Integrated Self-Supporting CoS2/Na2S@CNFs Cathode for Long-Cycle Room-Temperature Sodium-Sulfur Batteries
Source abstract
Abstract
Abstract Room-temperature sodium-sulfur (RT Na-S) batteries have emerged as promising candidates for next-generation scalable energy storage systems with significant resource and cost advantages and high energy density potential. However, their practical application faces challenges such as polysulfide shuttling, electrode volume expansion, and slow kinetics. Herein, through electrospinning combined with in situ carbon thermal reduction technology, a self-supporting three-dimensional cathode CoS2/Na2S@CNFs was successfully designed and prepared. This design ingeniously integrates active Na2S, highly conductive carbon matrix, and catalytic active CoS2, which can systematically address key challenges of poor conductivity, slow conversion kinetics, shuttle effect, and volume expansion in RT Na-S batteries. The incorporation of CoS2 significantly enhances electronic conductivity while effectively refining Na2S grains and promoting their uniform dispersion. As a result, the battery exhibits outstanding electrochemical performance with significantly reduced activation overpotential, exceptionally high initial charge specific capacity of 1142.6 mAh g–1, excellent rate capability of 570 mAh g–1 maintained at 2 C, and outstanding long cycle life. Even at a high active material loading of 4.6 mg cm–2, the battery can maintain stable performance for 500 cycles, demonstrating promising practical application potential. This study provides an effective avenue for designing integrated cathodes for high-performance practical RT Na-S batteries.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Thermal Expansion and Ionic Conductivity · Advanced battery technologies research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Qingdao University of Science and Technology , , ,
Chinese Academy of Sciences , , ,
University of Science and Technology of China , , ,
Hohai University , , , ,
Funding
Science and Technology Support Program of Jiangsu Province · Fundamental Research Funds for the Central Universities · Science and Technology Program of Suzhou
References (41)
Show source-provided references
1. Room-Temperature Sodium-Sulfur Batteries: Rules for Catalyst Selection and Electrode Design10.1002/adma.202204214 ↗
2. Recent advances in carbon-based sulfur host materials for lithium-sulfur batteries10.20517/microstructures.2023.82 ↗
3. Heterogeneous structure design for stable Li/Na metal batteries: Progress and prospects10.1016/j.esci.2024.100281 ↗
4. Coupling Lattice Strain and Sulfur Vacancy in Tin Monosulfide/Reduced Graphene Oxide Composite for High-Performance Sodium-Ion Storage10.1002/eem2.12891 ↗
5. A Heterogeneous Quasi-solid-State Hybrid Electrolyte Constructed from Electrospun Nanofibers Enables Robust Electrode/Electrolyte Interfaces for Stable Lithium Metal Batteries10.1007/s42765-023-00371-8 ↗
6. Batteries for electric vehicles: Technical advancements, environmental challenges, and market perspectives10.1002/sus2.234 ↗
7. Interface Engineering Strategies for Shuttle Mitigation in Alkali Metal–Sulfur Batteries: A Comparative Review from Li–S to Na–S and K–S Systems10.1007/s40820-025-02004-8 ↗
8. Enhanced Polysulfide Immobilization and Conversion Enabled by N/O/P Co-Doped Hollow Carbon Nanofibers Hosts in Room-Temperature Na-S Batteries10.1016/j.carbon.2026.121354 ↗
9. Electrospun heteroatoms-doped porous carbon nanofiber networks as free-standing and binder-free electrode for room temperature sodium sulfur batteries10.1016/j.est.2025.116575 ↗
10. Strategies to Mitigate the Shuttle Effect in Room Temperature Sodium-Sulfur Batteries: Improving Cathode Materials10.1039/D3DT00008G ↗
11. Remedies for Polysulfide Dissolution in Room-Temperature Sodium-Sulfur Batteries10.1002/adma.201903952 ↗
12. Status and Challenges of Cathode Materials for Room-Temperature Sodium-Sulfur Batteries10.1002/smsc.202100059 ↗
13. Room-Temperature Sodium-Sulfur Batteries: A Comprehensive Review on Research Progress and Cell Chemistry10.1002/aenm.201602829 ↗
14. Nanostructure Engineering Strategies of Cathode Materials for Room-Temperature Na-S Batteries10.1021/acsnano.2c00265 ↗
15. Pisiform Homojunction with Energy Band Bending Induced via Co-Implantation Design Enabling Fast-Charging Sodium-Sulfur Battery10.1007/s40820-026-02163-2 ↗
16. Selective and Facile Synthesis of Sodium Sulfide and Sodium Disulfide Polymorphs10.1021/acs.inorgchem.8b00776 ↗
17. Na2S–NaI Solid Solution as Positive Electrode in All-Solid-State Na/S Batteries10.1016/j.jpowsour.2022.231313 ↗
18. Performance Enhancement and Mechanistic Studies of Room-Temperature Sodium–Sulfur Batteries with a Carbon-Coated Functional Nafion Separator and a Na2S/Activated Carbon Nanofiber Cathode10.1021/acs.chemmater.5b04588 ↗
19. Small-Sized Microcrystalline SiO2 Catalyzed Na2S2-to-Na2S Conversion for High-Performance Room-Temperature Sodium–Sulfur Batteries10.1039/D5QI01291K ↗
20. Na2S-Carbon Nanotube Fabric Electrodes for Room-Temperature Sodium-Sulfur Batteries10.1002/chem.201405344 ↗
21. A Stable Anode-Free Na-S Full Cell at Room Temperature10.1016/j.ensm.2022.08.008 ↗
22. Design towards Recyclable Micron-Sized Na2S Cathode with Self-Refinement Mechanism10.1038/s41467-024-54316-9 ↗
23. Cobalt-Nitrogen-Doped ordered Macro-/Mesoporous Carbon for Highly Efficient Oxygen Reduction Reaction10.1016/j.apcatb.2016.04.006 ↗
24. Manufacture of Sodium Sulfide: Reduction of Sodium Sulfate to Sodium Sulfide at Temperatures below 800°C10.1021/ie50314a025 ↗
25. Electrospinning for Flexible Sodium-Ion Batteries10.1016/j.ensm.2021.12.022 ↗
26. In Situ Observation of Na2S Growth: A Step Toward High-Energy and Safer Room Temperature Sodium Sulfur Batteries10.1002/adma.202505966 ↗
27. Co-Co9S8-NC particles anchored on 3D hyperfine carbon nanofiber networks with a hierarchical structure as a catalyst promoting polysulfide conversion for lithium–sulfur batteries10.1039/D2TA09323E ↗
28. Laser-Induced Reactive Deposition of Nanostructured CoS2- and Co2CuS4-Based Films with Fenton Catalytic Properties10.1002/ejic.201801403 ↗
29. Metal Chalcogenide Hollow Polar Bipyramid Prisms as Efficient Sulfur Hosts for Na-S Batteries10.1038/s41467-020-19078-0 ↗
30. The Synthesis, Properties, and Potential Applications of CoS2 as a Transition Metal Dichalcogenide (TMD)10.1016/j.ijhydene.2023.01.056 ↗
31. Atomic Cobalt as An Efficient Electrocatalyst in Sulfur Cathodes for Superior Room-Temperature Sodium-Sulfur Batteries10.1038/s41467-018-06144-x ↗
32. Activating Li2S as the Lithium-Containing Cathode in Lithium–Sulfur Batteries10.1021/acsenergylett.0c00936 ↗
33. Streamline Sulfur Redox Reactions to Achieve Efficient Room-Temperature Sodium–Sulfur Batteries10.1002/anie.202200384 ↗
34. Stable Dendrite-Free Room Temperature Sodium-Sulfur Batteries Enabled by a Novel Sodium Thiotellurate Interface10.1002/anie.202412287 ↗
35. Frogspawn-Coral-Like Hollow Sodium Sulfide Nanostructured Cathode for High-Rate Performance Sodium–Sulfur Batteries10.1002/aenm.201803251 ↗
36. Locally Confined Polysulfide-Reactive Electrolytes for Shuttle-Free Sodium–Sulfur Batteries10.1021/jacs.5c05389 ↗
37. Sub-zero and Room-temperature sodium–sulfur battery cell operations: A rational current collector, catalyst and sulphur-host design and study10.1016/j.ensm.2021.08.014 ↗
38. Cycling-Driven Electrochemical Activation of Li-Rich NMC Positive Electrodes for Li-ion Batteries10.1021/acsaem.2c01239 ↗
39. Potassium Vanadates with Stable Structure and Fast Ion Diffusion Channel as Cathode for Rechargeable Aqueous Zinc-Ion Batteries10.1016/j.nanoen.2018.07.014 ↗
40. Lithium-Sulfur Battery Diagnostics through Distribution of Relaxation Times Analysis10.1016/j.ensm.2022.06.016 ↗
41. General Synthesis of Ultrafine Monodispersed Hybrid Nanoparticles from Highly Stable Monomicelles10.1002/adma.202100820 ↗