomography in a 347H stainless steel10.1016/j.mtla.2022.101485 ↗
42. Microstructural assessment of 310S stainless steel during creep at 800 °C10.1016/j.mtla.2019.100330 ↗